亚临界/超临界水条件下镍基合金 (Incoloy800,825,625)的硫化腐蚀特性研究 |
张洁( ), 曲积钰, 卢金玲, 刘倩, 罗兴锜 |
西安理工大学 西北旱区生态水利国家重点实验室 西安 710048 |
|
Sulfidation Corrosion Behavior of Nickel-based Alloys (Incoloy800, 825 and 625) in Sub/supercritical Water |
ZHANG Jie( ), QU Jiyu, LU Jinling, LIU Qian, LUO Xingqi |
State Key Laboratory of Eco-hydraulics in Northwest Arid Region of China, Xi'an University of Technology, Xi'an 710048, China |
引用本文:
张洁, 曲积钰, 卢金玲, 刘倩, 罗兴锜. 亚临界/超临界水条件下镍基合金 (Incoloy800,825,625)的硫化腐蚀特性研究[J]. 中国腐蚀与防护学报, 2021, 41(6): 892-898.
Jie ZHANG,
Jiyu QU,
Jinling LU,
Qian LIU,
Xingqi LUO.
Sulfidation Corrosion Behavior of Nickel-based Alloys (Incoloy800, 825 and 625) in Sub/supercritical Water. Journal of Chinese Society for Corrosion and protection, 2021, 41(6): 892-898.
链接本文:
https://www.jcscp.org/CN/10.11902/1005.4537.2020.162
或
https://www.jcscp.org/CN/Y2021/V41/I6/892
|
1 |
Ge Z W, Guo L J, Jin H. Catalytic supercritical water gasification mechanism of coal [J]. Int. J. Hydrog. Energy, 2020, 45: 9504
|
2 |
Ge Z W, Guo S H, Ren C Y F, et al. Non-catalytic supercritical water partial oxidation mechanism of coal [J]. Int. J. Hydrog. Energy, 2020, 45: 21178
|
3 |
Guo X L, Chen K, Gao W H, et al. A research on the corrosion and stress corrosion cracking susceptibility of 316L stainless steel exposed to supercritical water [J]. Corros. Sci., 2017, 127: 157
|
4 |
Behnamian Y, Mostafaei A, Kohandehghan A, et al. Characterization of oxide layer and micro-crack initiation in alloy 316L stainless steel after 20,000h exposure to supercritical water at 500 °C [J]. Mater. Charact., 2017, 131: 532
|
5 |
Yang J Q, Wang S Z, Li Y H, et al. Under-deposit corrosion of Ni-based alloy 825 and Fe-Ni based alloy 800 in supercritical water oxidation environment [J]. Corros. Sci., 2020, 167: 108493
|
6 |
Shen C, Du D H, Sun Y, et al. Corrosion behavior of nickel based alloy 825 in supercritical water [J]. Atom. Energy Sci. Technol., 2014, 48: 1660
|
6 |
沈朝, 杜东海, 孙耀等. 镍基合金825在超临界水中的腐蚀性能研究 [J]. 原子能科学技术, 2014, 48: 1660
|
7 |
Rodriguez D, Merwin A, Karmiol Z, et al. Surface chemistry and corrosion behavior of Inconel 625 and 718 in subcritical, supercritical, and ultrasupercritical water [J]. Appl. Surf. Sci., 2017, 404: 443
|
8 |
Chang K S, Huang J H, Yan C B, et al. Corrosion behavior of Alloy 625 in supercritical water environments [J]. Prog. Nucl. Energy, 2012, 57: 20
|
9 |
Chang K H, Chen S M, Yeh T K, et al. Effect of dissolved oxygen content on the oxide structure of Alloy 625 in supercritical water environments at 700 ℃ [J]. Corros. Sci., 2014, 81: 21
|
10 |
Meng N, Jiang D D, Liu Y, et al. Sulfur transformation in coal during supercritical water gasification [J]. Fuel, 2016, 186: 394
|
11 |
Liu S K, Li L H, Guo L J, et al. Sulfur transformation characteristics and mechanisms during hydrogen production by coal gasification in supercritical water [J]. Energy Fuels, 2017, 31: 12046
|
12 |
Reddy S N, Nanda S, Kozinski J A. Superc ritical water gasification of glycerol and methanol mixtures as model waste residues from biodiesel refinery [J]. Chem. Eng. Res. Des., 2016, 113: 17
|
13 |
Li Y H, Wang S Z, Yang J Q, et al. Corrosion characteristics of a nickel-base alloy C-276 in harsh environments [J]. Int. J. Hydrog. Energy, 2017, 42: 19829
|
14 |
Fulger M, Ohai D, Mihalache M, et al. Oxidation behavior of Incoloy 800 under simulated supercritical water conditions [J]. J. Nucl. Mater., 2009, 385: 288
|
15 |
Behnamian Y, Mostafaei A, Kohandehghan A, et al. A comparative study of oxide scales grown on stainless steel and nickel-based superalloys in ultra-high temperature supercritical water at 800 °C [J]. Corros. Sci., 2016, 106: 188
|
16 |
Choudhry K I, Guzonas D A, Kallikragas D T, et al. On-line monitoring of oxide formation and dissolution on alloy 800H in supercritical water [J]. Corros. Sci., 2016, 111: 574
|
17 |
Dieckmann R, Mason T O, Hodge J D, et al. Defects and cation diffusion in magnetite (III.) tracerdiffusion of foreign tracer cations as a function of temperature and oxygen potential [J]. Bericht. Bunsengesell. Physikal. Chem., 1978, 82: 778
|
18 |
LaBranche M, Garratt-Reed A, Yurek G. Early stages of the oxidation of chromium in H2-H2O-H2S gas mixtures [J]. J. Electrochem. Soc., 1983, 130: 2405
|
19 |
Lee J C, Kim M J, Lee D B. High-temperature corrosion of aluminized and chromized Fe-25.8%Cr-19.5%Ni alloys in N2/H2S/H2O-mixed gases [J]. Oxid. Met., 2014, 81: 617
|
20 |
Yang J Q, Wang S Z, Li Y H, et al. Oxidation-sulfidation attacks on alloy 600 in supercritical water containing organic sulfides [J]. Mater. Lett., 2020, 263: 127218
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|