X70管线钢近中性环境氢致开裂与阳极溶解的关系
邵绪分
北京科技大学
Relations between Hydrogen-induced Cracking and Anode Dissolution of Pipeline Steel X70 in Near-neutral Environment
北京科技大学
引用本文:

邵绪分 . X70管线钢近中性环境氢致开裂与阳极溶解的关系[J]. 中国腐蚀与防护学报, 2008, 28(2): 76-80 .

全文: PDF(1127 KB)  
摘要: 采用慢速率拉伸试验(SSRT)方法及电化学测量技术,研究了阴极电位下X70钢在某种近中性介质中的应力腐蚀开裂(SCC)机理。试验表明,在近中性介质中,随着电位的降低,管线钢的SCC敏感性增强,但当电位低于某一范围后,SCC敏感性减弱;随着溶液pH值的降低,管线钢的腐蚀速率增大,敏感电位区间负移。分析表明,在近中性介质中,管线钢应力腐蚀开裂主要受阳极溶解和氢致开裂两种机理的联合作用,氢的渗入可能与氢的还原过程及管线钢阳极溶解密切相关。适宜的电位可以使阳极溶解和氢的联合作用增强,增强应力腐蚀开裂倾向。
关键词 : 应力腐蚀开裂,  阳极溶解,  氢致开裂,  X70管线钢    
Abstract:Stress corrosion cracking (SCC) mechanism of pipeline steel X70 has been investigated in a solution of near-neutral pH by means of slow strain rate test and electrochemical test technology. The experiments showed that SCC susceptibility increased as the applied potential shifted in the cathodic direction, but when the potential was lower than the extent of susceptive potential, SCC susceptibility depressed. Besides, the susceptive potential became more negative as the pH value decreased and corrosion rate increased. The analysis showed that hydrogen-induced cracking together with anode dissolution played an important role in the SCC of pipeline steel X70. However, anode dissolution and hydrogen-induced cracking did not work separately. Hydrogen permeation was related to the process of hydrogen deoxidization and the anode dissolution at specimen surface. Relevant potential was able to make the two mechanisms combined to cause much more serious SCC.
Key words: Stress Corrosion Cracking    Anode dissolution    Hydrogen-induced Cracking
收稿日期: 2006-09-12     
[1]Parkins R N,Blanchard Jr.W K,Delanty B S.Transgranularstress corrosion cracking of high pressure pipelines in contact withsolutions of near neutral pH[J].Corrosion,1994,50(5):394-408
[2]Parkins R N.A review of stress corrosion cracking of high pressuregas pipelines[R].in Corrosion/2000,NACE International,Hous-ton,TX,2000,363
[3]Guo H,Li G F,Cai X,et al.Effect of applied potentials on stresscorrosion cracking of X70 pipeline steel in near neutral pH solu-tions[J].J.Chin.Soc.Corros.Prot.,2004,24(4):208-212(郭浩,李光福,蔡珣等.外加电位对X70管线钢在近中性pH值溶液中的应力腐蚀开裂的影响[J].中国腐蚀与防护学报,2004,24(4):208-212)
[4]Sutcliffe J M,Fessler R R,Boyd W K et al.Stress corrosion crack-ing of carbon steel in carbonate solutions[J].Corrosion,1972,28(8):313-320
[5]Li M X,Wang R,Li P L.Crack propagation quantitative modelsof X70 pipeline steel in the synthetic soil solution[J].J.Chin.Soc.Corros.Prot.,2004,24(3):163-166(李明星,王荣,李鹏亮.X70管线钢在模拟土壤介质中裂纹扩展量化模型[J].中国腐蚀与防护学报,2004,24(3):163-166)
[6]Wang Z F,Atrens A.Initiation of stress corrosion cracking forpipeline steels in a carbonate-bicarbonate solution[J].Metall.Mater.Trans.A:,1996,27A(9):2686-2691
[7]Kushida T,Nose K,Asahi H,et al.Effects of metallurgical fac-tors and test conditions on near neutral pH SCC of pipeline steels[R].Houston,TX:NACE International,2001,1213
[8]Rebak R B,Xia Z,Safruddin R et al.Effect of solution composi-tion and electrochemical potential on stress corrosion cracking ofX-52 pipeline steel[J].Corrosion,1996,52(5):396-405
[9]Parkins R N,Blanchard W K,Delanty B S.Transgranular stresscorrosion cracking of high-pressure pipelines in contact with solu-tions of near neutral pH[J].Corrosion,1994,50(5):394-408
[10]Gu B,Yu W Z,Luo J L,et al.Transgranular stress corrosioncracking of X280 and X52 pipeline steels in dilute aqueous solu-tion with near-neutral pH[J].Corrosion,1999,55(3):312-319
[11]Li H L.Highlights of research and application of gas transmittingpipeline[J].Welded Pipe,2000,23(3):43-38(李鹤林.天然气输送钢管研究与应用中的几个热点问题[J].焊管.2000,23(3):43-38)
[12]Harle B A,Beavers J A,Jaske C E.Technical note:Low pHstress corrosion crack propagation in APIX65 line pipe steel[J].Corrosion,1993,49(10):861-863
[13]Zhao Y,Wang R.An investigation on mechanical behaviors of pipeline X70 after electrochemical hydrogen charging[J].J.Chin.Soc.Corros.Prot.,2004,24(5):293-296(赵颖,王荣.X70管线钢电化学充氢后的力学行为[J].中国腐蚀与防护学报,2004,24(5):293-296)
[14]Zha Q X,et al.Electrode Process Kinetics Introduction(the Third Edition)[M].Beijing:Science Press,2002,238(查全性等.电极过程动力学导论(第三版)[M].北京:科学出版社,2002,238)
[1] 许佳程, 刘家兵, 黄诗雨, 金灵好, 谭伟, 郭娜, 刘涛. 人工极地海域环境致EH40船板钢的力学性能损伤与应力腐蚀行为研究[J]. 中国腐蚀与防护学报, 2026, 46(5): 1437-1451.
[2] 贾梦瑶, 张伟强, 王媛, 谭季波, 邱建科, 郝延天, 吴欣强. 在3.5%NaCl溶液中压力变化对Ti80合金应力腐蚀行为的影响[J]. 中国腐蚀与防护学报, 2026, 46(5): 1508-1516.
[3] 王磊, 陶泽宇, 刘锋, 匡文军, 马鑫, 姚尧, 张国威. 水化学工况对四代核电直流蒸汽发生器用T22钢应力腐蚀开裂行为的影响[J]. 中国腐蚀与防护学报, 2026, 46(4): 1067-1080.
[4] 李兴斌, 雷蕴博, 高栋, 于泽, 董福宇, 周宇. 动态塑性变形对商用纯钛微观结构和氢致开裂行为的影响[J]. 中国腐蚀与防护学报, 2026, 46(2): 583-589.
[5] 兰博韬, 吴斌, 明洪亮, 王俭秋, 韩恩厚. 选区激光熔化奥氏体不锈钢高温高压水中应力腐蚀开裂行为研究进展[J]. 中国腐蚀与防护学报, 2026, 46(1): 1-14.
[6] 张德平, 闫立震, 于洋, 杨广明, 代春宇, 孟乐, 徐博, 刘智勇. CO2 驱采油井复杂环境中N80油管断裂失效机理[J]. 中国腐蚀与防护学报, 2025, 45(6): 1698-1708.
[7] 诸滔, 孙浩翔, 周亚洪, 赵宇航, 王艳飞. 氢扩散模型对临氢结构裂尖氢浓度计算影响[J]. 中国腐蚀与防护学报, 2025, 45(4): 1070-1080.
[8] 白云龙, 冷冰, 韦博鑫, 董立谨, 于长坤, 许进, 孙成. 掺氢天然气管材及焊缝的氢损伤行为研究进展[J]. 中国腐蚀与防护学报, 2025, 45(2): 283-295.
[9] 苏志诚, 张弦, 程焱, 刘静, 吴开明. 同成分的超细贝氏体钢和Q&P钢在海水中应力腐蚀开裂行为对比研究[J]. 中国腐蚀与防护学报, 2024, 44(6): 1495-1506.
[10] 张颛利, 戴海龙, 张喆, 石守稳, 陈旭. HF溶液中316L应力腐蚀开裂行为研究[J]. 中国腐蚀与防护学报, 2024, 44(6): 1633-1640.
[11] 刘久云, 董立谨, 张言, 王勤英, 刘丽. 油气田异种金属焊接接头硫化物应力腐蚀开裂研究进展[J]. 中国腐蚀与防护学报, 2024, 44(4): 863-873.
[12] 裴莹莹, 管方, 董续成, 张瑞永, 段继周, 侯保荣. Desulfovibrio Bizertensis SY-1在阴极极化条件下对X70 管线钢的腐蚀行为研究[J]. 中国腐蚀与防护学报, 2024, 44(2): 345-354.
[13] 原玉, 向勇, 李晨, 赵雪会, 闫伟, 姚二冬. CCUS系统中CO2 注入井管材腐蚀研究进展[J]. 中国腐蚀与防护学报, 2024, 44(1): 15-26.
[14] 李双, 董立谨, 郑淮北, 吴铖川, 王洪利, 凌东, 王勤英. 飞机起落架用超高强钢应力腐蚀开裂研究进展[J]. 中国腐蚀与防护学报, 2023, 43(6): 1178-1188.
[15] 郭昭, 李晗, 崔中雨, 王昕, 崔洪芝. A100钢在动态薄液膜和人工海水环境中的应力腐蚀行为对比研究[J]. 中国腐蚀与防护学报, 2023, 43(6): 1303-1311.