ANALYSIS ON CORROSION BEHAVIORS OF THE BOILER FOR COMBUSTING WITH YELLOW PHOSPHORIC TAIL GAS |
GAO Huaping1, WU Fei1, LONG Jinming1, JIE Xingdi1, ZHANG Dongping2 |
1. School of Materials Science and Engineering, Kunming University of Science and Technology, Kunming 650093
2. Kunming Boiler Co., Ltd., Kunming 650217 |
|
|
Abstract The corrosion properties of 316L, 304 stainless steel and 20# boiler steel (20g) in a simulated corrosive atmosphere were investigated by means of accelerated corrosion test. The results show that corrosion rate of 316L was significantly lower than that of 304 and 20g in the simulated atmosphere. From temperature 250℃ to 300℃, the acid dew point corrosion became serious. Cavities were observed in the surface of 304 after the dew point corrosion, at where occurred pitting corrosion.
|
Received: 17 September 2009
|
|
Corresponding Authors:
GAO Huaping
E-mail: ynkmghp@263.net
|
[1] He H M. Development Direction and Measures of Phosphorus Chemicals in China [M]. Beijing: Chemical Industry Press,2007.19-21 (何浩明. 对中国磷化工业发展的思考 [M]. 北京: 化学工业出版社, 2007. 19-21)[2] Zhou S B. Conventional alloy used in WPA production [J]. Phosphat.Compd. Fert., 2005, 20(3): 64-67 (周绍彪. 湿法磷酸生产中常用的合金材料 [J]. 磷肥与复肥, 2005, 20(3): 64-67)[3] Lin C J, Xie Z X, Tian Z W. Electrochemical scanning tunneling microscope studies of initial pitting corrosion 18/8 stainless steel [J]. Corros. Sci. Prot. Technol., 1997, 9(4): 259-264) (林昌健, 谢兆雄, 田昭武. 不锈钢点腐蚀发生的早期过程 [J].腐蚀科学与防护技术, 1997, 9(4): 259-264)[4] Al-Hashem A, Caceres P G, Abdullah A. Cavitation corrosion of duplex stainless steel in sea water [J]. Corrosion, 1997, 53(2): 103-113[5] Guo Q S, Huang Y C.Wear-corrosion behavior of high Cr-Mo alloys in wet process for phosphoric acid production [J]. Corros. Sci. Prot.Technol., 1994, 6(4): 364-366 (郭清胜, 黄永昌. 高铬钼不锈钢在湿法磷酸中磨损腐蚀行为 [J]. 腐蚀科学与防护技术, 1994, 6(4): 364-366)[6] Mobin M, Malik A U. Investigations on the failure of economizer tubes in a high-pressure boiler [J]. J. Failure Anal.Prev., 2008. 69-74[7] Uusitalo M A, Vuoristo P M J, Mantyla T A. High temperature corrosion of coatings and boiler steels in oxidizing chlorine-containing atmosphere [J]. Mater. Sci. Eng., 2002, A322: 1-10[8] Wang R G, Wei Y, Zhang Q L, et al. Study on SCC behavior of austenitic stainless steels SUS316 and SUS316L in H2S saturated aqueous solutions containing Cl- [J]. J. Chin. Soc. Corros. Prot., 2000, 20(1): 48-53 (王荣光, 魏云, 张清廉等. 奥氏体不锈钢SUS316及SUS316L在含Cl-的饱和H2S水溶液中的应力腐蚀行为研究 [J].中国腐蚀与防护学报, 2000, 20(1): 48-53) |