API X56钢在含H2S的海洋大气中的应力腐蚀开裂
郑传波1;2;黄彦良1;霍春勇3;于青1;2;朱永艳1;2
1.中国科学院海洋研究所 青岛 266071
2.中国科学院研究生院 北京 100039
3.中国石油天然气总公司石油管材研究所 西安 710065
STRESS CORROSION CRACKING OF X56 GRADE PIPELINE STEEL IN ATMOSPHERIC ENVIRONMENT CONTAINING H2S
ZHENG Chuanbo1;2;HUANGYanliang1;HUO Chunyong3;YU Qing1;2;ZHU Yongyan1;2
1.Institute of Oceanology;Chinese Academy of Sciences; Qingdao 266071
2.Graduate University of Chinese Academy of Sciences; Beijing 100039
3.Tubular Goods Research Center of China National Petroleum Corporation; Xi'an 710065
引用本文:

郑传波 黄彦良 霍春勇 于青 朱永艳. API X56钢在含H2S的海洋大气中的应力腐蚀开裂[J]. 中国腐蚀与防护学报, 2009, 29(1): 19-23.
, , , . STRESS CORROSION CRACKING OF X56 GRADE PIPELINE STEEL IN ATMOSPHERIC ENVIRONMENT CONTAINING H2S[J]. J Chin Soc Corr Pro, 2009, 29(1): 19-23.

全文: PDF(1106 KB)  
摘要: 

采用慢应变速率拉伸及Devnathan-Stachurski双电解池技术研究了 X56钢在模拟海洋大气环境中形变及H2S含量对其应力腐蚀开裂及氢渗透行为的影响。结果表明,在H2S含量相同时,拉伸速率越小,试样断裂延伸率越小。在相同拉伸速率下,随着H2S含量增大,试样断裂延伸率减小,扫描电镜微观分析(SEM)表明,其断裂特征由塑性断裂逐渐转变为脆性断裂。电化学渗氢实验表明,随着H2S含量的增大,第一干湿循环氢渗透电流并不单调增大,H2S对氢渗透电流的作用由H2S的表面覆盖度和腐蚀产物膜来共同控制。从多个干湿循环来看,H2S可增大氢渗透电流,材料的渗氢加剧,脆性增大。

关键词 : H2S,  应力腐蚀开裂敏感性,  氢脆,  大气腐蚀    
Abstract:

Susceptibility to SCC of X56 grade pipeline steel was investigated by slow strain rate test (SSRT) and Devnathan-Stachurski double electrolytic cell in atmospheric environment containing H2S. The results showed that the fracture strain decreased while the strain rate decreased in the same H2S concentration environment. And the fracture strain decreased with increasing the concentration of H2S at the same strain rate 6.67x10-7 s-1. The SEM fractographs of the specimens also showed that the susceptibility to stress corrosion cracking (SCC) increased. The hydrogen permeation test showed that hydrogen permeation current did not increase with increasing the concentration of H2S in the first wet-dry cycle because of the formation of product film. The longer the experiment time, the more the hydrogen atom permeated through the specimen. This trend partially attribute to the surface coverage ratio (θ) of H2S and the corrosion product film.

Key words: hydrogen sulfide    stress corrosion cracking    hydrogen embrittlement    atmospheric environment
收稿日期: 2007-04-16     
ZTFLH: 

P734

 
基金资助:

国家自然科学基金项目(40576049),中国科学院知识创新工程重要方向项目(KZCX2-YW-210)

[1] Van Gelder K,Erlings J G,Damen J W M,et al. The stress corrosion cracking of duplex stainless steel in H2S/CO2/Cl- environments [J]. Corros. Sci.,1987, 27(10-11):1271-1279
[2] Barteri M,Mancia F,Tamba A,et al. Engineering diagrams and sulphide stress corrosion cracking of duplex stainless steels in deep sour well environment [J]. Corros. Sci.,1987,27(10-11):1239-1250
[3] Huang Y L,Zhu Y Y. Hydrogen ion reduction in the process of iron rusting [J]. Corros. Sci.,2005,47(6):1545-1554
[4] Devnathan M A V,Stachurski Z. A technique for the evaluation of hydrogen embrittlement characteristics of electroplating baths[J].J. Electrochem,Soc.,1963,110(8): 886-894
[5] GB17378. 4--1998,Seawater analysis--Part 4 of criterion of marine monitoring[S].
(GB17378. 4--1998,海洋监测规范第4部分~海水分析[S].)
[6] MasatoKobayashi,Atsushi Nishikata,Tooru Tsuru. Hydrogen embrittlement of reinforced steels in high alkaline chloride environments[A]. 45th Forum on Engineering Science and Technology, Chinese Academy of Engineering & 3rd international symposium on marine corrosion and control[C]. Qingdao,2006,93-97
[7] Tsai S Y,Shih H C. A statistical failure distribution and lifetime assessment of the HSLA steel plates in H2S containing environments[J]. Corros. Sci.,1996,38(5): 705-719
[8] Qiao L J,Wang Y B,Chu W Y. Mechanism of Stress Corrosion[M]. Beijing:Science Press,1993:83
(乔利杰,王燕斌,褚武扬. 应力腐蚀机理[M]. 北京:科学出版社,1993:83)
[9] Li M Q,Cai Z C,He X Y. Electrochemical study of 16Mn steel under H2S thin electrolyte film[J]. Mater. Prot., 2006,39(1):1-5
(李明齐,蔡铎昌,何晓英. H2S薄层液膜下16Mn钢腐蚀的电化学研究[J]. 材料保护,2006,39(1):1-5)
[10] Cao C N. Corrosion Electrochemistry[M]. Beijing: Chemistry Industry Press,1995,14
(曹楚南.腐蚀电化学[M].北京:化学工业出版社,1995,14)
[11] Li G M,Liu L W,Zheng J T. Corrosion behavior of carbon steel in high pressure dioxide saturated NaCl solutions containing hydrogen sulfide[J]. J. Chin. Soc. Corros. Prot.,2000,20(4):204-209
(李国敏,刘烈伟,郑家棠.碳钢在硫化氢及高压二氧化碳饱 和的NaC1溶液中的腐蚀行为[J].中国腐蚀与防护学报, 2000,20(4):204-209)
[12] Ma H Y,Cheng X L,Li G Q,et al. The influence of hydrogen sulfide on corrosion of iron under different conditions[J]. Corros.Sci.,2000,42(10):1669-1683

 

[1] 刘婉颖, 李磊, 朱鑫宇, 张智, 丁剑, 刘芃, 宋卓颖, 范祚媛. 掺氢天然气管线钢氢脆的多维因素与检测防护技术研究进展[J]. 中国腐蚀与防护学报, 2026, 46(5): 1400-1414.
[2] 臧勃林, 吴昊, 殷文昌, 杨艳冬, 田会云, 崔中雨. 阴极极化对两种高强度Ni-Cr-Mo-V钢氢脆行为的影响[J]. 中国腐蚀与防护学报, 2026, 46(5): 1527-1536.
[3] 徐云峰, 程凯源, 黄峰, 杨宝齐, 程向龙, 昝启飞, 彭志贤, 刘静. 预充氢时间对不同显微组织无缝钢管钢高压氢脆敏感性影响[J]. 中国腐蚀与防护学报, 2026, 46(3): 787-797.
[4] 谢睿, 蒋全通, 韩东晓, 陈烨, 刘万鹏, 裴炎彤, 段继周, 侯保荣. Al-10%RE (RE = Ce、Nd、Y、La)合金在典型海洋大气环境下的腐蚀行为研究[J]. 中国腐蚀与防护学报, 2026, 46(2): 365-380.
[5] 韩宇, 徐松, 华思然, 赵鹏, 王晓杰, 夏晓健, 张俊喜. 热镀锌层合金相的耐蚀性差异研究[J]. 中国腐蚀与防护学报, 2026, 46(2): 558-566.
[6] 岳远广, 尹志彪, 张子月, 江社明, 张启富. 一种大气腐蚀实时监测装置的开发及其在不同环境中的应用[J]. 中国腐蚀与防护学报, 2026, 46(1): 308-314.
[7] 李兆南, 侯禹岑, 莒鹏, 庄铁钢, 陈景杰, 王明昱, 徐云泽. 模拟液滴电导率变化对碳钢大气腐蚀的影响机制研究[J]. 中国腐蚀与防护学报, 2025, 45(6): 1537-1548.
[8] 项琦峰, 赵阳, 张涛, 王福会. 模拟浅海及深海环境中阴极极化对10CrNi5MoV钢氢脆敏感性的影响[J]. 中国腐蚀与防护学报, 2025, 45(6): 1599-1609.
[9] 冯宇芹, 郭同翰, 余韦汉, 吴伟, 张大全. Sb对高强结构钢在东海环境中腐蚀行为的影响[J]. 中国腐蚀与防护学报, 2025, 45(5): 1300-1308.
[10] 李秋博, 苏一喆, 吴伟, 张俊喜. 自源性磁场对Cu大气腐蚀行为的影响[J]. 中国腐蚀与防护学报, 2025, 45(4): 956-964.
[11] 诸滔, 孙浩翔, 周亚洪, 赵宇航, 王艳飞. 氢扩散模型对临氢结构裂尖氢浓度计算影响[J]. 中国腐蚀与防护学报, 2025, 45(4): 1070-1080.
[12] 彭文山, 辛永磊, 温杰平, 侯健, 孙明先. 极地冰覆盖下变温和恒温对高强钢腐蚀影响研究[J]. 中国腐蚀与防护学报, 2025, 45(3): 821-826.
[13] 王明洋, 夏大海. 高强铝合金氢脆机理研究进展[J]. 中国腐蚀与防护学报, 2025, 45(2): 261-270.
[14] 张倩茹, 孙擎擎. 氢促进局部塑性变形理论的发展趋势[J]. 中国腐蚀与防护学报, 2025, 45(2): 271-282.
[15] 崔博伦, 赵杰, 吕冉, 李敬法, 宇波, 闫东雷. 掺氢天然气输送管材氢脆与腐蚀复合防护技术研究进展[J]. 中国腐蚀与防护学报, 2025, 45(2): 327-337.