Please wait a minute...
J Chin Soc Corr Pro  2003, Vol. 23 Issue (1): 21-25     DOI:
Research Report Current Issue | Archive | Adv Search |
BEHAVIOR OF CO2 PITTING CORROSION OF N80 STEEL
Changfeng Chen;Minxv Lu;Guoxian Zhao
北京科技大学材料科学与工程学院
Download:  PDF(187KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  In simulating the environment of CO2 corrosion in oilfield,the XRD,EDS and SEM techniques were adopted to study the formation an d development of CO2 pitting corrosion on N80 steel.The results demonstrated t hat Cl- anions could be enriched and nucleated at the interface between corros ion scale and matrix,which subsequently catalyzed the formation of pitting.Where as pits could also be enriched by Cl- forming approximately 3 μm enrichment l ayer at interface,thus leading to the further development of pitting.In present case,the relationship between mechanisms of anodic reaction and morphology of pi tting was discussed.
Key words:  CO2 corrosion      pitting      N80 steel      corrosion scale      
Received:  04 April 2001     
ZTFLH:  TG174  
Corresponding Authors:  Changfeng Chen   

Cite this article: 

Changfeng Chen; Minxv Lu; Guoxian Zhao. BEHAVIOR OF CO2 PITTING CORROSION OF N80 STEEL. J Chin Soc Corr Pro, 2003, 23(1): 21-25 .

URL: 

https://www.jcscp.org/EN/     OR     https://www.jcscp.org/EN/Y2003/V23/I1/21

[1]ZhangXY ,DiC ,LeiLC .CO2CorrosionandControl[M ].Beijing:ChemicalIndustryPress,2000(张学元,邸超,雷良才.二氧化碳腐蚀与控制[M ].北京:化学工业出版社,2000)
[2]ChenCF ,ZhaoGX ,YanML ,etal.StudyofCO2 corrosionscalesonN80steel[J].J .ChineseSocietyforCorrosionandProtection,2002,22(3):143(陈长风,赵国仙,严密林.N80钢CO2腐蚀产物膜研究[J].中国腐蚀与防护学报,2002,22(3):143)
[3]YangW ,GuJX ,LiQS ,XiaoJX .LocalCorrosionofMetal[M ].Beijing:ChemicalIndustryPress,1995,44-46(杨武,顾氵睿祥,黎樵焱木,肖京先.金属的局部腐蚀[M ].北京:化学工业出版社,1995,44-46)
[4]NorioSato.Towardamorefundamentalunderstandingofcorrosionprocesses[J].Corrosion,1989,45(5):354-368
[5]MaoX ,LiuX ,RevieXW .Pittingcorrosionofpipelinesteelindi lutebicarbonatesolutionwithchlorideions[J].Corrosion,1994,50(9):651-657
[6]PalaciosCA ,ShadleyJR .CharacteristicsofcorrosionscalesonsteelsinCO2-saturatedNaCIbrine[J].Corrosion,1991,47(2):122-127
[7]LinterBR ,BursteinGT .Reactionofpipelinesteelsincarbondiox idesolutions[J].Corros.Sci.,1999,42(2):117-139
[8]DaviesDH ,BursteinGT .Theeffectsofbicarbonateonthecorro sionandpassivationofiron[J].Corrosion,1980,36(8):416-422
[9]OgundeleGI,WhiteWE .Someobservationoncorrosionofcarbonsteelinaqueousenvironmentscontainingcarbondioxide[J].Corro sion,1986,42(2):71-76
[10]CroletJL ,BonisMR .PHmeasurementsinaqueousCO2 solutionunderhighpressureandtemperature[J].Corrosion,1983,39(2):39-46
[11]ShanghaiPharmaceuticalIndustryDesignInstitute.HandbookforChemicalEngineeringTechnologyDesign[M ].Beijing:ChemicalIndustryPress,1996,2-364(上海医药设计院编.化工工艺设计手册[M ].北京:化学工业出版社,1996,2-364)
[1] RAN Dou, MENG Huimin, LIU Xing, LI Quande, GONG Xiufang, NI Rong, JIANG Ying, GONG Xianlong, DAI Jun, LONG Bin. Effect of pH on Corrosion Behavior of 14Cr12Ni3WMoV Stainless Steel in Chlorine-containing Solutions[J]. 中国腐蚀与防护学报, 2021, 41(1): 51-59.
[2] ZHANG Hao, DU Nan, ZHOU Wenjie, WANG Shuaixing, ZHAO Qing. Effect of Fe3+ on Pitting Corrosion of Stainless Steel in Simulated Seawater[J]. 中国腐蚀与防护学报, 2020, 40(6): 517-522.
[3] YU Haoran, ZHANG Wenli, CUI Zhongyu. Difference in Corrosion Behavior of Four Mg-alloys in Cl--NH4+-NO3- Containing Solution[J]. 中国腐蚀与防护学报, 2020, 40(6): 553-559.
[4] DAI Mingjie, LIU Jing, HUANG Feng, HU Qian, LI Shuang. Pitting Corrosion Behavior of X100 Pipeline Steel in a Simulated Acidic Soil Solution under Fluctuated Cathodic Protection Potentials Based on Orthogonal Method[J]. 中国腐蚀与防护学报, 2020, 40(5): 425-431.
[5] ZHANG Xin, YANG Guangheng, WANG Zehua, CAO Jing, SHAO Jia, ZHOU Zehua. Corrosion Behavior of Al-Mg-RE Alloy Wires Subjected to Different Cold Drawing Deformation[J]. 中国腐蚀与防护学报, 2020, 40(5): 432-438.
[6] HE San, SUN Yinjuan, ZHANG Zhihao, CHENG Jie, QIU Yunpeng, GAO Chaoyang. Corrosion Behavior of 20# Steel in Alkanolamine Solution Mixed with Ionic Liquid Containing Saturated CO2[J]. 中国腐蚀与防护学报, 2020, 40(4): 309-316.
[7] LI Qing, ZHANG Deping, WANG Wei, WU Wei, LU Lin, AI Chi. Evaluation of Actual Corrosion Status of L80 Tubing Steel and Subsequent Electrochemical and SCC Investigation in Lab[J]. 中国腐蚀与防护学报, 2020, 40(4): 317-324.
[8] JIA Yizheng, WANG Baojie, ZHAO Mingjun, XU Daokui. Effect of Solid Solution Treatment on Corrosion and Hydrogen Evolution Behavior of an As-extruded Mg-Zn-Y-Nd Alloy in an Artificial Body Fluid[J]. 中国腐蚀与防护学报, 2020, 40(4): 351-357.
[9] HE Zhuang,WANG Xingping,LIU Zihan,SHENG Yaoquan,MI Mengxin,CHEN Lin,ZHANG Yan,LI Yuchun. Passivation and Pitting of 316L and HR-2 Stainless Steel in Hydrochloric Acid Liquid Membrane Environment[J]. 中国腐蚀与防护学报, 2020, 40(1): 17-24.
[10] SU Xiaohong,HU Huie,KONG Xiaodong. Corrosion Behavior of W Particles/Zr41.2Ti13.8Cu12.5Ni10Be22.5 Metallic Glass Matrix Composite in 3%NaCl Solution[J]. 中国腐蚀与防护学报, 2020, 40(1): 70-74.
[11] WANG Biao,DU Nan,ZHANG Hao,WANG Shuaixing,ZHAO Qing. Accelerating Effect of Pitting Corrosion Products on Metastable Pitting Initiation and the Stable Pitting Growth of 304 Stainless Steel[J]. 中国腐蚀与防护学报, 2019, 39(4): 338-344.
[12] Yu LI,Lei GUAN,Guan WANG,Bo ZHANG,Wei KE. Influence of Mechanical Stresses on Pitting Corrosion of Stainless Steel[J]. 中国腐蚀与防护学报, 2019, 39(3): 215-226.
[13] Siqi ZHANG,Nan DU,Meifeng WANG,Shuaixing WANG,Qing ZHAO. Effect of Cathode Area on Stable Pitting Growth Rate of 304 Stainless Steel in 3.5%NaCl Solution[J]. 中国腐蚀与防护学报, 2018, 38(6): 551-557.
[14] Bobo HUANG,Ping LIU,Xinkuan LIU,Pinxiu MEI,Xiaohong CHEN. Seawater Corrosion Behavior of New 70-1 Tin Brass Net in Waters off Dachen Island for Two Years[J]. 中国腐蚀与防护学报, 2018, 38(6): 594-600.
[15] Zhimin FAN, Jin YU, Yingwei SONG, Dayong SHAN, En-Hou HAN. Research Progress of Pitting Corrosion of Magnesium Alloys[J]. 中国腐蚀与防护学报, 2018, 38(4): 317-325.
No Suggested Reading articles found!