Please wait a minute...
中国腐蚀与防护学报  2006, Vol. 26 Issue (2): 80-84          
  研究报告 本期目录 | 过刊浏览 |
X70钢在磷酸盐缓冲溶液中的孔蚀电化学行为研究
毛健鹏;唐聿明;左禹*
北京化工大学材料科学与工程学院
The Electrochemical Characteristics of Pitting of X70 Pipeline Steel
Jian Peng Mao;Yuming Tang;Yu Zuo
北京化工大学材料科学与工程学院
引用本文:

毛健鹏; 唐聿明; 左禹* . X70钢在磷酸盐缓冲溶液中的孔蚀电化学行为研究[J]. 中国腐蚀与防护学报, 2006, 26(2): 80-84 .
, , . The Electrochemical Characteristics of Pitting of X70 Pipeline Steel[J]. J Chin Soc Corr Pro, 2006, 26(2): 80-84 .

全文: PDF(167 KB)  
摘要: 研究了X70钢在磷酸盐缓冲溶液中的亚稳态与稳态孔蚀的电化学行为特征。发现Cl-浓度对X70钢在磷酸盐缓冲溶液中的孔蚀保护电位影响不大,而PO43-对X70钢有较强的孔蚀抑制作用,增加PO43-浓度,能够有效提高X70钢的孔蚀保护电位。提高缓冲溶液的pH值能够抑制X70钢小孔的形核和生长。X70钢亚稳态小孔形核主要受到铝氧夹杂物的影响, 且随着电位的升高,电流波动频率先升高后降低,而峰值电流则趋于增大。X70钢在磷酸盐缓冲溶液中形成的钝化膜在钝化区内阻抗基本不受电位的影响。
关键词 : 孔蚀,  亚稳态孔蚀,  电流波动,  X70钢,  交流阻抗    
Abstract:The Electrochemical Characteristics of pitting of X70 Pipeline Steel in Phosphate Buffer Solution are studied in this paper. It is found that the effect of Cl- ions on pitting protection potential is neglectable. PO43- ions show strong inhibition on nucleation and the growth of pitting. Impurity and the surface grooves left by polishing result in the nucleation and the growth of metastable pitting. The nucleation frequency increases at first and then decreases with potential, while peak current increases continually. In the potential range of metastable pitting, the impedance of passive film keeps almost unchanged with potential. However, the impedance shows an obvious decrease when potential is above pitting potential Eb.
Key words: pitting    metastable pitting    current fluctuations    X70 steel    EIS
收稿日期: 2005-01-13     
ZTFLH:  TG174  
[1]Frankel G S,Stockert L,Hunkeler F,et al.Metastable pitting ofstainless steel[J].Corrosion,1987,43(7):429-436
[2]Pistorius P C,Burstein G T.Growth of corrosion pits on stainlesssteel in chloride solution containing dilute sulphate[J].Corros.Sci.,1992,33(12):1885-1897
[3]Pistorious P C,Burstein G T.Aspects of the effects of electrolytecomposition on the occurrence of metastable pitting on stainlesssteel[J].Corros.Sci.,1994,36(3):255-261
[4]Cheng Y F,Luo J L.Metastable pitting of carbon steel under potentio-static control[J].J.Electrochem.Soc.,1999,146(3):970-978
[5]Cheng Y F,Wilmott M,Luo J L.Analysis of the role of electrodecapacitance on the initiation of pits for A516 carbon steel by elec-trochemical noise measurements[J].Corros.Sci.,1999,41:1245-1256
[6]Dong Z H,Guo X P,Zheng J S.Electrochemical noise characteris-tics of metastable pitting of 16Mn mild steel[J].Corros.Sci.Prot.Technol.,2001,13(4):195-201(董泽华,郭兴蓬,郑家焱木.用电化学噪声研究16Mn钢的亚稳态孔蚀特征[J].腐蚀科学与防护技术,2001,13(4):195-201)
[7]Tang Y M,Zuo Y.The metastable pitting of mild steel in bicar-bonate solutions[J].Materials Chemistry and Physics,2004,88(3):221-226
[8]Fujioka E,Nishihara H,Aramaki K.The inhibition of pit nucle-ation and growth on the passive surface of iron in a borate buffersolution coataining Cl-by oxidizing inhibitors[J].Corros.Sci.,1996,38(11):1915-1933
[9]Pistorius P C,Burstein G T.Surface roughness and the metastablepitting of stainless steel in chloride solutions[J].Corrosion,1995,51(5):380-385
[10]Wang H,Zuo Y,Mao J P.Metastable pitting and related morphol-ogy of pure iron in NaNO2+NaCl solution[J].J.Beijing Universi-ty of Chemical Technology,2004,31(5):41-43(王虎,左禹,毛健鹏.工业纯铁在NaNO2+NaCl溶液中的亚稳态孔蚀及其腐蚀形貌[J].北京化工大学学报,2004,31(5):41-43)
[11]Wei B M,Hao L.Physical characteristic of some non-semi-cricle AC depeadances[J].Total Corrosion Control,1990,4(3):9-15(魏宝明,郝凌.几种非正半圆交流阻抗图谱的物理意义[J].全面腐蚀控制,1990,4(3):9-15)
[1] 马欢欢, 吕晟东, 钱溢鑫, 林勇, 郝湘平, 张达威, 王鲁宁. 三水醋酸钠相变储热体系中铜换热管的局部腐蚀与寿命预测[J]. 中国腐蚀与防护学报, 2026, 46(4): 1045-1057.
[2] 吴宇航, 陈旭, 王首德, 刘畅, 刘杰. 直流电作用下X70钢在近中性土壤中应力腐蚀行为研究[J]. 中国腐蚀与防护学报, 2025, 45(2): 489-496.
[3] 李强, 路程, 唐颖浩, 唐建峰, 刘炳成. 湿气管道积液区X70钢CO2 局部腐蚀行为研究[J]. 中国腐蚀与防护学报, 2023, 43(4): 837-846.
[4] 冯丽, 张胜涛, 郑思远, 胡志勇, 朱海林, 马雪梅. 卤素阴离子对离子液体缓蚀性能的影响[J]. 中国腐蚀与防护学报, 2022, 42(5): 791-797.
[5] 李鸿瑾, 王歧山, 廖子涵, 孙祥锐, 孙晖, 张新阳, 陈旭. X70钢及其焊缝在含Cl-高pH值溶液中电化学噪声行为研究[J]. 中国腐蚀与防护学报, 2022, 42(1): 60-66.
[6] 林朝晖, 明南希, 何川, 郑平, 陈旭. 静水压力对X70钢在海洋环境中腐蚀行为影响研究[J]. 中国腐蚀与防护学报, 2021, 41(3): 307-317.
[7] 陈旭,马炯,李鑫,吴明,宋博. 温度与SRB协同作用下X70钢在海泥模拟溶液中应力腐蚀行为研究[J]. 中国腐蚀与防护学报, 2019, 39(6): 477-483.
[8] 李鑫,陈旭,宋武琦,杨佳星,吴明. pH值对X70钢在海泥模拟溶液中微生物腐蚀行为的影响[J]. 中国腐蚀与防护学报, 2018, 38(6): 565-572.
[9] 滕彧,陈旭,何川,王义闯,王冰. 显微组织对X70钢在含有硫酸盐还原菌的3.5%NaCl溶液中腐蚀行为的影响[J]. 中国腐蚀与防护学报, 2017, 37(2): 168-174.
[10] 蒋秀,宋晓良,屈定荣,刘小辉. X70钢输送气态和超临界状态CO2时的腐蚀行为研究[J]. 中国腐蚀与防护学报, 2016, 36(3): 225-230.
[11] 李阳恒,左禹,唐聿明,赵旭辉. 应变作用下Q235碳钢在NaHCO3+NaCl溶液中的孔蚀行为[J]. 中国腐蚀与防护学报, 2016, 36(3): 238-244.
[12] 刘彤, 张艳飞, 陈旭, 王丹, 陈宇, 王冠夫. SRB对X70钢在土壤模拟溶液中腐蚀行为的影响[J]. 中国腐蚀与防护学报, 2014, 34(2): 112-118.
[13] 石慧英,唐聿明,左禹. PO43-对304不锈钢在氯离子水溶液中小孔腐蚀形核过程的影响[J]. 中国腐蚀与防护学报, 2013, 33(1): 36-40.
[14] 张胜寒,檀玉,梁可心. 电化学阻抗谱法对304不锈钢孔蚀生长和再钝化阶段的原位研究[J]. 中国腐蚀与防护学报, 2011, 31(2): 130-134.
[15] 郜华萍,吴飞,龙晋明,介星迪,张冬平. 黄磷尾气燃气锅炉的腐蚀行为[J]. 中国腐蚀与防护学报, 2011, 31(1): 51-55.