| 酸洗致基板表面状态变化对镀锡板耐蚀性的影响 |
赖漾1, 徐清亮2, 罗群1, 李谦1,3( ) |
1.上海大学材料科学与工程学院 上海 200444 2.宝山钢铁股份有限公司冷轧厂 上海 200941 3.重庆大学材料科学与工程学院 重庆 400044 |
|
| Effect of Pickling-induced Surface Changes of Steel Substrate on Corrosion Resistance of Tinplate |
LAI Yang1, XU Qingliang2, LUO Qun1, LI Qian1,3( ) |
1.School of Materials Science and Engineering, Shanghai University, Shanghai 200444, China 2.Cold Rolling Mill, Baoshan Iron and Steel Co. Ltd. , Shanghai 200941, China 3.College of Materials Science and Engineering, Chongqing University, Chongqing 400044, China |
引用本文:
赖漾, 徐清亮, 罗群, 李谦. 酸洗致基板表面状态变化对镀锡板耐蚀性的影响[J]. 中国腐蚀与防护学报, 2026, 46(2): 393-404.
Yang LAI,
Qingliang XU,
Qun LUO,
Qian LI.
Effect of Pickling-induced Surface Changes of Steel Substrate on Corrosion Resistance of Tinplate[J]. Journal of Chinese Society for Corrosion and protection, 2026, 46(2): 393-404.
| [1] |
Biermann M C, Sandenbergh R F, von Moltke T V S. Characteristics and lacquer adhesion on dip and CDC chromium passivated tinplate [J]. Corros. Sci., 2006, 48: 2925
|
| [2] |
Xia D H, Song S Z, Wang J H, et al. Research progress on corrosion mechanism of tinned steel sheet used for food parkaging [J]. J. Chin. Soc. Corros. Prot., 2017, 37: 513
|
| [2] |
夏大海, 宋诗哲, 王吉会 等. 食品包装用镀锡薄钢板的腐蚀机理研究进展 [J]. 中国腐蚀与防护学报, 2017, 37: 513
|
| [3] |
Liu Z, Deng C M, Wei J S, et al. Fast evaluation of resistance to high temperature steam sterilization process for organic coating coated tinplate by electrochemical method [J]. J. Chin. Soc. Corros. Prot., 2024, 44: 883
|
| [3] |
刘 喆, 邓成满, 魏军胜 等. 涂覆有机涂层的镀锡薄钢板耐蒸煮性能电化学快速检测技术研究 [J]. 中国腐蚀与防护学报, 2024, 44: 883
|
| [4] |
Álvarez D, Collazo A, Nóvoa X R, et al. The anticorrosive properties of sol-gel films doped with hydrotalcite nanoparticles applied on tinplate [J]. Electrochim. Acta, 2014, 131: 137
|
| [5] |
Melvin C, Jewell E, Miedema J, et al. Identifying interlayer surface adhesion failure mechanisms in tinplate packaging steels [J]. Packag. Technol. Sci., 2019, 32: 345
|
| [6] |
Ma C, Zhou B, Xia D H, et al. In-situ study the corrosion degradation mechanism of tinplate in salty water by scanning electrochemical microscopy [J]. Russ. J. Electrochem., 2018, 54: 216
|
| [7] |
Pandey S, Mishra K K, Ghosh P, et al. Characterization of tin-plated steel [J]. Front. Mater., 2023, 10: 1113438
|
| [8] |
Mouayd A A, Orazem M E, Sutter E M M, et al. Contribution of electrochemical dissolution during pickling of low carbon steel in acidic solutions [J]. Corros. Sci., 2014, 82: 362
|
| [9] |
Wang L, An C Q, An K, et al. Effect of electrode polarity of electrolytic pickling on lead content of cold rolled steel sheet for tin plating [J]. Electroplat. Finish., 2018, 37: 674
|
| [9] |
王 雷, 安成强, 安 铠 等. 电解酸洗极性对电镀锡基板铅含量的影响 [J]. 电镀与涂饰, 2018, 37: 674
|
| [10] |
Li B H, Guo K K, Liu C S. Effect of PSA tin plating process on trace lead in tin coating [J]. Chin. J. Chem. Eng., 2015, 23: 1716
|
| [11] |
Dai W W. Analysis of influencing factors of lead content within tinplate surface by MSA solution [J]. Baosteel Technol., 2021, (4): 47
|
| [11] |
戴伟伟. MSA镀液体系下镀锡板面铅含量影响因素分析 [J]. 宝钢技术, 2021, (4): 47
|
| [12] |
An C Q, An K, Zhang W J, et al. Influences of different ways of electrochemical pickling on the performance of tin-plated strip steel [J]. Electroplat. Pollut. Control, 2015, 35(4): 23
|
| [12] |
安成强, 安 恺, 张文静 等. 电解酸洗方式对镀锡带钢性能的影响 [J]. 电镀与环保, 2015, 35(4): 23
|
| [13] |
Liu B, Li B H, Zheng Z, et al. Effect of electrochemical pickling of black plate on porosity of tin plate [J]. Electroplat. Finish., 2010, 29(1): 19
|
| [13] |
刘 彪, 李兵虎, 郑 振 等. 原板的电化学酸洗对镀锡板表面形貌及孔隙率的影响 [J]. 电镀与涂饰, 2010, 29(1): 19
|
| [14] |
Liu B Y, Wang Y W, Guan Y. A study of corrosion performance of tinplate with different tin coating thickness in H2SO4 solution [J]. Materialwiss. Werkstofftech., 2021, 52: 433
|
| [15] |
Huang X Q, Li N, Jiang L M, et al. Effect of black plate on corrosion resistance of T5 tinplate [J]. J. Iron Steel Res. Int., 2006, 13: 59
|
| [16] |
Liu Z, Che X, Jiang J L, et al. EIS measurement on atmospheric exposure induced degradation of a pre-engineered passive coating on tinplate surface [J]. Measurement, 2024, 231: 114646
|
| [17] |
Meysami A, Najafabadi R A, Varnoosfaderani E N, et al. Examination of surface contamination and impurities in tinplate samples, both passivated and non-passivated [J]. Mater. Technol. Rep., 2023, 1: 293
|
| [18] |
Cova Caiazzo F, Brambilla L, Montanari A, et al. Chemical and morphological characterization of commercial tinplate for food packaging [J]. Surf. Interface Anal., 2018, 50: 430
|
| [19] |
Shen P J, Wan Y Q, Qi W, et al. Effect of surface morphology of substrate on pitting of tinplate [J]. Electroplat. Finish., 2021, 40: 1793
|
| [19] |
沈鹏杰, 万一群, 齐 韦 等. 基板表面形貌对镀锡板点锈的影响 [J]. 电镀与涂饰, 2021, 40: 1793
|
| [20] |
Lan J, Tang C, Chen C Z. Effect of substrate roughness on tinplating product performance [J]. Non-Ferrous Min. Metall., 2014, 30(4): 48
|
| [20] |
兰 剑, 唐 超, 陈成增. 基板粗糙度对镀锡产品性能的影响研究 [J]. 有色矿冶, 2014, 30(4): 48
|
| [21] |
Bao X F. Effect of surface roughness of cold-rolled black plate on corrosion resistance of tinplate [J]. Mater. Prot., 2014, 47(2): 5
|
| [21] |
包信方. 原板粗糙度对镀锡板耐蚀性的影响 [J]. 材料保护, 2014, 47(2): 5
|
| [22] |
Sharma A, Bhattacharya S, Das S, et al. Fabrication of Sn nanostructures by template assisted pulse electrodeposition [J]. Surf. Eng., 2016, 32: 378
|
| [23] |
Shen P, Gu Y, Yang N N, et al. Influences of electric current on the wettability and interfacial microstructure in Sn/Fe system [J]. Appl. Surf. Sci., 2015, 328: 380
|
| [24] |
Gines M J L, Benítez G J, Egli W, et al. Formation of an Fe-Sn intermetallic layer during the reflow process after tin plating [J]. Plat. Surf. Finish., 2003, 90: 2
|
| [25] |
Xia D H, Song S Z, Wang J H, et al. Corrosion behavior of tinplate in NaCl solution [J]. Trans. Nonferrous Met. Soc. China, 2012, 22: 717
|
| [26] |
Chen S, Xie L, Xue F. X-ray photoelectron spectroscopy investigation of commercial passivated tinplate surface layer [J]. Appl. Surf. Sci., 2013, 276: 454
|
| [27] |
He Z B, Wu Z, Gao Z M, et al. Erosion-corrosion behavior of Ni-Al-Cu coating on nickel-aluminium bronze alloy in 3.5wt%NaCl solution [J]. Corros. Sci., 2024, 238: 112380
|
| [28] |
Stern M, Geary A L. Electrochemical polarization. I. A theoretical analysis of the shape of polarization curves [J]. J. Electrochem. Soc., 1957, 104: 56
|
| [29] |
Zhou D J, Wang J H, Han Z W, et al. Corrosion behavior of tinplate in aerated and deaerated NaCl solution [J]. Int. J. Electrochem. Sci., 2017, 12: 639
|
| [30] |
Feng Y J, Yi J, Luo Q, et al. The correlation between grain structures and the corrosion behaviors of as-extruded Mg-Sm-Zn-Zr alloys [J]. Corros. Sci., 2024, 239: 112397
|
| [31] |
Brug G J, van den Eeden A L G, Sluyters-Rehbach M, et al. The analysis of electrode impedances complicated by the presence of a constant phase element [J]. J. Electroanal. Chem. Interfacial Electrochem., 1984, 176: 275
|
| [32] |
Qi G C, Gong X N, Sun D E, et al. XPS analysis of chromate passive film deposited on tinplate [J]. J. Northeastern Univ. (Nat. Sci.), 2006, 27: 875
|
| [32] |
齐国超, 贡雪南, 孙德恩 等. 镀锡钢板铬酸盐钝化膜的X射线光电子谱分析 [J]. 东北大学学报(自然科学版), 2006, 27: 875
|
| [33] |
Wang M H, Wang Z Y, Li D Y, et al. Study of topography and distribution state of the nanoscale passivation film on a rough tinplate surface [J]. Coatings, 2018, 8: 94
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|