Al-Zn-Sn-Ga阳极合金的孔蚀活化钝化机理 |
李君峰,文九巴,贺俊光,马景灵,李高林 |
河南科技大学材料科学与工程学院 洛阳 471003 |
|
MECHANISM OF PITTING CORROSION ACTIVATION AND PASSIVATION OF Al-Zn-Sn-Ga ALLOY |
LI Junfeng, WEN Jiuba, HE Junguang, MA Jingling, LI Gaolin |
School of Materials Science and Engineering, Henan University of Science and Technology, Luoyang 471003 |
引用本文:
李君峰,文九巴,贺俊光,马景灵,李高林. Al-Zn-Sn-Ga阳极合金的孔蚀活化钝化机理[J]. 中国腐蚀与防护学报, 2012, 32(5): 407-411.
LI Junfeng,
WEN Jiuba,
HE Junguang,
MA Jingling,
LI Gaolin.
MECHANISM OF PITTING CORROSION ACTIVATION AND PASSIVATION OF Al-Zn-Sn-Ga ALLOY. Journal of Chinese Society for Corrosion and protection, 2012, 32(5): 407-411.
链接本文:
https://www.jcscp.org/CN/
或
https://www.jcscp.org/CN/Y2012/V32/I5/407
|
[1] Salinas D R, Garcia S G, Bessone J B. Influence of alloying elements and microstructure on aluminum sacrificial anode performance: case of Al-Zn [J]. J. Appl. Electrochem., 1999, 29(9): 1063-1071[2] Yang T J, Li G M, Chen S, et al. Self-catalysis action in pitting propagation process of low alloy steels[J]. Corros. Prot., 2010, 31(7): 540-541 (杨铁军, 李国明, 陈珊等. 低合金钢点蚀扩展过程中的自催化作用[J]. 腐蚀与防护, 2010, 31(7): 540-541)[3] Kang J, Fu R D, Luan G H, et al. In-situ investigation on the pitting corrosion behavior of friction stir welded joint of AA2024-T3 aluminum alloy[J]. Corros. Sci., 2010, 53(2): 620-626[4] Xu G, Cao C N, Lin H C, et al. Electrochemical study of active dissolution for aluminum in neutral NaCl solution[J]. Corros. Sci. Prot. Technol., 1998, 10(6): 321-326 (许刚, 曹楚南, 林海潮等. 纯铝在NaCl 溶液中活化溶解时电化学行为研究[J]. 腐蚀科学与防护技术, 1998, 10(6): 321-326)[5] Qi G T, Guo Z H, Wei B K, et al. The effect of water-quenching on microstructure and electrochemistry performance of Al-Zn-Sn-Mg anode[J]. Trans. Met. Heat Treat., 2000, 21(4): 68-72 (齐公台, 郭稚弧, 魏伯康等. 固溶处理对Al-Zn-In-Sn-Mg阳极组织与电化学性能的影响[J]. 金属热处理学报, 2000, 21(4): 68-72)[6] Cao C N. Principles of Electrochemistry[M]. Beijing: Chemical Industry Press, 2007 (曹楚南. 腐蚀电化学原理[M]. 北京: 化学工业出版社, 2004)[7] Wen J B, Wang G W, Ma J L, et al. Effect of gallium on electrochemical properties of Al-Zn-Sn alloy anode[J]. Trans. Met. Heat Treat., 2010, 31(8): 30-33 (文九巴, 王国伟, 马景灵等.Ga对Al-Zn-Sn系阳极合金电化学性能的影响[J]. 材料热处理学报, 2010, 31(8): 30-33)[8] Zhu H W, Qu X Y, Hu Y, et al. Corrosion inhibition of flaky aluminum powders prepared through sol-gel process[J]. Corros. Sci., 2010, 53(1): 481-486[9] Abedin S Z E, Enders F. Electrochemical behavior of Al, Al-In and Al-Ga-In alloys in chloride solutions containing zinc ions[J]. J. Appl. Electrochem., 2004, 34(10): 1071-1080[10] Dean J A. Lange's Chemistry Handbook[M]. American: McGraw-Hill, 2003[11] Naeini M F, Shariat M H, Eizadjou M. On the chloride-induced pitting of ultra fine grains 5052 aluminum alloy produced by accumulative roll bonding process[J]. J. Alloys Compd., 2011, 509(14): 4696-4700[12] Liu G L. Study of stress corrosion mechanism of Ti alloys by recursion method[J]. Acta Metall. Sin., 2007, 43(3): 249-253 (刘贵立. 递归法研究钛合金应力腐蚀机理[J]. 金属学报, 2007, 43(3): 249-253)[13] Ei Shabyeb H A, Abd Ei Vahab F M. Effect of gallium ions on the electrochemical behavior of Al-Sn and Al-Sn-Zn alloys in chloride solution[J]. Corros. Sci., 2001, 43(4): 642-643[14] Bessone J B, Flamini D O, Saidman S B. Comprehensive model for the activation mechanism of Al-Zn alloys produced by indium[J]. Corros. Sci., 2005, 47(1): 95-105[15] Li W, Li D Y. Influence of surface morphology on corrosion and electronic behavior[J]. Acta Mater., 2006, 54(2): 445-452[16] Zaid B, Saidi D, Benzaid A, et al. Effects of pH and chloride concentration on pitting corrosion of AA6061 aluminum alloy[J]. Corros. Sci., 2008, 50: 1841-1847 |
|