中国腐蚀与防护学报  2000, Vol. 20 Issue (4): 248-252          
  研究报告 本期目录 | 过刊浏览 |
塑性变形在氢致断裂中的作用
王燕斌;王胜;颜练武
北京科技大学 材料物理系
THE EFFECTS OF PLASTIC DEFORMATION ON HYDROGEN INDUCED CRACKING
Yanbin Wang;Sheng Wang;
北京科技大学 材料物理系
引用本文:

王燕斌; 王胜; 颜练武 . 塑性变形在氢致断裂中的作用[J]. 中国腐蚀与防护学报, 2000, 20(4): 248-252 .
, , . THE EFFECTS OF PLASTIC DEFORMATION ON HYDROGEN INDUCED CRACKING[J]. J Chin Soc Corr Pro, 2000, 20(4): 248-252 .

全文: PDF(136 KB)  
摘要: 采用慢应变速率拉伸方法,研究了Fe-Si试样在空气中拉伸\动态充氢拉伸及在空气中预应变一定量后动态充氢拉伸等实验条件下的断裂过程.结果表明,只有在充氢过程中进行塑性变形才能引起氢致开裂,即塑性变形是氢致开裂的必要条件,氢致开裂过程是氢与位错交互作用的过程.
关键词 : 塑性变形,  氢致开裂,  位错    
Abstract:The fracture behaviors during hydrogen charging of Fe-3% Si single crystal was studied by low strain rate tension.The experiments included tension in air,tension during gynamically charging and charging after certain pre-strain.The results indicated that hydrogen induced cracking can occur only when the sample deformed during charging .That is, deformation is a necessary conditon for hydrogen induced cracking and hydrogen induced cracking results from the interaction between hydrogen and dislocation.
Key words: deforation    hydrogen induced cracking    dislocation
收稿日期: 1999-08-09     
ZTFLH:  TG172.83  
[1] Hirth J P. Effect of hydrogen on the properties of iron and steel[J] .Metall .Trans., 1980, 11A:861 - 873
[2] An S, Shiozawa K,GU J, Chen N J. Investigation of deformation field and hydrogen partition around crack tip in fcc single crystal[J].Metall. Trans., 1995, 26A:731 - 739
[3] Qiao L J, Chu W Y, Wao X. Critical hydrogen concentration for hydrogen-induced cracking of the 321 stainless steel[J]. Corrosion, 1996,52:275-279
[4] Rozenak P, Robertson I M, Bimbaum H K. HVEM studies of the effect of hydrogen on the deformation and fracture of AISI type 316 steel[J]. Acta Metall.Mater, 1990, 38:2031-2040
[5] Birnbaum H K, Sofronis P. Hydrogen-enhanced localized plasticity - a mechanism for hydrogen related fracture[J]. Mater. Sci. Eng.,1994, A176: 191 - 202
[6]李密丹,张天成,吕宏,褚武扬.氢促进位错发射和运动导致裂纹形核的研究[J].中国科学,1997,27E:481-487
[7] Chu W Y, Liu T W, Hsiao C M.Mechanism of stress corrosion cracking of low alloy steel[J]. Corrosion. 1981, 37:320 - 325
[8] Chen S H, Katz Y, Gerberich W W. Crack-tip strain field and fracture microplasticity in hydrogen induced cracking of Fe-3wt% Si singlecrystals[J]. Phil. Mag., 1991, 63: 131 - 155
[9] Abrahum D P, Altstertter C J. Hydrogen-enhanced localization of plasticity in an austenitic stainless steel [J]. Metall. Mater. Trans. A,1995, 26A: 2859 - 2871
[10]张柏玉,刁凤琼,唐祥云.20钢氢致开裂临界浓度与应力的关系[J].金属学报,1990.26:A454-459
[11] Wang Y B, Chu W Y, Hsiao C M. X-ray topographic study of hydrogen damage in Fe-3wt%Si Steel[J]. Acta Mitall. Sinica B, 1993, 6:87 - 91
[12] Marrow TJ, Aindow M, Prangnell P, Strangwood M, Knott J F. Hydrogen stable crack growth in Fe-3wt% Si steel [J]. ActaMetall. Mater. 1996, 44: 3125 - 3140
[13] Gao G Y, Dexter S C. Effect of hydrogen on creep behavior of Ti-6Al-4V alloy at room temperature[J] .Metall. Mater. Trans.A, 1987,18A: 1125 - 1130
[14] Gu B, Chu W Y, Qiao L J.The facilitation effect of anodic polarization on ambient creep of brass[J]. Corrosion Science, 1994, 36:1437
[15] Maier H J,Popp W,Kaescha H. Effects of hydrogen on ductile fracture of a spheroidized low alloy steel[J] .Mater. Sci. Eng., 1995,A191: 17 - 26.
[16] Keh A S. Weissmann S. Electron Microscopy and Strength of Crystals[M]. Thomas G, Washburn T eds, New York: John Wiley andSons, 1963. 231
[1] 李兴斌, 雷蕴博, 高栋, 于泽, 董福宇, 周宇. 动态塑性变形对商用纯钛微观结构和氢致开裂行为的影响[J]. 中国腐蚀与防护学报, 2026, 46(2): 583-589.
[2] 诸滔, 孙浩翔, 周亚洪, 赵宇航, 王艳飞. 氢扩散模型对临氢结构裂尖氢浓度计算影响[J]. 中国腐蚀与防护学报, 2025, 45(4): 1070-1080.
[3] 张倩茹, 孙擎擎. 氢促进局部塑性变形理论的发展趋势[J]. 中国腐蚀与防护学报, 2025, 45(2): 271-282.
[4] 白云龙, 冷冰, 韦博鑫, 董立谨, 于长坤, 许进, 孙成. 掺氢天然气管材及焊缝的氢损伤行为研究进展[J]. 中国腐蚀与防护学报, 2025, 45(2): 283-295.
[5] 彭浩, 程晓英, 李晓亮, 王兆丰, 蔡贞祥. 高强度低合金钢中V和Nb对氢陷阱的影响[J]. 中国腐蚀与防护学报, 2023, 43(2): 415-420.
[6] 马成, 崔彦发, 张青, 赵林林, 王立辉, 熊自柳. 中锰TRIP钢氢致开裂性能研究现状与进展[J]. 中国腐蚀与防护学报, 2022, 42(6): 885-893.
[7] 王保杰,栾吉瑜,王士栋,许道奎. 镁合金应力腐蚀开裂行为研究进展[J]. 中国腐蚀与防护学报, 2019, 39(2): 89-95.
[8] 郭强, 陈长风, 李世瀚, 于浩波, 李鹤林. 冷焊修复层在H2S环境下的开裂行为研究[J]. 中国腐蚀与防护学报, 2018, 38(2): 167-173.
[9] 史显波, 王威, 严伟, 单以银, 杨柯. M/A组元对高强度管线钢抗H2S性能的影响[J]. 中国腐蚀与防护学报, 2015, 35(2): 129-136.
[10] 王斌, 周翠, 李良君, 胡红梅, 朱加祥. X100管线钢焊接接头抗HIC性能研究[J]. 中国腐蚀与防护学报, 2014, 34(3): 237-242.
[11] 董希青,黄彦良. 不锈钢在海洋环境中的环境敏感断裂研究进展[J]. 中国腐蚀与防护学报, 2012, 32(3): 189-194.
[12] 姚学军,王俭秋,左景辉,韩恩厚,柯伟. 微观组织对X52钢抗H2S腐蚀和开裂性能的影响[J]. 中国腐蚀与防护学报, 2012, 32(2): 95-101.
[13] 饶思贤,万章,宋光雄,张铮,钟群鹏. 基于规则的晶间腐蚀和氢致开裂的失效模式诊断[J]. 中国腐蚀与防护学报, 2011, 31(4): 260-264.
[14] 镇凡;刘静;黄峰;程吉浩;李翠玲;郭斌;徐进桥. 夹杂物对X120管线钢氢致开裂的影响[J]. 中国腐蚀与防护学报, 2010, 30(2): 145-149.
[15] 胡道春 孙乐民 上官宝. 动载荷条件下紫铜/铬青铜受流摩擦磨损性能[J]. 中国腐蚀与防护学报, 2009, 29(1): 35-39.