REGULARITY OF VARIATION OF CORROSION OF Pb, Al, Cu WITH CLIMATE
;;;;
电信科学技术第五研究所
Download:  PDF(193KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  By means of naturally burying and testing metal specimen seasonally, testing soil environment factors such as temperature, humidity, salinity and conductance every half a month, the rule of cable metal materials’ ( Pb, Al and Cu) corrosion rate varying with the seasonal changing of soil environment factors within one year in Yingtan was studied. The testing result indicated that there was relativity between Pb, Al and Cu corrosion rate during different burying periods and the varying of soil environment. The maximum corrosion rate occurred when spring and summer alternated (from April to July) when the soil environment factors altered severely. The corrosion rate of Pb which was the highest among the three kind of metals was 11 times of that of Al and 3 times of that of Cu as Pb was affected by pH of acid soil, dissolvable salinity (No3—,CO32- and HCO3-) and soil animalcule.
Key words:  Pb      Al      Cu      soil corrosion      
Received:  30 May 2006     
ZTFLH:  TG172。4  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

Cite this article: 

. REGULARITY OF VARIATION OF CORROSION OF Pb, Al, Cu WITH CLIMATE. J Chin Soc Corr Pro, 2007, 27(6): 326-328 .

URL: 

https://www.jcscp.org/EN/     OR     https://www.jcscp.org/EN/Y2007/V27/I6/326

[1]Wu J,Zhang D M,Sun H Z.In-situ consecutive measuring ofsoil corrosion factors(abstract)[J].Corros.Sci.Prot.Technol.,1995,7(3):278(吴,张道明,孙慧珍.土壤腐蚀环境因素的原位连续动态检测(摘要)[J].腐蚀科学与防护技术,1995,7(3):278)氵匀
[2]Wang Y H,Zhong Z C,Wen J,et al.In-situ studies on cableand optical fibre cable and jacket metal material corrosion in soil[J].Corros.Sci.Prot.Technol.,1998,10(4):234-237(王永红,钟泽成,文杰等.电缆、光缆及金属护套材料土壤腐蚀原位测试研究[J].腐蚀科学与防护技术,1998,10(4):234-237)
[3]National Network for Corrosion Survey in Soil.Material Soil Corro-sion Testing Methods[M].Beijing:Chemical Industry Press,1990(全国土壤腐蚀试验网站编.材料土壤腐蚀试验方法[M].北京:科学出版社,1990)
[4]Wang Y H,Wen J,Lu Z H.Regularity of variation of corrosion ofmild steel with climate[J].Corros.Sci.Prot.Technol.,2000,12(6):359-360(王永红,文杰,鹿中辉.碳钢土壤腐蚀随季节变化规律[J].腐蚀科学与防护技术,2000,12(6):359-360)
[5]Cao C N.Material Natural Environmental Corrosion in China[M].Beijing:Chemical Industry Press,2005,481(曹楚南主编.中国材料自然环境腐蚀[M].北京:化学工业出版社,2005,481)
[6]ITU-T:Handbook on Outside Plant Technologies for Public Net-works ITU.Geneva,1992
[7]Wang Y H,Wen J,Lu Z H.Research on accelerated corrosiontest of Pb and Al for anions in soil[J].Modern Cable Transmis-sion,2002,2:28(王永红,文杰,鹿中晖.土壤中阴离子对铅、铝腐蚀的加速试验[J].现代有线传输,2000,2:28)
[8]Wang Y H,Lu Z H,Li Y Z.Research on corrosion behavior ofcable's metal materials in soil[J].Modern Cable Transmission,2004,4:79-83(王永红,鹿中晖,李英志.线缆金属材料在土壤中腐蚀行为研究[J].现代有线传输,2004,4:79-83)
[9]Lv R H.Research on Microbes Corrosion in Soil.Florilegium of Na-tional Network for Corrosion Survey in Soil,Vol 2[M].Shanghai:Shanghai Jiaotong University Press,1992,112(吕人豪.土壤中微生物腐蚀的研究[J].全国土壤腐蚀试验网站资料选编,第二集,上海:上海交大出版社1992,112)
[1] HUANG Peng, GAO Rongjie, LIU Wenbin, YIN Xubao. Fabrication of Superamphiphobic Surface for Nickel-plate on Pipeline Steel by Salt Solution Etching and Its Anti-corrosion Properties[J]. 中国腐蚀与防护学报, 2021, 41(1): 96-100.
[2] DAI Ting, GU Yanhong, GAO Hui, LIU Kailong, XIE Xiaohui, JIAO Xiangdong. Electrochemical Performance of Underwater Friction Stud Welding Joint in CO2 Saturated NaCl Solution[J]. 中国腐蚀与防护学报, 2021, 41(1): 87-95.
[3] DONG Xucheng, GUAN Fang, XU Liting, DUAN Jizhou, HOU Baorong. Progress on the Corrosion Mechanism of Sulfate-reducing Bacteria in Marine Environment on Metal Materials[J]. 中国腐蚀与防护学报, 2021, 41(1): 1-12.
[4] TANG Rongmao, ZHU Yichen, LIU Guangming, LIU Yongqiang, LIU Xin, PEI Feng. Gray Correlative Degree Analysis of Q235 Steel/conductive Concrete Corrosion in Three Typical Soil Environments[J]. 中国腐蚀与防护学报, 2021, 41(1): 110-116.
[5] HAN Yuetong, ZHANG Pengchao, SHI Jiefu, LI Ting, SUN Juncai. Surface Modification of TA1 Bipolar Plate for Proton Exchange Membrane Fuel Cell[J]. 中国腐蚀与防护学报, 2021, 41(1): 125-130.
[6] ZHANG Yuxuan, CHEN Cuiying, LIU Hongwei, LI Weihua. Research Progress on Mildew Induced Corrosion of Al-alloy[J]. 中国腐蚀与防护学报, 2021, 41(1): 13-21.
[7] ZUO Yong, CAO Mingpeng, SHEN Miao, YANG Xinmei. Effect of Mg on Corrosion of 316H Stainless Steel in Molten Salts MgCl2-NaCl-KCl[J]. 中国腐蚀与防护学报, 2021, 41(1): 80-86.
[8] REN Yan, QIAN Yuhai, ZHANG Xintao, XU Jingjun, ZUO Jun, LI Meishuan. Effect of Thermal Shock on Mechanical Properties of Siliconized Graphite with ZrB2-SiC-La2O3/SiC Coating[J]. 中国腐蚀与防护学报, 2021, 41(1): 29-35.
[9] WANG Xintong, CHEN Xu, HAN Zhenze, LI Chengyuan, WANG Qishan. Stress Corrosion Cracking Behavior of 2205 Duplex Stainless Steel in 3.5%NaCl Solution with Sulfate Reducing Bacteria[J]. 中国腐蚀与防护学报, 2021, 41(1): 43-50.
[10] SHI Kunyu, WU Weijin, ZHANG Yi, WAN Yi, YU Chuanhao. Electrochemical Properties of Nb Coating on TC4 Substrate in Simulated Body Solution[J]. 中国腐蚀与防护学报, 2021, 41(1): 71-79.
[11] ZHENG Li, WANG Meiting, YU Baoyi. Research Progress of Cold Spraying Coating Technology for Mg-alloy[J]. 中国腐蚀与防护学报, 2021, 41(1): 22-28.
[12] WEI Zheng, MA Baoji, LI Long, LIU Xiaofeng, LI Hui. Effect of Ultrasonic Rolling Pretreatment on Corrosion Resistance of Micro-arc Oxidation Coating of Mg-alloy[J]. 中国腐蚀与防护学报, 2021, 41(1): 117-124.
[13] YU Hongfei, SHAO Bo, ZHANG Yue, YANG Yange. Preparation and Properties of Zr-based Conversion Coating on 2A12 Al-alloy[J]. 中国腐蚀与防护学报, 2021, 41(1): 101-109.
[14] SUN Haijing, QIN Ming, LI Lin. Performance of Al-Zn-In-Mg-Ti Sacrificial Anode in Simulated Low Dissolved Oxygen Deep Water Environment[J]. 中国腐蚀与防护学报, 2020, 40(6): 508-516.
[15] WANG Lei, DONG Junhua, HAN Da, LIANG Jiankun, LI Quan, KE Wei. Phenonmenon of Cu Segregation in Cu-containing steel During Soaking at 1150 ℃[J]. 中国腐蚀与防护学报, 2020, 40(6): 545-552.
No Suggested Reading articles found!