Please wait a minute...
中国腐蚀与防护学报  2006, Vol. 26 Issue (1): 37-42          
  研究报告 本期目录 | 过刊浏览 |
304奥氏体不锈钢离子辐照后再活化性能测试和表面形貌观察
李红梅;刘杏;蔡珣;杨武
上海交通大学材料学院
Electrochemical Potentiokinetic Reactivation Measurement and Surface Feature Observation on Austenitic Stainless Steel Irradiated by High Energy He+ or Fe+ Ions
Hongmei Li;Xing Liu;Xun Cai;Wu Yang
上海交通大学材料学院
引用本文:

李红梅; 刘杏; 蔡珣; 杨武 . 304奥氏体不锈钢离子辐照后再活化性能测试和表面形貌观察[J]. 中国腐蚀与防护学报, 2006, 26(1): 37-42 .
, , , . Electrochemical Potentiokinetic Reactivation Measurement and Surface Feature Observation on Austenitic Stainless Steel Irradiated by High Energy He+ or Fe+ Ions[J]. J Chin Soc Corr Pro, 2006, 26(1): 37-42 .

全文: PDF(377 KB)  
摘要: 对核电用奥氏体不锈钢进行固溶和敏化处理,对部分固溶试样进行Fe+和He+辐照,随后测量了4种处理状态试样的再活化率(EPR),并观察表面形 貌.结果表明:经He+辐照试样出现了2.88%的再活化率,敏化试样的再活化率是19.5%,固溶试样和经Fe+辐照试样的再活化率为0.离子辐照试样的表面形貌与固溶或敏化试样完全不同.
关键词 : 不锈钢,  离子辐照,  再活化,  表面形貌    
Abstract:The effect of coating used to cover airplane on corrosion fatigue behaviour of LY12CZ aluminum alloy has been studied.The corrosion fatigue lives for uncoated and coated specimens in both air and 3.5% NaCl solution were compared,and the evolution of free corrosion potential with cyclic number was measured.The equations of fatigue and corrosion fatigue lives were obtained on some experiment conditions by quantitative analysis.The results showed that the corrosion fatigue life of LY12CZ aluminum alloy was greatly improved by coating.
Key words: Austenitic stainless steel    Ion irradiation    EPR    Surface appearance
收稿日期: 2004-09-15     
ZTFLH:  TG172  
[1]Yang W,Zhang M J,Zhao G Z.Stress corrosion cracking ofaustenitic stainless steel in high temperature water[J].Acta Metall.Sin.,1991,27(2):116-120(杨武,张美杰,赵国珍.304不锈钢在高温水中的应力腐蚀破裂[J].金属学报,1991,27(2):116-120)
[2]Yang W.Advances in research on irradiation assisted stress corro-sion cracking[J].Mater.Prot.,1994,27(2):1-4
[3]Was G S,Allen T.Intercomparison of microchemical evolution un-der various types of particle irradiation[J].J.Nuclear Mater.,1993,205:332-338
[4]Semenov A A,Woo C H.Stochastic fluctuations and microstructuralevolution during irradiation by neutrons and heavy ions[J].J.Nu-clear Mater.,1993,205:74-83
[5]Lee E L,Hunn J D,Hashimoto N,et al.Hardness and defect struc-tures in EC316LN austenitic alloy irradiated under a simulated spal-lation neutron source environment using triple ion-beams[J].J.Nuclear Mater.,2000,278:266-272
[6]Ahmet Cakir,Sabri Tuncell,Alptekin Aydin.AE response of 316LSS test under potentiostatic control[J].Corros.Sci.,1999,41:1175-1183
[7]Van N R.Electrochemical noise measurements under pressurizedwater reactor conditions[J].Corrosion,2000,56(2):161-166
[8]Kim Y J.In-situ electrochemical impedance measurement of oxidefilm formed on type 304 stainless steel in high-temperature water[J].Corrosion,2000,56(4):389-394
[9]Wan F R.Irradiation Damage of Metal Material[M].Beijing:Sci-ence Press,1993(万发荣.金属材料的辐射损伤[M].北京:科学出版社,1993)
[10]Wei B M.Corrosion Theory and Application of Metal[M].Beijing:Chemical Industry Press,1984(魏宝明主编.金属腐蚀理论及应用[M].北京:化学工业出版社,1984)
[11]Cao C N.Corrosion Electrochemistry[M].Beijing:Chemical In-dustry Press,1994(曹楚南编著.腐蚀电化学[M].北京:化学工业出版社,1994)
[12]Liu Y H,Zhang P F.Metal Corrosion Theory[M].Beijing:Pub-lishing Company of Aviation Industry,1993(刘永辉,张佩芬.金属腐蚀学原理[M].北京:航空工业出版社,1993)
[13]Xiao J M.Metal Corrosion Under Stress[M].Beijing:Chemical In-dustry Prss,1990(肖纪美著.应力作用下的金属腐蚀[M].北京:化学工业出版社,1990)
[14]Xiao J M.Metallurgy of Austenitic Stainless Steel[M].Beijing:Publishing Company of Metallurgical Industry,1993(肖纪美著.不锈钢的金属学问题[M].北京:冶金工业出版社,1993)
[15]Zhao W Z.New Surface Technique of Metal Material[M].Xi’an:Publishing Company of Xi’an Jiaotong University,1992(赵文珍编.金属材料表面新技术[M].西安:西安交通大学出版社,1992)
[16]Poate J M,Foti G,Jacobson D C.Surface Property Changing andAlloying[M].Beijing:Science Press,1988(J.M.波特,G.福蒂,D.C.雅各布森主编.表面改性与合金化[M].北京:科学出版社,1988)
[17]Liu J L,Zhou Z R,Su B R.Heat Treatment of High Energy Beam[M].Beijing:Publishing Company of Mechanical Industry,1997(刘江龙,邹至荣,苏宝容编著.高能束热处理[M].北京:机械工业出版社,1997)
[1] 郑凯, 王艺陶, 王东胜, 刘伟, 蒋颖畅, 黄嵘, 常雪婷. 腐蚀-应力耦合作用对极地船用螺旋桨低碳马氏体不锈钢失效机理影响研究[J]. 中国腐蚀与防护学报, 2026, 46(5): 1452-1462.
[2] 董少阳, 刘朝坤, 李昱彤, 夏忠虎, 甘浪, 李聪, 任延杰. 高速激光熔覆NiCrAlY涂层在900 ℃空气中的高温氧化行为[J]. 中国腐蚀与防护学报, 2026, 46(5): 1463-1474.
[3] 叶海锋, 沈书成, 陈江华. 增材制造316L不锈钢在不同温度海水环境中的腐蚀行为研究[J]. 中国腐蚀与防护学报, 2026, 46(5): 1569-1578.
[4] 何章平, 袁誉坤, 杜颖哲, 林鹏, 徐健. 在模拟电加热器过热条件下316LN奥氏体钢缝隙腐蚀行为的研究[J]. 中国腐蚀与防护学报, 2026, 46(5): 1579-1587.
[5] 刘夏城, 邹建荣, 高良文, 周龙, 谭季波, 吴欣强, 张兹瑜. 压水堆核电站不锈钢焊缝材料腐蚀疲劳模型[J]. 中国腐蚀与防护学报, 2026, 46(5): 1613-1618.
[6] 孙欣, 屈佳伟, 高子淋, 郑越, 马爱利, 姚琳, 张连民, 郑玉贵. Mn2+ 对304L和C25不锈钢在高温硝酸中腐蚀行为的协同作用机制与响应曲面模型研究[J]. 中国腐蚀与防护学报, 2026, 46(4): 1015-1030.
[7] 张晶晶, 张震, 赵占勇, 白培康, 周杰. NaHSO3 添加对445J2铁素体不锈钢在NaCl溶液中腐蚀行为影响研究[J]. 中国腐蚀与防护学报, 2026, 46(4): 1197-1206.
[8] 王彦峰, 王流火, 孙仕达, 刘琦, 李亚梅, 王显宗. 柔直换流阀冷却系统关键材料失效与缓解措施研究进展[J]. 中国腐蚀与防护学报, 2026, 46(3): 653-662.
[9] 张新瑞, 薛宝权, 谭季波, 张兹瑜, 高军, 吴欣强. 含铝奥氏体不锈钢液态铅铋环境相容性研究进展[J]. 中国腐蚀与防护学报, 2026, 46(3): 671-679.
[10] 陈旭, 刘宇航, 郭建, 王岐山, 刘畅, 刘彬. 超级13Cr不锈钢在饱和CO2 油田采出液中的缝隙腐蚀行为[J]. 中国腐蚀与防护学报, 2026, 46(2): 523-532.
[11] 杜乾, 马泽林, 恽迪, 顾龙, 郭少强. Fe离子辐照对ODS钢在饱和氧液态铅中腐蚀行为的影响[J]. 中国腐蚀与防护学报, 2026, 46(2): 567-575.
[12] 张金宇, 李欣, 张磊, 陈志华, 杜雨昕, 冯贺鑫, 张雪, 张洋鹏, 林如山, 李瑛, 戎利建. 几种17Cr系不锈钢在氯化物蒸汽中的腐蚀行为研究[J]. 中国腐蚀与防护学报, 2026, 46(2): 576-582.
[13] 兰博韬, 吴斌, 明洪亮, 王俭秋, 韩恩厚. 选区激光熔化奥氏体不锈钢高温高压水中应力腐蚀开裂行为研究进展[J]. 中国腐蚀与防护学报, 2026, 46(1): 1-14.
[14] 谷清宇, 宋雁飞, 张亮亮, 王楠, 雷晓维. 激光定向能量沉积17-4PH不锈钢钝化与点蚀行为研究[J]. 中国腐蚀与防护学报, 2026, 46(1): 103-114.
[15] 冯浩轩, 王馥丽, 李甲林, 杜瑶, 韦博鑫, 朱圣龙. SLM-316L不锈钢的高温氧化与腐蚀行为研究[J]. 中国腐蚀与防护学报, 2026, 46(1): 137-144.