7A52铝合金双丝MIG焊接头的不均匀性对其表面微弧氧化膜腐蚀防护作用的影响
郝利新1,2, 贾瑞灵1(), 张慧霞2, 张伟3, 赵婷1, 翟熙伟1
1 内蒙古工业大学材料学院 内蒙古自治区薄膜与涂层重点实验室 呼和浩特 010051
2 中国船舶重工集团公司第七二五研究所 海洋腐蚀与防护国家重点实验室 青岛 266101
3 中国科学院金属研究所金属腐蚀与防护实验室 沈阳 110016
Influence of Inhomogeneity of Tandem Welding Joint of 7A52 Al-alloy on Protectiveness of Micro-arc Oxidation Films on Its Surface
Lixin HAO1,2, Ruiling JIA1(), Huixia ZHANG2, Wei ZHANG3, Ting ZHAO1, Xiwei ZHAI1
1 Key Laboratory for Thin Film and Coatings of Inner Mongolia Autonomous Region, School of Materials Science and Engineering, Inner Mongolia University of Technology, Hohhot 010051, China
2 State Key Laboratory for Marine Corrosion and Protection, Luoyang Ship Material Research Institute (LSMRI), Qingdao 266101, China
3 Laboratory for Corrosion and Protection, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
全文: PDF(3266 KB)   HTML
摘要: 

以装甲用7A52铝合金双丝MIG焊接接头易于腐蚀,需要进行必要的防护为背景,采用金相显微镜、扫描电镜、能谱分析和极化曲线为表征手段,研究了焊缝组织和成分的不均匀性对表面微弧氧化膜腐蚀防护作用的影响。结果表明:焊缝区为树枝状的铸态组织;熔合区靠近焊缝一侧为细小的等轴晶组织,紧邻热影响区一侧为柱状晶;热影响区的组织部分发生了再结晶;母材为典型的轧制态纤维组织。微弧氧化膜在焊缝表面生长速率慢,Mg参与形成焊缝表面的氧化膜,使得氧化膜的钝化性减弱,致密性和均一性变差,其腐蚀防护作用不及母材和热影响区表面氧化膜的。短期浸泡时,焊缝区、热影响区及母材表面微弧氧化膜的腐蚀防护作用差别较小;长期浸泡后,焊缝表面微弧氧化膜的腐蚀防护作用明显不及母材和热影响区的。

关键词 铝合金双丝MIG焊腐蚀微弧氧化膜    
Abstract

Taking the susceptibility of the tandem welding joint of 7A52 Al-alloy into account,it is of significance to reveal the effect of the microstructural heterogeneity of the tandem metal inert gas welding joints of 7A52 Al-alloy on the corrosion performance of the micro-arc oxidation (MAO) films prepared on the surface of the weld plate by means of potentiondynamic polarization measurement, OM and SEM with EDS. It follows that the rolling base metal presents a typical fiber-like microstructure. The microstructure of the weld seam is as-cast dendritic structure. Grains in the fusion zone are equiaxed crystallites on the side adjacent to the weld, but are columnar on the other side near the heat-affected zone (HAZ). Recrystallization of grains in the heat affected zone has occurred. The growth rate of the MAO film on the weld seam is slower and Mg can be detected in the film, which may be responsible to the poor compactness and uniformity, and thus the weak passivity of the prepared MAO film, as a result, the protectiveness of the MAO film on the weld seam is worse than that on the HAZ and base metal. In general, for short-term immersion, the difference of the protectiveness of the MAO films on the weld seam, HAZ and base metal is not obvious, however, for long-term immersion, the protectiveness of the MAO film on the weld seam is obviously inferior to that on the HAZ and base metal.

Key wordsAl-alloy    tandem welding    corrosion    micro-arc oxidation
收稿日期: 2017-11-16     
ZTFLH:  TG174.45  
基金资助:内蒙古自然科学基金 (2017MS(LH)0511) 和海洋腐蚀与防护重点实验室开放研究基金 (KF160408)
作者简介:

作者简介 郝利新,男,1992年生,硕士生

引用本文:

郝利新, 贾瑞灵, 张慧霞, 张伟, 赵婷, 翟熙伟. 7A52铝合金双丝MIG焊接头的不均匀性对其表面微弧氧化膜腐蚀防护作用的影响[J]. 中国腐蚀与防护学报, 2018, 38(3): 219-225.
Lixin HAO, Ruiling JIA, Huixia ZHANG, Wei ZHANG, Ting ZHAO, Xiwei ZHAI. Influence of Inhomogeneity of Tandem Welding Joint of 7A52 Al-alloy on Protectiveness of Micro-arc Oxidation Films on Its Surface. Journal of Chinese Society for Corrosion and protection, 2018, 38(3): 219-225.

链接本文:

https://www.jcscp.org/CN/10.11902/1005.4537.2017.191      或      https://www.jcscp.org/CN/Y2018/V38/I3/219

图1  MAO样品及金相样品的截取位置及尺寸
图2  7A52铝合金双丝MIG焊接头的金相显微组织
图3  7A52铝合金双丝MIG焊接头表面MAO膜的SEM像
图4  7A52铝合金双丝MIG焊接头MAO膜截面上EDS分析结果
图5  7A52铝合金焊接接头MAO前后在3.5%NaCl溶液中浸泡不同时间的动电位极化曲线
[1] Huang J W, Yin Z M, Lei X F.Microstructure and properties of 7A52 Al alloy welded joint[J]. Trans. Nonferrous Met. Soc. China, 2008, 18: 804
[2] Zhai X W, Chen F R, Bi L Y, et al.Welding parameters and mechanical properties of electron beam welding of 7A52 aluminum alloy[J]. Trans. China Weld. Inst., 2012, 33(8): 73(翟熙伟, 陈芙蓉, 毕良艳等. 7A52铝合金电子束焊接参数及性能[J]. 焊接学报, 2012, 33(8): 73)
[3] Xie R J, Chen F R, Zhang C C, et al.Twin-wire welding technology and corrosion resistance of weld seam for 7A52 aluminum alloy[J]. Trans. China Weld. Inst., 2008, 29(12): 57(解瑞军, 陈芙蓉, 张传臣等. 7A52铝合金双丝焊工艺及焊缝耐腐蚀性[J]. 焊接学报, 2008, 29(12): 57)
[4] Zhao J J, Li Q, Cai Z H, et al.Effects of secondary phases on stress corrosion property of friction stir welded seam of 7A52 aluminum alloy under different strain rates[J]. Trans. China Weld. Inst., 2013, 34(8): 63(赵军军, 李奇, 蔡志海等. 应变速率条件下第二相对7A52铝合金搅拌摩擦焊焊缝应力腐蚀性能的影响[J]. 焊接学报, 2013, 34(8): 63)
[5] Zhang P, Li Q, Zhao J J, et al.Analysis of secondary phases and measurement of Volta potential of 7A52 aluminum alloy[J]. Chin. J. Nonferrous Met., 2011, 21: 1252(张平, 李奇, 赵军军等. 7A52铝合金中第二相分析及微区电位测试[J]. 中国有色金属学报, 2011, 21: 1252)
[6] Zhang P, Li Q, Zhao J J, et al.Electrochemical local corrosion behavior of 7A52 aluminum alloy[J]. J. Shenyang Univ. Technol., 2012, 34: 154(张平, 李奇, 赵军军等. 7A52铝合金电化学局部腐蚀行为[J]. 沈阳工业大学学报, 2012, 34: 154)
[7] Zhang C C, Chen F R, Gao Y X.Analysis on single and double wire welding technology of 7A52 aluminum alloy[J]. Trans. China Weld. Inst., 2008, 29(9): 67(张传臣, 陈芙蓉, 高云喜. 7A52铝合金单双丝焊工艺对比分析[J]. 焊接学报, 2008, 29(9): 67)
[8] Zhu J, Wang Y Q, Chen D G, et al.Distortion and properties of 7A52 aluminum alloy welded joint by single and twin wire MIG welding[J]. Ordnance Mater. Sci. Eng., 2009, 32(5): 39(朱军, 王有祁, 陈东高等. 单丝、双丝MIG对7A52铝合金焊缝性能和变形的影响[J]. 兵器材料科学与工程, 2009, 32(5): 39)
[9] Yu J, Wang K H, Xu Y L, et al.Microstructures and properties of 7A52 aluminum alloy welded joint by twin wire welding[J]. Trans. China Weld. Inst., 2005, 26(10): 87(余进, 王克鸿, 徐越兰等. 7A52铝合金双丝焊接头的组织与性能[J]. 焊接学报, 2005, 26(10): 87)
[10] Miao J G, Wang Z Z, Shen Y.Analysis of phase compositions of the micro-arc oxidation ceramic coatings on aluminum and aluminum alloy[J]. Light Alloy Fabric. Technol., 2015, 43(4): 21(苗景国, 王泽忠, 沈钰. 铝合金微弧氧化陶瓷膜层相组成述评及分析[J]. 轻合金加工技术, 2015, 43(4): 21)
[11] Mu W Y, Li Z X, Du J H, et al.Research progress of ceramic coatings formed on aluminum alloys by micro-arc oxidation[J]. Surf. Technol., 2013, 42(4): 94(慕伟意, 李争显, 杜继红等. 铝合金微弧氧化陶瓷涂层研究进展[J]. 表面技术, 2013, 42(4): 94)
[12] Walsh F C, Low C T J, Wood R J K, et al. Plasma electrolytic oxidation (PEO) for production of anodised coatings on lightweight metal (Al, Mg, Ti) alloys[J]. Trans. IMF, 2009, 87: 122
[13] Zhang Z H, Dong S Y, Wang Y J, et al.Microstructure and properties of fiber laser welded 7A52 Al alloy joints[J]. Appl. Laser, 2014, 34: 567(张智慧, 董世运, 王玉江等. 7A52铝合金光纤激光焊接接头组织与性能研究[J]. 应用激光, 2014, 34: 567)
[14] Zhang P, Li Q, Zhao J J, et al.Morphology and phase constituent of second phases in friction stir welded joint of 7A52 aluminum alloy[J]. J. Shenyang Univ. Technol., 2011, 33: 246(张平, 李奇, 赵军军等. 7A52铝合金搅拌摩擦焊接头第二相的形貌及相组成[J]. 沈阳工业大学学报, 2011, 33: 246)
[15] Tseng C C, Lee J L, Kuo T H, et al.The influence of sodium tungstate concentration and anodizing conditions on microarc oxidation (MAO) coatings for aluminum alloy[J]. Surf. Coat. Technol., 2012, 206: 3437
[16] Xu L N, Zhu J Y, Wang B.Influence of Cr content and PH value on the semi-passivation behavior of low Cr pipeline steels[J]. Acta Metall. Sin., 2017, 53: 677(徐立宁, 朱金阳, 王贝. Cr含量和PH值对低铬管线钢半钝化行为的影响[J]. 金属学报, 2017, 53: 677)
[17] Li Z S, Wu H L, Pan F S, et al.Effect of oxidation time on micro-arc oxidation ceramic coatings formed on 7A55 aluminium alloy[J]. J. Aeronaut. Mater., 2009, 29(3): 23(李忠盛, 吴护林, 潘复生等. 氧化时间对7A55铝合金微弧氧化膜的影响[J]. 航空材料学报, 2009, 29(3): 23)
[18] Liu X L, Lu L, Zou Z F, et al.Preparation and corrosion behaviors of micro-arc oxidation ceramic coating on 5083 aluminum alloy[J]. Spec. Cast. Nonferrous Alloy., 2013, 33: 85(刘晓龙, 鲁亮, 邹志锋等. 5083铝合金微弧氧化膜的制备及腐蚀特性[J]. 特种铸造及有色合金, 2013, 33: 85)
[1] 董续成, 管方, 徐利婷, 段继周, 侯保荣. 海洋环境硫酸盐还原菌对金属材料腐蚀机理的研究进展[J]. 中国腐蚀与防护学报, 2021, 41(1): 1-12.
[2] 唐荣茂, 朱亦晨, 刘光明, 刘永强, 刘欣, 裴锋. Q235钢/导电混凝土在3种典型土壤环境中腐蚀的灰色关联度分析[J]. 中国腐蚀与防护学报, 2021, 41(1): 110-116.
[3] 韩月桐, 张鹏超, 史杰夫, 李婷, 孙俊才. 质子交换膜燃料电池中TA1双极板的表面改性研究[J]. 中国腐蚀与防护学报, 2021, 41(1): 125-130.
[4] 张雨轩, 陈翠颖, 刘宏伟, 李伟华. 铝合金霉菌腐蚀研究进展[J]. 中国腐蚀与防护学报, 2021, 41(1): 13-21.
[5] 冉斗, 孟惠民, 刘星, 李全德, 巩秀芳, 倪荣, 姜英, 龚显龙, 戴君, 隆彬. pH对14Cr12Ni3WMoV不锈钢在含氯溶液中腐蚀行为的影响[J]. 中国腐蚀与防护学报, 2021, 41(1): 51-59.
[6] 左勇, 曹明鹏, 申淼, 杨新梅. MgCl2-NaCl-KCl熔盐体系中金属Mg对316H不锈钢的缓蚀性能研究[J]. 中国腐蚀与防护学报, 2021, 41(1): 80-86.
[7] 王欣彤, 陈旭, 韩镇泽, 李承媛, 王岐山. 硫酸盐还原菌作用下2205双相不锈钢在3.5%NaCl溶液中应力腐蚀开裂行为研究[J]. 中国腐蚀与防护学报, 2021, 41(1): 43-50.
[8] 史昆玉, 吴伟进, 张毅, 万毅, 于传浩. TC4表面沉积Nb涂层在模拟体液环境下的电化学性能研究[J]. 中国腐蚀与防护学报, 2021, 41(1): 71-79.
[9] 郑黎, 王美婷, 于宝义. 镁合金表面冷喷涂技术研究进展[J]. 中国腐蚀与防护学报, 2021, 41(1): 22-28.
[10] 于宏飞, 邵博, 张悦, 杨延格. 2A12铝合金锆基转化膜的制备及性能研究[J]. 中国腐蚀与防护学报, 2021, 41(1): 101-109.
[11] 贾世超, 高佳祺, 郭浩, 王超, 陈杨杨, 李旗, 田一梅. 再生水水质因素对铸铁管道的腐蚀研究[J]. 中国腐蚀与防护学报, 2020, 40(6): 569-576.
[12] 赵鹏雄, 武玮, 淡勇. 空间分辨技术在金属腐蚀原位监测中的应用[J]. 中国腐蚀与防护学报, 2020, 40(6): 495-507.
[13] 马鸣蔚, 赵志浩, 荆思文, 于文峰, 谷义恩, 王旭, 吴明. 17-4 PH不锈钢在含SRB的模拟海水中的应力腐蚀开裂行为研究[J]. 中国腐蚀与防护学报, 2020, 40(6): 523-528.
[14] 岳亮亮, 马保吉. 超声表面滚压对AZ31B镁合金腐蚀行为的影响[J]. 中国腐蚀与防护学报, 2020, 40(6): 560-568.
[15] 艾芳芳, 陈义庆, 钟彬, 李琳, 高鹏, 伞宏宇, 苏显栋. T95油井管在酸性油气田环境中的应力腐蚀开裂行为及机制[J]. 中国腐蚀与防护学报, 2020, 40(5): 469-473.