Please wait a minute...
中国腐蚀与防护学报  2008, Vol. 28 Issue (2): 70-75          
  研究报告 本期目录 | 过刊浏览 |
氢对纳米不锈钢涂层钝化膜性能的影响
叶威
中科院金属研究所
Effects of Hydrogen on Passive Film of Nanocrystallized Stainless Steel Coating
中科院金属研究所
引用本文:

叶威 . 氢对纳米不锈钢涂层钝化膜性能的影响[J]. 中国腐蚀与防护学报, 2008, 28(2): 70-75 .

全文: PDF(1523 KB)  
摘要: 用动电位极化、恒电位极化、Mott-Schottky测量、X射线光电子能谱(XPS)分析及扫描电子显微镜(SEM)等手段研究了氢对纳米不锈钢涂层在0.5 mol/L NaCl + 0.05 mol/L H2SO4溶液中腐蚀行为及钝化膜性能的影响。结果表明,氢与涂层表面吸附的OH-反应使OH- 吸附减少,从而延迟了钝化膜的形成;氢使钝化膜的成分发生改变,钝化膜中的OH-/O2-的比率升高,因而钝化膜的点蚀敏感性增加;同时,氢促使钝化膜的介电常数增大,空间电荷电容增大,载流子密度增加,从而降低了钝化膜的稳定性。随着充氢量的增加,钝化膜的维钝电流和载流子密度随之增加,说明钝化膜的稳定性和涂层耐蚀性能都随之降低。
关键词 : 氢,  纳米不锈钢涂层,  钝化膜,  电子性能    
Abstract:The effects of hydrogen on corrosion behavior and passive film of nano-crystalline stainless steel coat?鄄ing in 0.5 mol/L NaCl + 0.05 mol/L H2SO4 solution were investigated using electrochemical technique, X-ray photoelectron spectroscopy (XPS) analysis and scanning electron microscopy (SEM) observation. During the for?鄄mation process of passive film, the hydrogen could slow down the formation of the passive film because the exis?鄄tence of hydrogen would reduce the adsorbed OH- ions on the coating surface. XPS analysis results indicated that the OH-/O2- ratio in the passive film was changed after hydrogen charging. The susceptibility to pitting of the charged coating was enhanced because of the increment of OH-/O2- ratio in the passive film.Mott-Schottky analy?鄄sis showed that the hydrogen protons could enhance the dielectric constant of the passive film and account for the increase in capacitance and carrier density of passive films. In addition, the passive current density decreased and the carrier densities increased with the increment of hydrogen charging current.
Key words:
收稿日期: 2006-07-21     
[1]Yang M Z,Luo J L,Yang Q,et al.Effects of hydrogen on semi-conductivity of passive films and corrosion behavior of 310 stain-less steel[J].J.Electrochem.Soc.,1999,146:2107-2122
[2]Yu J G,Luo J L,Norton P R.Effects of hydrogen on the electronicproperties and stability of the passive films on iron[J].Appl.Surf.Sci.,2001,177:129-138
[3]Hasegawa M,Osawa M.Anomalous corrosion of hydrogen-contain-ing ferritic steels in aqueous acid solution[J].Corrosion,1983,39:115-120
[4]Yang M Z,Qiao J L,Chiovelli S,et al.Critical hydrogen charging conditions for martensite transformation and surface cracking intype 304 stainless steel[J].Scr.Mater.,1999,40:1209-1214
[5]Pyun S I,Lim C,Oriani R A.The role of hydrogen in the pitting of passivating films on pure iron[J].Corros.Sci.,1992,33:437-444
[6]Ryan M P,Laycock N J,Issaacs H S,et al.Corrosion pits in thinfilms of stainless steel[J].J.Electrochem.Soc.,1999,146:91-97
[7]Wang X Y,Li.D Y.The influence of electrolyte reduction poten-tial on weld corrosion[J].Electrochim.Acta,2002,47:3939-3947
[8]Ye W,Li Y,Wang F H.Effects of nanocrystallization on the cor-rosion behavior of 309 stainless steel[J].Electrochim.Acta,2006,51:4426-4432
[9]Cao C N.The Principle of the Corrosion Electrochemistry[M].Beijing:Chemical Industry Press,2004(曹楚南.腐蚀电化学原理[M].北京:化学工业出版社,2004)
[10]Femenia M,Pan J,Leygraf C,et al.In situ study of selective dis-solution of duplex stainless steel 2205 by electrochemical scanningtunneling microscopy[J].Corros.Sci.,2001,43:1939-1951
[11]Okamoto G,Shibata T.Stability of passive stainless steel in rela-tion to the potential of passivation treatment[J].Corros.Sci.,1970,10:371-378
[12]Engell H J.Stabilityand breakdown phenomena of passivatingfilms[J].Electrochim.Acta,1977,22:987-993
[13]Fugassi P,Haney E G.Titanium Science and Technology(JaffeeR I,Burte H M,eds)[M].New York:Plenum Press,1973,2611
[14]McBee C L,Kruger J.Localized Corrosion[A].Corrosion/74[C].Houston,TX:NACE,1974,252
[15]Yu J G,Luo J L,Norton P R.Electrochemical investigation ofthe effects of hydrogen on the stability of the passive film on iron[J].Electrochim.Acta,2002,47:1527-1536
[1] 刘婉颖, 李磊, 朱鑫宇, 张智, 丁剑, 刘芃, 宋卓颖, 范祚媛. 掺氢天然气管线钢氢脆的多维因素与检测防护技术研究进展[J]. 中国腐蚀与防护学报, 2026, 46(5): 1400-1414.
[2] 臧勃林, 吴昊, 殷文昌, 杨艳冬, 田会云, 崔中雨. 阴极极化对两种高强度Ni-Cr-Mo-V钢氢脆行为的影响[J]. 中国腐蚀与防护学报, 2026, 46(5): 1527-1536.
[3] 赵先锐, 戴中国, 李战江, 徐育烺, 张会霞, 李旺. 添加Y、Hf对AlCoCrFeNi高熵合金涂层在NaCl溶液中的腐蚀行为的影响[J]. 中国腐蚀与防护学报, 2026, 46(5): 1549-1559.
[4] 党桂铭, 陈锴, 吕良, 杜一帆, 高浩然, 郑树启. 拉伸变形与氢渗透动态协同作用下X65钢的氢扩散行为研究[J]. 中国腐蚀与防护学报, 2026, 46(5): 1619-1626.
[5] 黄涛, 朱宇, 邓宇, 王岐山, 田一晨, 陈旭. 氢对X65钢及其焊缝力学性能及腐蚀行为影响[J]. 中国腐蚀与防护学报, 2026, 46(4): 1107-1116.
[6] 周炜龙, 郭玉冰, 胡梦茹, 沈凯杰, 杨正桓, 谢林君. 磷酸钠浓度对40Cr钢耐蚀性能的影响[J]. 中国腐蚀与防护学报, 2026, 46(4): 1185-1196.
[7] 张晶晶, 张震, 赵占勇, 白培康, 周杰. NaHSO3 添加对445J2铁素体不锈钢在NaCl溶液中腐蚀行为影响研究[J]. 中国腐蚀与防护学报, 2026, 46(4): 1197-1206.
[8] 刘状, 乔创, 姜金利, 车欣, 代春丽, 沈勇, 郝龙. 电镀锡板表面Cr2O3 钝化膜结构及耐蚀性演化的电化学阻抗谱研究[J]. 中国腐蚀与防护学报, 2026, 46(3): 756-766.
[9] 徐云峰, 程凯源, 黄峰, 杨宝齐, 程向龙, 昝启飞, 彭志贤, 刘静. 预充氢时间对不同显微组织无缝钢管钢高压氢脆敏感性影响[J]. 中国腐蚀与防护学报, 2026, 46(3): 787-797.
[10] 刘凡, 刘凤莲, 范松海, 邵千秋, 周凯, 李泽瑞, 陈熠东, 文柯成, 张静. 自由基对高压电缆中间接头析氢腐蚀过程的影响[J]. 中国腐蚀与防护学报, 2026, 46(3): 919-930.
[11] 赖漾, 徐清亮, 罗群, 李谦. 酸洗致基板表面状态变化对镀锡板耐蚀性的影响[J]. 中国腐蚀与防护学报, 2026, 46(2): 393-404.
[12] 李兴斌, 雷蕴博, 高栋, 于泽, 董福宇, 周宇. 动态塑性变形对商用纯钛微观结构和氢致开裂行为的影响[J]. 中国腐蚀与防护学报, 2026, 46(2): 583-589.
[13] 严建成, 冯向东, 卢得勇, 李进, 孟鹏军, 娄宝辉, 郭健, 李正涛, 朱正旺. 一种Cu-Zn基高熵合金在硬水中的腐蚀行为研究[J]. 中国腐蚀与防护学报, 2026, 46(2): 601-610.
[14] 衣俊达, 冷傲, 宫得伦, 韦博鑫. 低模量耐腐蚀亚稳 β 钛合金的电子束增材制造与性能研究[J]. 中国腐蚀与防护学报, 2026, 46(1): 49-59.
[15] 谷清宇, 宋雁飞, 张亮亮, 王楠, 雷晓维. 激光定向能量沉积17-4PH不锈钢钝化与点蚀行为研究[J]. 中国腐蚀与防护学报, 2026, 46(1): 103-114.