Study on SCC Behavior of Austenitic Stainless Steels in H2S Saturated Aqueous Solutions Containing Cl-
Rongguang Wang;;;
上海材料研究所
Cite this article: 

Rongguang Wang. Study on SCC Behavior of Austenitic Stainless Steels in H2S Saturated Aqueous Solutions Containing Cl-. J Chin Soc Corr Pro, 2000, 20(1): 47-53 .

Download:  PDF(263KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Stress corrosion cracking(SCC) sensibility of austentic stainless steels SUS 316L in H2Ssaturated aqueous solution containing Cl- or CO32- was investigated by U bend samples. Addition of Cl- and reduction of solution pH intensified the SCC susceptibility of these two steels. But it was decreased obviously when adding 0.001mol/L Na2CO3 into the aq ueous solution especially for SUS316. Intergranular corrosion sensibility of SUS 316 was increased after sensitization heat treatment, and its SCC resistance got worse. However, SUS 316L exhibited remarkable immunity to sensitization. The SCC cracking morphology and the mechanism were also discussed.
Key words:  austenitic stainless steel      stress corrosion cracking      
Received:  22 March 1999     
ZTFLH:  TG172.9  

URL: 

https://www.jcscp.org/EN/     OR     https://www.jcscp.org/EN/Y2000/V20/I1/47

[1]EdeleanuC .Tansgranularstresscorrosioninchromium nickelstainlesssteels [J].JIronstInst,1953,173:140 .
[2 ]HinesJC ,HearTP .Streescorrosionofausteniticstainlesssteelsinsteamandhotwatersystems [J].JIronstInst,1956 ,186 :4 0 6 .
[3]StaehleRW ,BeckFH ,Fontana,MG .Mechanismofstresscorrosionofausteniticstainlesssteelsinchloridewaters[J].Corrosion ,1959,15:373.
[4 ]高佩玉 .H2 S H2 O系统中奥氏体不锈钢破裂机理的研究 [J].中国腐蚀与防护学报 ,1982 ,2 (3) :10 .
[5]SnowdenPP .Stresscorrosionofausteniticstainlesssteelbyhigh temperaturesolutionsandcontaminatedsteam [J].JIron&SteelInst,196 0 ,194 :181.
[6 ]Thorne ,PCL ,RobertER .InorganicChemistry[M].GurneyandJackson ,194 8.
[7]ZhengWL ,HardieD ,Hydrogen inducededcrackingsusceptibilityof18Mn5Crand 18Mn18CrNinon magneticAlloy[A].ProceedingsofInternationalConferenceonEnvironment -SensitiveCracking :MechanismsandIndustrialsApplications,1994 .390 .
[8]乔利杰 ,褚武扬 ,肖纪美 ,氢在奥氏体不锈钢应力腐蚀中的作用 [J]. 金属学报 ,1987,2 3(3) :2 2 8.
[9]肖纪美 .高速钢的金属学问题 [M].北京 :冶金工业出版社 ,1976 :10 .
[1] XU Jiacheng, LIU Jiabing, HUANG Shiyu, JIN Linghao, TAN Wei, GUO Na, LIU Tao. Mechanical Property Damage and Stress Corrosion Behavior of EH40 Steel Ship Plate in Artificial Polar Marine Environments[J]. 中国腐蚀与防护学报, 2026, 46(5): 1437-1451.
[2] JIA Mengyao, ZHANG Weiqiang, WANG Yuan, TAN Jibo, QIU Jianke, HAO Yantian, WU Xinqiang. Effect of Pressure Variation on Stress Corrosion Behavior of Ti80 Alloy in 3.5%NaCl Solution[J]. 中国腐蚀与防护学报, 2026, 46(5): 1508-1516.
[3] WANG Lei, TAO Zeyu, LIU Feng, KUANG Wenjun, MA Xin, YAO Yao, ZHANG Guowei. Effect of Water Chemistry on Stress Corrosion Cracking of T22 Steel Used in Once Through Steam Generator of Nuclear Power[J]. 中国腐蚀与防护学报, 2026, 46(4): 1067-1080.
[4] ZHANG Xinrui, XUE Baoquan, TAN Jibo, ZHANG Ziyu, GAO Jun, WU Xinqiang. A Review on environmental degradation of Alumina-forming Austenitic Stainless Steel in Liquid Lead-bismuth Eutectic[J]. 中国腐蚀与防护学报, 2026, 46(3): 671-679.
[5] LAN Botao, WU Bin, MING Hongliang, WANG Jianqiu, HAN En-Hou. Research Progress of Stress Corrosion Crack Behavior of Selected Laser Melted Austenitic Stainless Steel in High Temperature Pressurized Water[J]. 中国腐蚀与防护学报, 2026, 46(1): 1-14.
[6] ZHANG Deping, YAN Lizhen, YU Yang, YANG Guangming, DAI Chunyu, MEGN Le, XU Bo, LIU Zhiyong. Fracture Failure Mechanism of N80 Tubing in Sophisticated CO2 Flooding Production Well Environment[J]. 中国腐蚀与防护学报, 2025, 45(6): 1698-1708.
[7] HE Yan, LIU Yan, TIAN Hua, CHEN Ye. Effect of Low Temperature Diffusion Pretreatment on Precipitation of Phases During Post-aging Treatment for B-containing S31254 Super Austenitic Stainless Steel and its Corrosion Resistance[J]. 中国腐蚀与防护学报, 2025, 45(6): 1773-1778.
[8] HE Wuhao, LIU Yang, YANG Siyi, ZHANG Shaodong, WU Wei, ZHANG Junxi. Effect of Sensitization Treatment on Electrochemical Behavior and Intergranular Corrosion of Conventional and Additively Manufactured 316L Stainless Steels[J]. 中国腐蚀与防护学报, 2025, 45(5): 1331-1340.
[9] ZHANG Huiyun, ZHENG Liuwei, LIANG Wei. Effect of Annealing Process on Microstructure Evolution and Hydrogen Embrittlement Behavior of 304 Austenitic Stainless Steel[J]. 中国腐蚀与防护学报, 2025, 45(2): 438-448.
[10] SU Zhicheng, ZHANG Xian, CHENG Yan, LIU Jing, WU Kaiming. Comparative Study on Stress Corrosion Cracking Behavior of Ultrafine Bainitic Steel and Q&P Steel with Same Composition in Seawater[J]. 中国腐蚀与防护学报, 2024, 44(6): 1495-1506.
[11] MA Jinyao, DONG Nan, GUO Zhensen, HAN Peide. Effect of B and Ce Micro-alloying on Secondary Phase Precipitation and Corrosion Resistance of S31254 Super Austenitic Stainless Steel[J]. 中国腐蚀与防护学报, 2024, 44(6): 1610-1616.
[12] ZHANG Zhuanli, DAI Hailong, ZHANG Zhe, SHI Shouwen, CHEN Xu. Stress Corrosion Cracking Behavior of 316L in Hydrofluoric Acid Solution[J]. 中国腐蚀与防护学报, 2024, 44(6): 1633-1640.
[13] LIU Jiuyun, DONG Lijin, ZHANG Yan, WANG Qinying, LIU Li. Research Progress on Sulfide Stress Corrosion Cracking of Dissimilar Weld Joints in Oil and Gas Fields[J]. 中国腐蚀与防护学报, 2024, 44(4): 863-873.
[14] LI Chan, WANG Qingtian, YANG Chenggang, ZHANG Xianwei, HAN Dongao, LIU Yuwei, LIU Zhiyong. Corrosion Behavior of 904L Super-austenitic Stainless Steel in Simulated Primary Water in Nuclear Power Plants[J]. 中国腐蚀与防护学报, 2024, 44(3): 716-724.
[15] GENG Zhenzhen, ZHANG Yuzhu, DU Xiaojiang, WU Hanhui. Synergistic Effect of S2- and Cl- on Corrosion and Passivation Behavior of 316L Austenitic Stainless Steel[J]. 中国腐蚀与防护学报, 2024, 44(3): 797-806.
No Suggested Reading articles found!