X65碳钢在模拟油田采出水中的阴极保护研究 |
邱景1, 杜敏1, 陆原2, 张颖2, 郭海军2, 李成杰1 |
1. 中国海洋大学化学化工学院 海洋化学理论与工程技术教育部重点实验室 青岛 266100; 2. 中海油能源发展采油技术服务分公司 天津 300452 |
|
Cathodic Protection of X65 Carbon Steel in a Simulated Oilfield Produced Water |
QIU Jing1, DU Min1, LU Yuan2, ZHANG Ying2, GUO Haijun2, LI Chengjie1 |
1. Key Laboratory of Marine Chemistry Theory and Technology, Ministry of Education, College of Chemistry and Chemical Engineering, Ocean University of China, Qingdao 266100, China; 2. CNOOC-ETS-Oilfield Technology Services Co., Tianjin 300452, China |
引用本文:
邱景, 杜敏, 陆原, 张颖, 郭海军, 李成杰. X65碳钢在模拟油田采出水中的阴极保护研究[J]. 中国腐蚀与防护学报, 2014, 34(4): 333-338.
QIU Jing,
DU Min,
LU Yuan,
ZHANG Ying,
GUO Haijun,
LI Chengjie.
Cathodic Protection of X65 Carbon Steel in a Simulated Oilfield Produced Water. Journal of Chinese Society for Corrosion and protection, 2014, 34(4): 333-338.
链接本文:
https://www.jcscp.org/CN/10.11902/1005.4537.2013.155
或
https://www.jcscp.org/CN/Y2014/V34/I4/333
|
[1] Qu H, Ma Z H, Guan S F, et al. Corrosion and protection of dissolved gases in produced water from oil field [J]. Environ. Sci. Technol., 2011, 24(2): 65-69 (曲虎, 马梓涵, 管善峰等. 油田采出水中溶解性气体的腐蚀与防护 [J]. 环境科学, 2011, 24(2): 65-69) [2] Yin Z F, Liu L, Zhang Y Q, et al. Characteristics and mechanism of?corrosion?film formation on antisulphur steels in CO 2 /H 2 S environments [J]. Corros. Eng. Sci. Technol., 2012, 47(2): 138-144 [3] Ren C Q, Wang X, Liu L, et al. Lab and field investigations on localized?corrosion?of casing [J]. Mater. Corros., 2012, 63(2): 168-172 [4] Zhang X J, Ji W, Wang B H, et al. Study on the treatment technology of oilfield produced water [J]. Ind. Safety Environ. Prot., 2007, 33(4): 13-16 (张学佳, 纪巍, 王宝辉等. 油田采出水处理技术进展 [J]. 工业安全与环保, 2007, 33(4): 13-16) [5] Cheng L H, Bi X J, Ni Y T. Oilfield?produced water treatment by ozone-enhanced flocculation [J]. Energy Educ. Sci. Technol., 2012, [6] Wei D, Wang H Y, Zhu S D, et al. Corrosion behavior of low-nickel alloy steels in a simulated oilfield environment containing carbon dioxide [J]. Proc. Inst. Mech. Eng. B-J. Eng. Ma., 2012, 266(A11): 1891-1899 [7] Han J. Research of the treatment technology of oilfield produced water [J]. China Chem. Trade, 2012, (4): 278 (韩剑. 油田采出水处理技术方法研究 [J]. 中国化工贸易, 2012, (4): 278) [8] Horsup D I, Clark J C, Binks B P, et al. The fate of?oilfield?corrosion?inhibitors in multiphase systems [J]. Corrosion, 2010, 66(3): 036001 [9] Mohammed K Z, Hamdy A, Abdel-Wahab A, et al. Temperature effect on?corrosion?inhibition of carbon steel in formation water by non-ionic inhibitor and synergistic influence of halide ions [J]. Life Sci. J., 2012, 9(2): 424-434 [10] Alikin I N, Malkov Y K, Khan S V. Corrosion Inhibitor in Mineralised Hydrogen Sulphide-containing Oilfield Media [P]. Russia: RU2454488-C1, 2012 [11] Hartt W H. 2012 Frank Newman Speller Award: cathodic protection of offshore structures-history and current status [J]. Corrosion, 2012, 68(12): 1063-1075 [12] Neville A, Morizot A P. Calcareous scales formed by cathodic protection-an assessment of characteristics and kinetics [J]. Cryst. Growth, 2002, 234: 490-502 [13] Yan J F, Nyuyen T V, White R E, et al. Mathematical modeling of the formation of calcareous deposits on cathodically protected steel in seawater [J]. Electrochem. Soc., 1993, 140(3): 733-744 [14] Lajevardi S A, Tafreshi H, Shahrabi T. Investigation of calcareous deposits formation on 5052 aluminium alloy under cathodic polarisation in natural and artificial sea water [J]. Corros. Eng. Sci. Technol., 2011, 46(3): 249-255 [15] Cabrini M, Lorenzi S, Marcassoli P, et al. Effect of hydrogen diffusion on environmental assisted cracking of pipeline steels under cathodic protection [J]. Metall. Ital., 2008, (2): 15-22 [16] Honarvar Nazari M, Allahkaram S R, Kermani M B. The effects of temperature and pH on the characteristics of corrosion product in CO 2 corrosion of grade X70 steel [J]. Mater. Design, 2010, 31: 3559-3563 [17] M?ller H. The influence of Mg 2+ on the formation of calcareous deposits on a freely corroding low carbon steel in seawater [J]. Corros. Sci., 2007, 49: 1992-2001 [18] Li C J, Du M, Li Y, et al. The influences of protection potentials on the formation of calcareous deposits in dynamic seawater [J]. Periodical Ocean Univ. China, 2011, 41 (7/8): 149-153 (李成杰, 杜敏, 李妍等. 动态海水中保护电位对钙质沉积层形成的影响 [J]. 中国海洋大学学报, 2011, 41(7/8): 149-153) [19] Li C J, Du M. Research and development of cathodic protection for steel materials in deep seawater [J]. J. Chin. Soc. Corros. Prot., 2013, 33(1): 10-15 (李成杰, 杜敏. 深海钢铁材料的阴极保护技术研究及发展 [J]. 中国腐蚀与防护学报, 2013, 33(1): 10-15) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|