Please wait a minute...
J Chin Soc Corr Pro  1995, Vol. 15 Issue (3): 196-202    DOI:
Current Issue | Archive | Adv Search |
CORROSION FATIGUE BEHMIOUR OF A HIGH STRENGTH STEEL FOR OIL-DRAWING STICKS
Li Mingqi;Meng Fanzong(Lunzhou University)Sui Xianzeng;Zhou Xiang(Xining Steel Works)
Cite this article: 

Li Mingqi;Meng Fanzong(Lunzhou University)Sui Xianzeng;Zhou Xiang(Xining Steel Works). CORROSION FATIGUE BEHMIOUR OF A HIGH STRENGTH STEEL FOR OIL-DRAWING STICKS. J Chin Soc Corr Pro, 1995, 15(3): 196-202.

Download:  PDF(2383KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Fatigue craCk.growth rates (FCGR)of tempered and normalized specimen of high strength steel38MnCrNiMo exposed to air,distilled water and 3.5%NaCl solution were evaluated. The effects of appliedpolarization potentials on FCGR in 3.5%NaCl solution were examined. The corrosion fatigUe fracturesurfaCe features and metallographic microstructure were also observed. The results indicated that thefatigue crack growth for the steel was controlled by hydrogen embrittlement(HE)and the FCGR oftempered specimens was lower than that of normalized specimens in air,distilled water and 3.5% NaCI' solution. The HE sensitivity of fatigue crack growth for the sted in corrosive environments was aLsodiscussed.
Key words:  Corrosion fatigue      Fatigue crack growth rate      Hydrogen embrittlement      Polarization potential     
Received:  25 June 1995     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.jcscp.org/EN/     OR     https://www.jcscp.org/EN/Y1995/V15/I3/196

1LiMingqi,WeiZhenwei,ZhangFusheng,TangJieqing.Corros.Sci.,1993,34(9):1403-14102李明奇,冯博学.理化检验(物理分册),1986,22(4):31-333李明奇,冯博学,魏振伟.中国腐蚀与防护学报,1987,7(4):2574BrownBF,etal.J,Electrochem.Soc,1969,116(2):2185褚武扬.断裂力学基础,北京:科学出版社,1979,p.386李明奇,张福生,魏振伟,潘水才.兰州大学学报(自然科学版),1993,29(2):43-467李明奇,冯博学,童志深.兰州大学学报(自然科学版),1986,22(3):42-48
[1] LIU Wanying, LI Lei, ZHU Xinyu, ZHANG Zhi, DING Jian, LIU Peng, SONG Zhuoying, FAN Zuoyuan. A Review on Inflencing Factors, Detection Methods and Protection Techniques for Hydrogen-induced Embrittlement of Hydrogen-bearing Natural Gas Pipeline Steels[J]. 中国腐蚀与防护学报, 2026, 46(5): 1400-1414.
[2] ZANG Bolin, WU Hao, YIN Wenchang, YANG Yandong, TIAN Huiyun, CUI Zhongyu. Effect of Cathodic Polarization on Hydrogen Embrittlement Behavior of Two High-strength Ni-Cr-Mo-V Steels[J]. 中国腐蚀与防护学报, 2026, 46(5): 1527-1536.
[3] LIU Xiacheng, ZOU Jianrong, GAO Liangwen, ZHOU Long, TAN Jibo, WU Xinqiang, ZHANG Ziyu. Corrosion Fatigue Model for Stainless Steel Weld Seam Used in Pressurized Water Reactor Nuclear Power Plants[J]. 中国腐蚀与防护学报, 2026, 46(5): 1613-1618.
[4] XU Yunfeng, CHENG Kaiyuan, HUANG Feng, YANG Baoqi, CHENG Xianglong, ZAN Qifei, PENG Zhixian, LIU Jing. Effect of Hydrogen Pre-charging Time on Hydrogen Embrittlement Susceptibility in High Pressure Hydrogen Environment for Two Seamless Steel Pipe Steels with Different Microstructures[J]. 中国腐蚀与防护学报, 2026, 46(3): 787-797.
[5] XIANG Qifeng, ZHAO Yang, ZHANG Tao, WANG Fuhui. Influence of Cathodic Polarization on Hydrogen Embrittlement Susceptibility of 10CrNi5MoV Steel in Simulated Shallow-sea and Deep-sea Environment[J]. 中国腐蚀与防护学报, 2025, 45(6): 1599-1609.
[6] SHI Xuanming, TAN Jibo, ZHANG Ziyu, WU Xinqiang. A Review on Fatigue Behavior of Candidate Structure Materials for Lead-cooled Fast Reactors in Liquid Lead-bismuth Eutectic[J]. 中国腐蚀与防护学报, 2025, 45(5): 1187-1195.
[7] ZHU Tao, SUN Haoxiang, ZHOU Yahong, ZHAO Yuhang, WANG Yanfei. Effect of Hydrogen Diffusion Model on Hydrogen Concentration Calculation Around a Crack Tip in Hydrogen-exposed Structures[J]. 中国腐蚀与防护学报, 2025, 45(4): 1070-1080.
[8] WANG Mingyang, XIA Da-Hai. Research Progress on Hydrogen Embrittlement Mechanism of High Strength Al-alloy[J]. 中国腐蚀与防护学报, 2025, 45(2): 261-270.
[9] ZHANG Qianru, SUN Qingqing. Hydrogen Enhanced Localized Plasticity: A Critical Review[J]. 中国腐蚀与防护学报, 2025, 45(2): 271-282.
[10] CUI Bolun, ZHAO Jie, LV Ran, LI Jingfa, YU Bo, YAN Donglei. Research Progress in Composite Protection Technology Against Hydrogen-embrittlement and -corrosion for Hydrogen-blended Natural Gas Pipeline[J]. 中国腐蚀与防护学报, 2025, 45(2): 327-337.
[11] WAN Hongjiang, MING Hongliang, WANG Jianqiu, HAN En-Hou. Effect of Small Amount of O2 and CO on Hydrogen Embrittlement Susceptibility of X52 Pipeline Steel[J]. 中国腐蚀与防护学报, 2025, 45(2): 371-380.
[12] CHEN Kai, DU Yifan, XU Haoyun, LV Liang, DANG Guiming, WANG Yujin, ZHENG Shuqi. Hydrogen Permeation and Hydrogen Embrittlement Sensitivity of X80 Pipeline Steel[J]. 中国腐蚀与防护学报, 2025, 45(2): 388-396.
[13] CHENG Kaiyuan, PENG Yang, HUANG Feng, CHENG Xianglong, XU Yunfeng, PENG Zhixian, LIU Jing. Adaptability of Typical Seamless Tube Steels to Hydrogen-blended Natural Gas Environments and Hydrogen- induced Damage Mechanism[J]. 中国腐蚀与防护学报, 2025, 45(2): 397-406.
[14] LI Xincheng, LI Zhaonan, WANG Haifeng, XU Yunze, WANG Mingyu, ZHEN Xingwei. Hydrogen Embrittlement Sensitivity for Welded Structural Parts of DH36 Marine Engineering Steel[J]. 中国腐蚀与防护学报, 2025, 45(2): 416-422.
[15] LIU Tianle, WEI Boxin, FU Anqing, SU Hang, CHEN Tingshu, WANG Chaoming, WANG Sui. Hydrogen Damage of X80 Pipeline Steel in Hydrogen-doped Gaseous Atmosphere[J]. 中国腐蚀与防护学报, 2025, 45(2): 423-430.
No Suggested Reading articles found!