西部油田油管腐蚀结垢机理研究
万里平;孟英峰
中国石油天然气集团公司石油管材研究所
MECHANISM OF CORROSION AND SCALE DEPOSIT OF TUBES IN WESTERN OILFIELD
;
中国石油天然气集团公司石油管材研究所
引用本文:

万里平; 孟英峰 . 西部油田油管腐蚀结垢机理研究[J]. 中国腐蚀与防护学报, 2007, 27(4): 247-251 .
, . MECHANISM OF CORROSION AND SCALE DEPOSIT OF TUBES IN WESTERN OILFIELD[J]. J Chin Soc Corr Pro, 2007, 27(4): 247-251 .

全文: PDF(316 KB)  
摘要: 通过对西部某油田油管腐蚀结垢现状调查、单井采出液成分分析和垢样XRD分析,结合油管结垢趋势预测及室内高温高压腐蚀试验,探讨了油管腐蚀结垢机理。结果表明:垢物主要是CaCO3、CaSO4和铁锈产物,在结垢出现的同时伴随油管腐蚀的发生。影响油管腐蚀结垢的主要因素是采出液中含有丰富的的Ca2+、HCO3-、Cl-以及原油伴生气中的CO2含量较多。该油田存在严重的腐蚀结垢趋势。
关键词 : 腐蚀,  结垢,  油管,  防腐,  防垢    
Abstract:Corrosion and scale deposit reasons of tubes were discussed, through the in-situ investigation, pro?鄄duced water composition analysis, XRD analysis of scaling samples of single well in Western oilfield, combining scaling prediction and corrosion rate monitor. The results show that scaling types are mainly CaCO3?CaSO4 and iron rust, scaling in connection with corrosion. Predominating factors affecting corrosion and scaling of tubing are abundant in Ca2+?HCO3-?Cl- containing in produced water and CO2 exiting in accompanying gas with crude oil. Severe corrosion and scaling of tubes were found in this oilfield.
Key words: corrosion    scale deposit    tube    anti-corrosion    scaling control
收稿日期: 2006-02-21     
ZTFLH:  TG172  
[1]Zhang Y,Zhang N S,Wu J Q.Scaling prediction and software devel-opment in Huachi oilfield[J].Special Oil&Gas Reservoir,2004,11(6):100-102(张益,张宁生,吴金桥.华池油田结垢预测及软件开发[J].特种油气藏,2004,11(6):100-102)
[2]Li J P,Zhao G X,Hao S M.The study on static corrosion of oil thimble used in Tarim oil field[J].J.Chin.Soc.Corros.Prot.,2004,24(4):230-233(李建平,赵国仙,郝士明.塔里木油田用油套管钢的静态腐蚀研究[J].中国腐蚀与防护学报,2004,24(4):230-233)
[3]Wu S L,Cui Z D,Li C F.Study on corrosion of oil tubes in carbon dioxide saturated crude oil/water mixtures[J].J.Chin.Soc.Corros.Prot.,2003,23(6):340-344(吴水林,崔振铎,李春福等.油管钢在饱和二氧化碳模拟油田液中的腐蚀研究[J].中国腐蚀与防护学报,2003,23(6):340-344)
[4]Nesi S,John P,Vrhova M.CO2corrosion of carbon steel-from mech-anism to empirical modeling[J].Corros.Rev.,1997,15:112-126
[5]Eugenio L P,Lucrezia S.Corrosion and environmental cracking e-valution of high density brines for use in HPHT fields[A].SPE97593High Pressure/High Temperature Sour Well Design Application Technology Workshop[C].The Woodland,Texas,2005,5
[6]Gunaltun Y.Carbon dioxide corrosion in oil wells[A].Middle East Oil Show[C].SPE21330Bahrain,1991,11
[7]Skillman H F,McDonald J P,Stiff H A.A simple,accurate,fast method for calculating calcium sulfate solubility in oilfield brine[A].API Spring Meeting of the Southwestern District[C].Texas,1969,3
[8]Zhu Y W,Zhao Z Z,Ju Q Y.Scaling Mechanism and Prevention Technology of Oilfield Development[M].Xi'an:Science Technology Press of Shannxi,1995(朱义吾,赵作滋,巨全义.油田开发中的结垢机理及其防治技术[M].西安:陕西科学技术出版社,1995)
[9]Chen D C,Liu J R,Wu X D.Models for predicting paraffin deposi-tion profile in waxy oil wellbore[J].J.Univ.Petroleum China,1999,23(4):36-39(陈德春,刘均荣,吴晓东.含蜡原油井筒结蜡剖面的预测模型[J].石油大学学报,1999,23(4):36-39)
[10]Yin X Q,Wu J Z,Wang Z L.Analysis and prediction of scaling mechanism of CaCO3from oilfield injection waters[J].PetroleumExploration and Development,2002,29(3):85-87(尹先清,伍家忠,王正良.油田注入水碳酸钙垢结垢机理分析与结垢预测[J].石油勘探与开发,2002,29(3):85-87)
[11]DuZG.ResearchondescalingandanticorrosionofwellboreinQian-miqiao oilfield[D].Chengdou:Southwest Petroleum University,2002(杜志广.千米桥地区井筒除垢防腐技术研究[D].成都:西南石油大学,2002)
[1] 黎敏, 魏高飞, 邓书端, 李向红. 扫描电化学显微镜(SECM)在缓蚀剂研究中的进展与展望[J]. 中国腐蚀与防护学报, 2026, 46(5): 1326-1342.
[2] 谢敬礼, 王友志, 乔书振, 牛佳雨, 郝龙, 曹胜飞, 王俭秋. 高放废物地质处置库近场环境中碳钢腐蚀产物演化研究进展[J]. 中国腐蚀与防护学报, 2026, 46(5): 1343-1352.
[3] 周书宇, 刘昌璞, 杨留洋, 耿杰, 范海明, 张大磊, 鞠虹. 在超临界CO2 工况和典型环境因素共影响下的管线钢腐蚀及防护技术研究进展[J]. 中国腐蚀与防护学报, 2026, 46(5): 1353-1368.
[4] 黄绘, 李树丽, 邓书端, 李向红. 自修复材料在防护涂层中的研究进展及展望[J]. 中国腐蚀与防护学报, 2026, 46(5): 1369-1388.
[5] 曾崎, 虞文军, 门向南, 冯保净, 杨耀, 朱凯, 葛玉麟, 应韬, 曾小勤. 高强耐蚀稀土镁合金研究进展[J]. 中国腐蚀与防护学报, 2026, 46(5): 1415-1424.
[6] 张强, 卢壹梁, 金焱, 陈云, 杨丙坤, 王晓芳, 韩钰. 环境腐蚀性分级及大气/土壤腐蚀性地图绘制技术研究进展[J]. 中国腐蚀与防护学报, 2026, 46(5): 1425-1436.
[7] 许佳程, 刘家兵, 黄诗雨, 金灵好, 谭伟, 郭娜, 刘涛. 人工极地海域环境致EH40船板钢的力学性能损伤与应力腐蚀行为研究[J]. 中国腐蚀与防护学报, 2026, 46(5): 1437-1451.
[8] 郑凯, 王艺陶, 王东胜, 刘伟, 蒋颖畅, 黄嵘, 常雪婷. 腐蚀-应力耦合作用对极地船用螺旋桨低碳马氏体不锈钢失效机理影响研究[J]. 中国腐蚀与防护学报, 2026, 46(5): 1452-1462.
[9] 齐晓涵, 翟海民, 李文生, 洪昊, 曹元, 俞雷, 陈博瀚. Al2O3 磨加量对铝合金搪瓷涂层组织结构及腐蚀性能的影响[J]. 中国腐蚀与防护学报, 2026, 46(5): 1497-1507.
[10] 贾梦瑶, 张伟强, 王媛, 谭季波, 邱建科, 郝延天, 吴欣强. 在3.5%NaCl溶液中压力变化对Ti80合金应力腐蚀行为的影响[J]. 中国腐蚀与防护学报, 2026, 46(5): 1508-1516.
[11] 李晓峰, 李艳茹, 卢云飞, 张泰华, 常雪婷, 安燕. 力学与防腐性能协同增强的聚吡咯改性芳纶纤维/环氧复合涂料[J]. 中国腐蚀与防护学报, 2026, 46(5): 1517-1526.
[12] 曹天慧, 杨砚淇, 刘雨薇, 吴磊, 郭泉忠, 贾志刚, 曹公望, 汪川. 23MnNiMoCr54钢在不同pH的模拟高矿化水中腐蚀机理研究[J]. 中国腐蚀与防护学报, 2026, 46(5): 1537-1548.
[13] 赵先锐, 戴中国, 李战江, 徐育烺, 张会霞, 李旺. 添加Y、Hf对AlCoCrFeNi高熵合金涂层在NaCl溶液中的腐蚀行为的影响[J]. 中国腐蚀与防护学报, 2026, 46(5): 1549-1559.
[14] 王兴斌, 李家民, 伍登骏, 唐伟能, 杨静, 郭嘉成, 杨欣宇, 侯娟. Al含量对Mg-xAl-Zn合金耐腐蚀性能的影响[J]. 中国腐蚀与防护学报, 2026, 46(5): 1560-1568.
[15] 叶海锋, 沈书成, 陈江华. 增材制造316L不锈钢在不同温度海水环境中的腐蚀行为研究[J]. 中国腐蚀与防护学报, 2026, 46(5): 1569-1578.