Please wait a minute...
中国腐蚀与防护学报  2007, Vol. 27 Issue (5): 274-278          
  研究报告 本期目录 | 过刊浏览 |
不同地区大气曝晒对涂层耐蚀性能的影响I.丙烯酸聚氨酯涂层
邓洪达;张三平;杨丽霞
西南石油大学材料工程学院
ANTI-CORROSION BEHAVIOR OF COATING EXPOSED IN DIFFERENT REGIONS I. ACRYLIC/POLYURETHANE COATING
;;
西南石油大学材料工程学院
引用本文:

邓洪达; 张三平; 杨丽霞 . 不同地区大气曝晒对涂层耐蚀性能的影响I.丙烯酸聚氨酯涂层[J]. 中国腐蚀与防护学报, 2007, 27(5): 274-278 .

全文: PDF(294 KB)  
摘要: 痛过检测不同大气环境中曝晒后丙烯酸聚氨酯涂层的光泽度、吸水率、涂层/金属间结合强度、涂层的耐盐雾腐蚀性和界面电化学腐蚀特征,研究武汉和拉萨地区大气环境对丙烯酸聚氨酯涂层耐蚀性能的影响。结果表明,丙烯酸聚氨酯涂层在拉萨大气环境中老化程度相对较为严重。在拉萨地区涂层主要以光降解方式老化,而在武汉地区涂层以光降解和水降解方式老化;在拉萨地区,涂层阻挡腐蚀性介质能力下降较为明显,曝晒12个月后涂层的界面电极电化学反应由扩散步骤控制,而在武汉地区该反应主要由电化学步骤控制。
关键词 : 涂层老化,  大气曝晒,  丙烯酸聚氨酯,  耐蚀性能    
Abstract:Effect of different climates on anti-corrosion of acrylic/polyurethane coating have been studied in this paper. Anti-corrosion of the coatings after exposed at Wuhan and Lasa were evaluated by gross loss rate, water absorption rate, rupture strength, salt spray test and EIS. The results showed that coating exposed in Lasa aged more severely than in Wuhan, accordingly anti-corrosion of coating in Lasa lost more badly than that in Wuhan. The main way of the degradation of the coating exposed in Lasa was photo-oxidation degradation. However the way of the degradations of the coating exposed in Wuhan were photo-oxidation and hydrolytic degradation. The capability of the coating exposed in Lasa to prohibit corrosive media through coating lost more badly than that in Wuhan. The electrochemical reaction rate, which was produced on the interface, was controlled by diffusion step after the coating was exposed in Lasa for 12 months. However, the electrochemical reaction rate was controlled by electrochemical step in Wuhan.
Key words: aging    outdoor exposure    Acrylic/polyurethane coating    anti-corrosion
收稿日期: 2006-04-12     
ZTFLH:  TG174.41  
[1]Armstrong R D,Jenkins A T A,Johnson B W.An investigationinto the UV breakdown of thermoset polyester coatings usingimpedance spectroscopy[J].Corros.Sci.,1995,37:1615-1625
[2]Funke W.Application of EIS to study the degradation of polymer-coated metals[A].Polymeric Materials for Corrosion Control[C].Washington,USA,1986:222-229
[3]Deng H D,Zhang S P,Cheng L T.A comparative study of agingbehavior of different fluorocarbon coating exposed in Wuhan[J].Mater.Prot.,2006,39(10):19-22(邓洪达,张三平,陈澜涛.不同氟碳丙烯酸聚氨酯涂层在武汉地区老化行为的比较[J].材料保护,2006,39(10):19-22)
[4]Weathering Test and Research Center of Science Technology andIndustry for National Defense,Report on weathering factors datumin corrosion test sites in China and its changing law[R].Chongqing:China No.59 Institute of Weapon Industry,2004(国防科技工业自然环境试验研究中心.全国大气腐蚀试验网站地面气象因素数据汇总及其规律总结报告[R].重庆:中国兵器工业第五九研究所,2004)
[5]Cao C N,Zhang J Q.Introduction of EIS[M].Beijing:SciencePress,2002(曹楚南,张鉴清.电化学阻抗谱导论[M].北京:科学出版社,2002)
[6]Armstrong R D,Wright J D.Polymer protective coatings:The dis-tinction between coating porosity and the wetted metal area[J].Electrochem.Acta,1993,38:1799-1801
[7]Kurt A Wood,Christopher Cypcar,Lotfi Hedhli.Predicting theexterior durability of new fluoropolymer coatings[J].FluorineChemistry,2000,104:63-71
[8]Tinh N Nguyen,Joseph B Hubbard,Geoffrey B McFadded.Amathematical model for the cathodic blistering of organic coatingson steel immersed in electrolytes[J].J.Coat.Technol.,1991,63(794):55-60
[9]Xu Y X,Yan C W,Ding J.Diffusion and absorption of hydro-sphere in coating[J].Corros.Sci.Prot.Technol.,2001,13(sup-pl.):493-496(徐永祥,严川伟,丁杰等.水汽在氟碳涂层中的扩散和吸收[J].腐蚀科学与防护技术,2001,13(suppl.):493-496)
[10]Liu B,Li Y,Lin H C.Progress in study on degradation of anti-corrosion coatings[J].Corros.Sci.Prot.Technol.,2001,13:305-307(刘斌,李瑛,林海潮.防腐蚀丙烯酸聚氨酯涂层失效行为研究进展[J].腐蚀科学与防护技术,2001,13:305-307)
[1] 郑凯, 王艺陶, 王东胜, 刘伟, 蒋颖畅, 黄嵘, 常雪婷. 腐蚀-应力耦合作用对极地船用螺旋桨低碳马氏体不锈钢失效机理影响研究[J]. 中国腐蚀与防护学报, 2026, 46(5): 1452-1462.
[2] 张春艳, 张瑜心, 陈必秀, 于宝兴, 周鹏. 铸造缺陷对AZ91D镁合金Mn-P系化学转化膜耐蚀性能的影响[J]. 中国腐蚀与防护学报, 2026, 46(5): 1475-1484.
[3] 张晓晨, 杨闯, 姜旭, 陈永生, 赵佳祥, 赵阳, 周鹏, 张涛, 王福会. 镁合金的一种致密微弧氧化涂层工艺及性能的研究[J]. 中国腐蚀与防护学报, 2026, 46(4): 1218-1226.
[4] 赖漾, 徐清亮, 罗群, 李谦. 酸洗致基板表面状态变化对镀锡板耐蚀性的影响[J]. 中国腐蚀与防护学报, 2026, 46(2): 393-404.
[5] 张雄斌, 党恩, 于晓婧, 汤玉斐, 赵康. 油气田用马氏体不锈钢腐蚀性能研究现状与进展[J]. 中国腐蚀与防护学报, 2025, 45(4): 837-848.
[6] 周谦永, 赖漾, 李谦. 酸洗工艺对不同锡量二次冷轧镀锡板耐蚀性能的影响[J]. 中国腐蚀与防护学报, 2025, 45(4): 939-946.
[7] 陈宇强, 冉光林, 陆丁丁, 黄磊, 曾立英, 刘阳, 支倩. 循环强化对7075铝合金腐蚀行为的影响[J]. 中国腐蚀与防护学报, 2025, 45(4): 1051-1060.
[8] 马晋遥, 董楠, 郭振森, 韩培德. B、Ce微合金化对S31254超级奥氏体不锈钢析出相及耐蚀性能的影响[J]. 中国腐蚀与防护学报, 2024, 44(6): 1610-1616.
[9] 程永贺, 付俊伟, 赵茂密, 沈云军. 高熵合金耐蚀性研究进展[J]. 中国腐蚀与防护学报, 2024, 44(5): 1100-1116.
[10] 李刚卿, 刘茜, 孙晓光, 潘景龙, 曹祥康, 董泽华. 缺陷自预警涂层的触发机制及制备策略研究进展[J]. 中国腐蚀与防护学报, 2024, 44(3): 540-552.
[11] 汪涵敏, 黄峰, 袁玮, 张佳伟, 王昕煜, 刘静. 新型Cu-Mo耐候钢在模拟海洋大气环境中的腐蚀行为[J]. 中国腐蚀与防护学报, 2023, 43(3): 507-515.
[12] 毛训聪, 陈乐平, 彭聪. Ca-P涂层和Sr-P涂层对脉冲磁场下凝固的Mg-Zn-Zr-Gd合金耐蚀性的影响[J]. 中国腐蚀与防护学报, 2023, 43(3): 647-655.
[13] 蒋芳芳, 云虹, 彭莉, 张依豪, 李卫顺, 代文静, 王保峰, 徐群杰. 原位聚合聚苯胺改性NiFe-LDH复合涂层的防护性能研究[J]. 中国腐蚀与防护学报, 2023, 43(2): 312-320.
[14] 张小丽, 寻懋年, 梁小红, 张彩丽, 韩培德. 含Ce S31254超级奥氏体不锈钢析出相析出行为及耐蚀性[J]. 中国腐蚀与防护学报, 2023, 43(2): 384-390.
[15] 郎丰军, 黄峰, 徐进桥, 李利巍, 岳江波, 刘静. Mg处理X70级抗酸性海底管线钢 (X70MOS) 成分设计及耐蚀性能研究[J]. 中国腐蚀与防护学报, 2021, 41(5): 617-624.