Abstract The protection performance of four polymer/Dacromet composite systems, namely three solvent-borne polymers, polyurethane, alkyd primers and fluorinated polymer as well as a water-borne coating, styrene-acrylate latex, was studied with or without pretreatment by gamma-aminopropyltriethoxysilane (γ-APS) by electrochemical impedance spectra (EIS) in 3.5%NaCl solution. The results showed that the sequence of protective performance was: fluorinated polymer>styrene-acrylate latex>polyurethane>alkyd/Dacromet composite system due to the different hydrophobic Pretreaties of organic polymers and eistence of the dispersed microorganic particles in styrene-acrylate latex. Pretreatment with γ- APS on Dacromet illustrated a markedly enhanced anti-corrosion performance of the polyurethane and alkyd/Dacromet systems because of the presence of the silane film restrained the diffusion of corrosive particles. But it also suppressed the synergetic protective effect in styrene- acrylate latex system,which led to decrease anti- corrosion performance. Pretreatment presented no obvious influence on fluorinated polymer/ Dacromet system due to the good hydrophobic property of the polymer.
|
Received: 29 December 2004
|
|
[1]Gheno F.Clean processes—alternatives to electroplating[J].Trans.Inst.Metal.Finish.,1996,74(5):7-10 [2]Lonca M.Dacrotizing—an effective protecting against corrosion[J].Finishing,1990,14(9):35-38 [3]Fourez M,Gheno F,White P E.The application of zinc-alumini-umflake non-electrolytic surface coating[J].Trans.Inst.Metal.Finish.,1993,71(1):21-25 [4]Chen M,Yu Q S,Reddy C M.Model study investigation role ofinterfacial factors in electrochemical i mpedance spectroscopy mea-surements[J].Corrosion,2000,56(7):709-720 [5]Potvin E,Brossard L,Larochelle G.Corrosion protective perfor-mances of commercial low-VOC epoxy/urethane coatings on hot-rolled 1010 mild steel[J].Prog.Org.Coat.,1997,31:363-373 [6]Scully J R.Electrochemical i mpedance of polymer-coated steelcorrelation of i mpedance parameters withlong-termcoatings de-terioration[J].J.Electrochem.Soc.,1989,136(4):979-989 [7]Kending M,Scully J.Basic aspects of electrochemical i mpedanceapplication for thelife prediction of organic coatings on metals[J].Corrosion,1990,46:22-29 [8]Hack HP,Scully J R.Defect area determination of organic coatedsteelsin seawater using the breakpoint frequency method[J].J.Electrochem.Soc.,1991,138(1):31-40 [9]Del Amo B,Romagnoli R,Dey偄C.High performance water-based paints with non-toxic anticorrosive pigments[J].Prog.Org.Coat.,2002,45:389-397 [10]Takeshi Y.The recent progress of acrylic emulsion for coatingin-dustries[J].Prog.Org.Coat.,1983,11:205-218 [11]Liu J G,Gong G P,Yan C W.EISstudy of corrosion behaviour oforganic coating/Dacromet composite systems[J].Electrochi m.Acta,2005,50(16-17):3320-3332 [12]Zhu D Q,Van Ooij WJ.Corrosion protection of AA2024-T3 bybis-[3-(triethoxysilyl)propyl]tetrasulfide in sodiumchloridesolution,Part 2:mechanismfor corrosion protection[J].Corros.Sci.,2003,45:2177-2197 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|