304不锈钢晶间腐蚀过程中的电化学阻抗谱特征
秦丽雁;宋诗哲;卢玉琢
天津大学材料学院
EIS CHARACTERISTICS OF 304 STAINLESS STEEL DURING INTERGRANULAR CORROSION
;;
天津大学材料学院
引用本文:

秦丽雁; 宋诗哲; 卢玉琢 . 304不锈钢晶间腐蚀过程中的电化学阻抗谱特征[J]. 中国腐蚀与防护学报, 2007, 27(2): 74-79 .

全文: PDF(1143 KB)  
摘要: 用电化学阻抗谱(EIS)方法研究了固溶态、敏化态304不锈钢在0.5mol/L H2SO4+0.01mol/L KSCN溶液中的阻抗谱特征.研究表明,不锈钢在不同极化电位下的阻抗谱呈现活性溶解、活化-钝化、钝化及再活化的特征.达到再活化之前,固溶态和敏化态的不锈钢在0.5mol/L H2SO4+0.01mol/L KSCN溶液中呈现相同的EIS特征;而在再活化区,钝化膜局部溶解,EIS图有两个容抗弧,低频容抗弧延伸到第二象限,呈现负电阻特征,低频下敏化态比固溶态不锈钢阻抗模值小一个数量级.
关键词 : 不锈钢,  晶间腐蚀,  电化学阻抗谱    
Abstract:Electrochemical impedance spectroscopy (EIS) measurements were performed on sensitized and solutioned 304 stainless steels respectively in the process of Electrochemical potentiodynamic reactivation (EPR) polarization in 0.5mol/L H2SO4+0.01mol/L KSCN solution.The variation rules of impedance resistance in process of EPR polarization were analyzed.It was found that the EIS spectra of the stainless steels during EPR polarization exhibited features of active dissolution,activation-passivation,passivation and reactivation.Before reactivation,the two kinds of stainless steels had the same EIS characteristics.In the reactivating region the passivated film dissolved partially and the impedance modulus of the sensitized stainless steel was one magnitude order smaller than that of the solution-treated stainless steel,indicating that intergranular corrosion had occurred on the surface of the sensitized stainless steel.In addition two capacitive loops appeared in the EIS of the sensitized stainless steel and it was quite interesting that the second arc at the low frequency range was actually a negative resistance capacitive loop.These results may provide essential basis for detecting intergranular corrosion susceptibility of stainless steel by electrochemical impedance spectroscopy.
Key words: stainless steel    intergranular corrosion    electrochemical impedance spectroscopy
收稿日期: 2005-10-31     
ZTFLH:  TG174.3  
[1]Fang Z,Zhang Y L,Wu Y S.Detecting susceptibility to intergranularcorrosion of 308L stainless steel by EPR method[J].Corros.Sci.Prot.Technol.,1996,8:87-93(方智,张玉林,吴荫顺等.电化学动电位再活化法评价308L不锈钢的晶间腐蚀敏感性[J].腐蚀科学与防护技术,1996,8:87-93)
[2]Fang Z,Wu Y S,Zhang L,et al.Application of the modified electro-chemical potentiodynamic reactivation method to evaluate intergranu-lar corrosion susceptibility of stainless steel[J].Corrosion,1998,54:339-346
[3]Matula M,Hyspecka L,Svoboda M,et al.Intergranular corrosion ofAISI 316L steel[J].Mater.Charact.,2001,46:203-210
[4]Huang C A,Chang Y Z,Chen S C.The electrochemical behavior ofaustenitic stainless steel with different degrees of sensitization in thetranspassive potential region in 1 mol/L H2SO4containing chloride[J].Corros.Sci.,2004,46:1501-1513
[5]Cihal C,Desestret A,Froment M,et al.Tests for evaluation of sensi-bility of stainless steels to intergranular corrosion[A].Proc.5th Eu-ropean Corros.Cong[C].Paris,1973,249-255
[6]Qin L Y,Dong Z D.Application of electrochemical method to evalu-ate intergranular corrosion susceptibility of stainless steels[J].TaiGang Science and Technology,1991,3:80-86(秦丽雁,董征东.用电化学方法测量不锈钢晶间腐蚀的敏感性[J].太钢科技,1991,3:80-86)
[7]Conde A,Damborenea J de.Evaluation of exfoliation susceptibility bymeans of the electrochemical impedance spectroscopy[J].Corros.Sci.,2000,42:1363-1377
[8]Yu F Z,Ma D Z,Liu G R,et al.Corrosion and Protection HandbookI.Corrosion theories tests and detections[M].Beijing:Chemical In-dustry Press,1990,70-80(于福州,马德章,刘国瑞等.腐蚀与防护手册第一册,腐蚀理论试验及监测[M].北京:化学工业出版社.1990,70-80)
[9]Bastidas J M,Lpez MF,Gutirrez A,Torres C L.Chemical analysisof passive films on type AISI 304 stainless steel using soft X-rayabsorption spectroscopy[J].Corros.Sci.,1998,40:431-438
[10]Cao C N,Zhang J Q.An Introduction to Electrochemical ImpedanceSpectroscopy[M].Beijing:Science Press,2002,45-75(曹楚南,张鉴清.电化学阻抗谱导论[M].北京:科学出版社,2002.45-75)
[1] 郑凯, 王艺陶, 王东胜, 刘伟, 蒋颖畅, 黄嵘, 常雪婷. 腐蚀-应力耦合作用对极地船用螺旋桨低碳马氏体不锈钢失效机理影响研究[J]. 中国腐蚀与防护学报, 2026, 46(5): 1452-1462.
[2] 董少阳, 刘朝坤, 李昱彤, 夏忠虎, 甘浪, 李聪, 任延杰. 高速激光熔覆NiCrAlY涂层在900 ℃空气中的高温氧化行为[J]. 中国腐蚀与防护学报, 2026, 46(5): 1463-1474.
[3] 叶海锋, 沈书成, 陈江华. 增材制造316L不锈钢在不同温度海水环境中的腐蚀行为研究[J]. 中国腐蚀与防护学报, 2026, 46(5): 1569-1578.
[4] 何章平, 袁誉坤, 杜颖哲, 林鹏, 徐健. 在模拟电加热器过热条件下316LN奥氏体钢缝隙腐蚀行为的研究[J]. 中国腐蚀与防护学报, 2026, 46(5): 1579-1587.
[5] 刘夏城, 邹建荣, 高良文, 周龙, 谭季波, 吴欣强, 张兹瑜. 压水堆核电站不锈钢焊缝材料腐蚀疲劳模型[J]. 中国腐蚀与防护学报, 2026, 46(5): 1613-1618.
[6] 俞春林, 顾铭飞, 孙一昂, 袁可鑫, 杨静, 王丽熙, 朱承飞, 朱海奎. 海洋环境中316不锈钢表面喷涂粉末涂层的耐久性评估[J]. 中国腐蚀与防护学报, 2026, 46(5): 1627-1633.
[7] 雍兴跃, 董晓梅, 高新华, 李卓玄, 陈燕飞, 纪灏天. 电化学阻抗谱在有机涂层研究中的应用[J]. 中国腐蚀与防护学报, 2026, 46(4): 945-961.
[8] 孙欣, 屈佳伟, 高子淋, 郑越, 马爱利, 姚琳, 张连民, 郑玉贵. Mn2+ 对304L和C25不锈钢在高温硝酸中腐蚀行为的协同作用机制与响应曲面模型研究[J]. 中国腐蚀与防护学报, 2026, 46(4): 1015-1030.
[9] 张晶晶, 张震, 赵占勇, 白培康, 周杰. NaHSO3 添加对445J2铁素体不锈钢在NaCl溶液中腐蚀行为影响研究[J]. 中国腐蚀与防护学报, 2026, 46(4): 1197-1206.
[10] 陆海峰, 缪强, 梁文萍, 姚志猛, 魏少翀, 陈国星. 激光清洗对不锈钢表面耐腐蚀性能的影响[J]. 中国腐蚀与防护学报, 2026, 46(4): 1227-1237.
[11] 王彦峰, 王流火, 孙仕达, 刘琦, 李亚梅, 王显宗. 柔直换流阀冷却系统关键材料失效与缓解措施研究进展[J]. 中国腐蚀与防护学报, 2026, 46(3): 653-662.
[12] 张新瑞, 薛宝权, 谭季波, 张兹瑜, 高军, 吴欣强. 含铝奥氏体不锈钢液态铅铋环境相容性研究进展[J]. 中国腐蚀与防护学报, 2026, 46(3): 671-679.
[13] 王萌萌, 曹国民, 孟繁兴, 李天亮, 宋沁峰, 单太航, 董亮. 混凝土配重层对近海海底钢质管道阴极保护效果的影响[J]. 中国腐蚀与防护学报, 2026, 46(3): 680-692.
[14] 陈旭, 刘宇航, 郭建, 王岐山, 刘畅, 刘彬. 超级13Cr不锈钢在饱和CO2 油田采出液中的缝隙腐蚀行为[J]. 中国腐蚀与防护学报, 2026, 46(2): 523-532.
[15] 张金宇, 李欣, 张磊, 陈志华, 杜雨昕, 冯贺鑫, 张雪, 张洋鹏, 林如山, 李瑛, 戎利建. 几种17Cr系不锈钢在氯化物蒸汽中的腐蚀行为研究[J]. 中国腐蚀与防护学报, 2026, 46(2): 576-582.