Please wait a minute...
中国腐蚀与防护学报  2009, Vol. 29 Issue (6): 415-420         
  研究报告 本期目录 | 过刊浏览 |
静水压力对Fe-20Cr合金点蚀行为的影响
杨延格1;崔中雨1;陈杰1;曹靖涛1;张涛1;2;邵亚薇1;2;孟国哲1;2;王福会1;2
1. 哈尔滨工程大学材料科学与化学工程学院腐蚀与防护实验室 哈尔滨 150001
2. 中国科学院金属研究所金属腐蚀与防护国家重点实验室 沈阳 110016
INFLUENCE OF HYDROSTATIC PRESSURE ON THE PITTING BEHAVIOR OF Fe-20Cr Alloy
YANG Yange1; CUIZhongyu1; CHEN Jie1; CAO Jingtao1; ZHANG Tao1;2; SHAO Yawei1;2; MENG Guozhe1;2; WANG Fuhui1;2
1. Corrosion and Protection Laboratory; College of Material Science and Chemical Engineering;Harbin Engineering University; Harbin 150001
2. State Key Laboratory for Corrosion and Protection;Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110016
引用本文:

杨延格 崔中雨 陈杰 曹靖涛 张涛 邵亚薇 孟国哲 王福会. 静水压力对Fe-20Cr合金点蚀行为的影响[J]. 中国腐蚀与防护学报, 2009, 29(6): 415-420.
. INFLUENCE OF HYDROSTATIC PRESSURE ON THE PITTING BEHAVIOR OF Fe-20Cr Alloy[J]. J Chin Soc Corr Pro, 2009, 29(6): 415-420.

全文: PDF(921 KB)  
摘要: 

基于统计学方法和随机理论,利用动电位极化曲线和恒电位测试技术研究静水压力对Fe-20Cr合金点蚀行为的影响。随着静水压力的增加, Fe-20Cr合金的击破电位降低,维钝电流密度减小,耐蚀性能变差。静水压力对Fe-20Cr合金点蚀产生和点蚀生长的研究表明:高的静水压力下,亚稳态点蚀发生的频率加快且向稳态点蚀发展的倾向增大,从而导致点蚀的产生速度加快,点蚀的孕育期缩短,但点蚀的产生机制并没有发生改变;静水压力的增加增大了点蚀的生长概率,高压下产生的点蚀更容易成长为大的腐蚀坑。

关键词 : 静水压力,  腐蚀,  随机理论,  Fe-20Cr,  深海    
Abstract:

The effect of hydrostatic pressure on pitting behavior of Fe-20Cr alloy in 3.5% NaCl solution was investigated by means of potentiodynamic polarization and potentiostatic technology. For the polarization curve measurement, the specimens were kept for 1 h in the NaCl solution at various hydrostatic pressures and then scanned in 0.333 mV/s, 3 mV/s, and 5 mV/s scan rate respectively. For the induction time measurement, the specimen was pretreated in Na2SO4 solution at a constant potential, -0.22 V, for 500 s. After pretreatment, the specimen was kept in the NaCl solution at various hydrostatic pressures, and a potentiostatic technique\linebreak(-0.22 V) was used to measure the anodic current trace. Experiment data was analyzed based on statistical and stochastic approaches. With the increasing of hydrostatic pressure, the pit corrosion resistance of Fe-20Cr alloy was deteriorated, which was distinguished by the decrease of Ecrit and the increase of passive current density.The results also showed that there were obvious effects on processes of pit initiation and pit growth of Fe-20Cr alloy: (1) the pit generation rate was evidently increased compared with that under lower hydrostatic pressure resulting from the metastable pits'  frequent initiation and increased tendency to stable pits. However, it seemed that pit generation mechanism showed no hydrostatic pressure dependence. (2) the probability of pit growth increased with the increasing of hydrostatic pressure, which implied that the metastable pit on Fe-20Cr alloy exhibited higher probability to become larger pit cavity during the same time interval than that under lower hydrostatic pressure.

Key words: hydrostatic pressure    corrosion    stochastic theory    Fe-20Cr    deep ocean
收稿日期: 2008-10-27     
ZTFLH: 

TG174.41

 
基金资助:

国家自然科学基金项目(50771038)资助

作者简介: 杨延格,男,1985年生,硕士生,研究方向为材料腐蚀与防护

[1] Xu L K, Li W J, Chen G Z. Deep sea corrosion test technique [J]. Marine Sci., 2005, 29(7):1-3
(许立坤,李文军,陈光章. 深海腐蚀试验技术 [J]. 海洋科学, 2005,29(7):1-3)
[2] Guo W M, Li W J,Chen G Z. Corrosion testing in the deep ocean [J]. Equip. Env. Eng.,2006, 3(1):11-12
(郭为民,李文军,陈光章.材料深海环境腐蚀试验 [J]. 装备环境工程, 2006,3(1):11-12)
[3] Beccaria A M, Poggi G, Gingaud D, et al. Effect of hydrostatic
pressure on passivating power of corrosion layers formed on 6061 T6 aluminum alloy in sea water [J]. Br. Corros. J., 1994, 29(1): 65-69
[4] Beccaria A M, Fiordiponti P, Msttogno G. The effect of hydrostatic pressure on the corrosion of nickel in slightly alkaline solutions containing Cl-ions [J]. Corros. Sci., 1989, 29(4): 403-416
[5] Beccaria A M, Poggi G. Influence of hydrostatic pressure on pitting of aluminum in sea water [J]. Br. Corros. J., 1985, 20(4): 183-186
[6] Barous B. The kinetics of pit generation on stainless steels [J].Corros. Sci., 1988, 28(10): 969-986
[7] ShibataT. Stochastic studies of passivity breakdown [J]. Corros. Sci., 1990, 31: 413-423
[8] Gabrielli C, Huet F, Keddam M, Oltra R. A review of the probabilistic aspects of localized corrosion [J]. Corrosion.1990, 46: 266-278
[9] Salvago G, Fumagali G, Mollica A. A statistical evaluation of AISI 316 stainless steel resistance to crevice corrosion in 3.5% NaCl solution and in natural sea water after pre-treatment in HNO3 [J]. Corros.Sci., 1987, 27(9): 927-936
[10] Fujimoto S, Shibata T, Minamida M, et al. A statistical evaluation of crevice corrosion on type 304 stainless steel [J]. Corros. Sci., 1994 36(8): 1575-1583
[11] Shibata T, Yaocan Zhu. The effect of film formation potential on the stochastic processes of pit generation on anodized titanium [J].Corros. Sci., 1994, 36(1): 153-163
[12] Ilevbare G, Burstein G. Role of alloyed molybdenum in the inhibition of pitting corrosion in stainless steel [J]. Corros. Sci., 2001, 43: 485-513
[13] Burstein G, Vines S. Repetitive nucleation of  corrosion pits on stainless steel and the effects of surface roughness [J]. J. Electrochem.Soc. 2001, 148: B504-B516
[14] Burstein G, Soutob R. Improvement in pitting resistance of stainless steel surfaces by prior anodic treatment in metasilicate solution [J]. J. Electrochem. Soc., 2004, 151: B537-B542
[15] Shibata T. Statistical and stochastic approaches to localized corrosion [J]. 1996, 52(11): 813-830
[16] Moayed M H, Newman R C. Evolution of current transients and morphology of metastable pitting and stable pitting on stainless steel near the critical pitting temperature [J]. Corros. Sci., 2006, 48: 1004-1018
[17] Shibata T. Stochastic studies of passivity breakdown [J]. Corros.Sci., 1990, 31: 413-423
[18] Salvago G, Fumagalli G. Application of breakdown potential distribution in corrosion comparisons of stainless steels [J]. Corros. Sci., 1996, 52(10): 760-767
[19] Trueman Antony R. Determining the probability of stable pit initiation on aluminium alloys using potentiostatic electrochemical measurements [J]. Corros. Sci., 2005, 47: 2240-2256

[1] 李岩, 高科, 张伟, 陈信斌, 隋显杰, 陈洪生, 王晓雅, 冷雪松, 武俊伟. 深海装备涂层功能强化设计及性能调控机制研究进展[J]. 中国腐蚀与防护学报, 2026, 46(5): 1305-1325.
[2] 黎敏, 魏高飞, 邓书端, 李向红. 扫描电化学显微镜(SECM)在缓蚀剂研究中的进展与展望[J]. 中国腐蚀与防护学报, 2026, 46(5): 1326-1342.
[3] 谢敬礼, 王友志, 乔书振, 牛佳雨, 郝龙, 曹胜飞, 王俭秋. 高放废物地质处置库近场环境中碳钢腐蚀产物演化研究进展[J]. 中国腐蚀与防护学报, 2026, 46(5): 1343-1352.
[4] 周书宇, 刘昌璞, 杨留洋, 耿杰, 范海明, 张大磊, 鞠虹. 在超临界CO2 工况和典型环境因素共影响下的管线钢腐蚀及防护技术研究进展[J]. 中国腐蚀与防护学报, 2026, 46(5): 1353-1368.
[5] 黄绘, 李树丽, 邓书端, 李向红. 自修复材料在防护涂层中的研究进展及展望[J]. 中国腐蚀与防护学报, 2026, 46(5): 1369-1388.
[6] 曾崎, 虞文军, 门向南, 冯保净, 杨耀, 朱凯, 葛玉麟, 应韬, 曾小勤. 高强耐蚀稀土镁合金研究进展[J]. 中国腐蚀与防护学报, 2026, 46(5): 1415-1424.
[7] 张强, 卢壹梁, 金焱, 陈云, 杨丙坤, 王晓芳, 韩钰. 环境腐蚀性分级及大气/土壤腐蚀性地图绘制技术研究进展[J]. 中国腐蚀与防护学报, 2026, 46(5): 1425-1436.
[8] 许佳程, 刘家兵, 黄诗雨, 金灵好, 谭伟, 郭娜, 刘涛. 人工极地海域环境致EH40船板钢的力学性能损伤与应力腐蚀行为研究[J]. 中国腐蚀与防护学报, 2026, 46(5): 1437-1451.
[9] 郑凯, 王艺陶, 王东胜, 刘伟, 蒋颖畅, 黄嵘, 常雪婷. 腐蚀-应力耦合作用对极地船用螺旋桨低碳马氏体不锈钢失效机理影响研究[J]. 中国腐蚀与防护学报, 2026, 46(5): 1452-1462.
[10] 齐晓涵, 翟海民, 李文生, 洪昊, 曹元, 俞雷, 陈博瀚. Al2O3 磨加量对铝合金搪瓷涂层组织结构及腐蚀性能的影响[J]. 中国腐蚀与防护学报, 2026, 46(5): 1497-1507.
[11] 贾梦瑶, 张伟强, 王媛, 谭季波, 邱建科, 郝延天, 吴欣强. 在3.5%NaCl溶液中压力变化对Ti80合金应力腐蚀行为的影响[J]. 中国腐蚀与防护学报, 2026, 46(5): 1508-1516.
[12] 李晓峰, 李艳茹, 卢云飞, 张泰华, 常雪婷, 安燕. 力学与防腐性能协同增强的聚吡咯改性芳纶纤维/环氧复合涂料[J]. 中国腐蚀与防护学报, 2026, 46(5): 1517-1526.
[13] 曹天慧, 杨砚淇, 刘雨薇, 吴磊, 郭泉忠, 贾志刚, 曹公望, 汪川. 23MnNiMoCr54钢在不同pH的模拟高矿化水中腐蚀机理研究[J]. 中国腐蚀与防护学报, 2026, 46(5): 1537-1548.
[14] 赵先锐, 戴中国, 李战江, 徐育烺, 张会霞, 李旺. 添加Y、Hf对AlCoCrFeNi高熵合金涂层在NaCl溶液中的腐蚀行为的影响[J]. 中国腐蚀与防护学报, 2026, 46(5): 1549-1559.
[15] 王兴斌, 李家民, 伍登骏, 唐伟能, 杨静, 郭嘉成, 杨欣宇, 侯娟. Al含量对Mg-xAl-Zn合金耐腐蚀性能的影响[J]. 中国腐蚀与防护学报, 2026, 46(5): 1560-1568.