| NiCrMoNb和NiCoFeCrMoNb合金在700 ℃熔融NaCl-KCl-MgCl2 中的腐蚀行为研究 |
卢华轶, 李若愚, 程宇飞, 白英雄, 王艳丽( ) |
| 广西大学化学化工学院 广西石化资源加工及过程强化技术重点实验室 南宁 530004 |
|
| Corrosion Behavior of NiCrMoNb and NiCoFeCrMoNb Alloys in Molten NaCl-KCl-MgCl2 at 700 ℃ |
LU Huayi, LI Ruoyu, CHENG Yufei, BAI Yingxiong, WANG Yanli( ) |
| Guangxi Key Laboratory of Petrochemical Resource Processing and Process Intensification Technology, School of Chemistry and Chemical Engineering, Guangxi University, Nanning 530004, China |
引用本文:
卢华轶, 李若愚, 程宇飞, 白英雄, 王艳丽. NiCrMoNb和NiCoFeCrMoNb合金在700 ℃熔融NaCl-KCl-MgCl2 中的腐蚀行为研究[J]. 中国腐蚀与防护学报, 2026, 46(3): 730-742.
Huayi LU,
Ruoyu LI,
Yufei CHENG,
Yingxiong BAI,
Yanli WANG.
Corrosion Behavior of NiCrMoNb and NiCoFeCrMoNb Alloys in Molten NaCl-KCl-MgCl2 at 700 ℃[J]. Journal of Chinese Society for Corrosion and protection, 2026, 46(3): 730-742.
| [1] |
Gong Q, Hanke A, Kessel F, et al. Molten chloride salt technology for next-generation CSP plants: Selection of cold tank structural material utilizing corrosion control at 500 ℃ [J]. Sol. Energy Mater. Sol. Cells, 2023, 253: 112233
doi: 10.1016/j.solmat.2023.112233
|
| [2] |
Ding W J, Bauer T. Progress in research and development of molten chloride salt technology for next generation concentrated solar power plants [J]. Engineering, 2021, 7: 334
doi: 10.1016/j.eng.2020.06.027
|
| [3] |
Dunham M T, Iverson B D. High-efficiency thermodynamic power cycles for concentrated solar power systems [J]. Renew. Sust. Energy Rev., 2014, 30: 758
doi: 10.1016/j.rser.2013.11.010
|
| [4] |
Sun H, Su X Z, Zhang P, et al. Research status and progress of molten salts corrosion for concentrated solar thermal power [J]. Corros. Sci. Prot. Technol., 2017, 29: 282
|
| [4] |
孙 华, 苏兴治, 张 鹏 等. 聚焦太阳能热发电用熔盐腐蚀研究现状与展望 [J]. 腐蚀科学与防护技术, 2017, 29: 282
|
| [5] |
Grégoire B, Oskay C, Meißner T M, et al. Corrosion mechanisms of ferritic-martensitic P91 steel and Inconel 600 nickel-based alloy in molten chlorides. Part II: NaCl-KCl-MgCl2 ternary system [J]. Sol. Energy Mater. Sol. Cells, 2020, 216: 110675
doi: 10.1016/j.solmat.2020.110675
|
| [6] |
Xu X K, Dehghani G, Ning J X, et al. Basic properties of eutectic chloride salts NaCl-KCl-ZnCl2 and NaCl-KCl-MgCl2 as HTFs and thermal storage media measured using simultaneous DSC-TGA [J]. Sol. Energy, 2018, 162: 431
doi: 10.1016/j.solener.2018.01.067
|
| [7] |
Li Y Y, Xu X K, Wang X X, et al. Survey and evaluation of equations for thermophysical properties of binary/ternary eutectic salts from NaCl, KCl, MgCl2, CaCl2, ZnCl2 for heat transfer and thermal storage fluids in CSP [J]. Sol. Energy, 2017, 152: 57
doi: 10.1016/j.solener.2017.03.019
|
| [8] |
Vidal J C, Klammer N. Molten chloride technology pathway to meet the U.S. DOE sunshot initiative with Gen3 CSP [J]. AIP Conf. Proc., 2019, 2126: 080006
|
| [9] |
Ibrahim A, Peng H, Riaz A, et al. Molten salts in the light of corrosion mitigation strategies and embedded with nanoparticles to enhance the thermophysical properties for CSP plants [J]. Sol. Energy Mater. Sol. Cells, 2021, 219: 110768
doi: 10.1016/j.solmat.2020.110768
|
| [10] |
Yang X D, Li X, Yu Z, et al. Corrosion behavior of enamel coatings in molten salts MgCl2-KCl-NaCl at 600 ℃ [J]. J. Chin. Soc. Corros. Prot., 2025, 45: 155
|
| [10] |
杨啸东, 李 雪, 喻 政 等. 搪瓷涂层在600 ℃熔融MgCl2-NaCl-KCl中热腐蚀行为研究 [J]. 中国腐蚀与防护学报, 2025, 45: 155
doi: 10.11902/1005.4537.2024.186
|
| [11] |
Kruizenga A M. Corrosion mechanisms in chloride and carbonate salts [R]. Albuquerque: Sandia National Laboratories, 2012
|
| [12] |
Fernández A G, Cabeza L F. Corrosion evaluation of eutectic chloride molten salt for new generation of CSP plants. Part 1: Thermal treatment assessment [J]. J. Energy Storage, 2020, 27: 101125
doi: 10.1016/j.est.2019.101125
|
| [13] |
Zhao Y Y, Klammer N, Vidal J. Purification strategy and effect of impurities on corrosivity of dehydrated carnallite for thermal solar applications [J]. RSC Adv., 2019, 9: 41664
doi: 10.1039/C9RA09352D
|
| [14] |
Ding W J, Gomez-Vidal J, Bonk A, et al. Molten chloride salts for next generation CSP plants: Electrolytical salt purification for reducing corrosive impurity level [J]. Sol. Energy Mater. Sol. Cells, 2019, 199: 8
doi: 10.1016/j.solmat.2019.04.021
|
| [15] |
Wagman D D, Evans W H, Parker V B, et al. Selected Values of Chemical Thermodynamic Properties. Tables for the First Thirty-Four Elements in the Standard Order of Arrangement [M]. Washington: U.S. Dept. of Commerce, Natl Bureau of Standards, 1968
|
| [16] |
Xiang R Q. Corrosion behavior and mechanisms of Ni-Fe-M alloy in molten chloride salt [D]. Xining: Qinghai University, 2019
|
| [16] |
向荣桥. Ni-Fe-M合金在熔融氯化盐中腐蚀机理研究 [D]. 西宁: 青海大学, 2019
|
| [17] |
Wang J W, Zhang C Z, Li Z H, et al. Corrosion behavior of nickel-based superalloys in thermal storage medium of molten eutectic NaCl-MgCl2 in atmosphere [J]. Sol. Energy Mater. Sol. Cells, 2017, 164: 146
doi: 10.1016/j.solmat.2017.02.020
|
| [18] |
Liu S J, Wang R D, Wang L, et al. Corrosion behavior of iron-based and Ni-based alloys melted in NaCl-MgCl2-KCl mixed molten salt under vacuum atmosphere [J]. J. Mater. Res. Technol., 2024, 28: 1915
doi: 10.1016/j.jmrt.2023.12.121
|
| [19] |
D'Souza B, Zhuo W Q, Yang Q F, et al. Impurity driven corrosion behavior of HAYNES® 230® alloy in molten chloride salt [J]. Corros. Sci., 2021, 187: 109483
doi: 10.1016/j.corsci.2021.109483
|
| [20] |
Garip Y. An investigation on the corrosion performance of Fe2CoCrNi0.5 based high entropy alloys [J]. Corros. Sci., 2022, 206: 110497
doi: 10.1016/j.corsci.2022.110497
|
| [21] |
Patel K, Sadeghilaridjani M, Pole M, et al. Hot corrosion behavior of refractory high entropy alloys in molten chloride salt for concentrating solar power systems [J]. Sol. Energy Mater. Sol. Cells, 2021, 230: 111222
doi: 10.1016/j.solmat.2021.111222
|
| [22] |
Gineys N, Aouad G, Sorrentino F, et al. Incorporation of trace elements in Portland cement clinker: Thresholds limits for Cu, Ni, Sn or Zn [J]. Cem. Concr. Res., 2011, 41: 1177
doi: 10.1016/j.cemconres.2011.07.006
|
| [23] |
Sarkar K, Kumar V, Das S B, et al. Studies of structural, electrical and optical properties of MgNb2O6-Mg4Nb2O9 nanocomposite for possible opto-electronic applications [J]. Mater. Today: Proc., 2021, 44: 2459
|
| [24] |
Sun D C, Senz S, Hesse D. Crystallography, microstructure and morphology of Mg4Nb2O9/MgO and Mg4Ta2O9/MgO interfaces formed by topotaxial solid state reactions [J]. J. Eur. Ceram. Soc., 2006, 26: 3181
doi: 10.1016/j.jeurceramsoc.2005.10.007
|
| [25] |
Sun H, Wang J Q, Li Z J, et al. Corrosion behavior of 316SS and Ni-based alloys in a ternary NaCl-KCl-MgCl2 molten salt [J]. Sol. Energy, 2018, 171: 320
doi: 10.1016/j.solener.2018.06.094
|
| [26] |
Ménétrey M, Markovits A, Minot C. DFT study of Cl/MgO(100), influence of the stoichiometry [J]. Surf. Sci., 2004, 566-568: 693
doi: 10.1016/j.susc.2004.06.001
|
| [27] |
Li X D, Bai L F, Zhao H H, et al. Sinterable MgO powders via precipitation: Effects of chloride ions on powder synthesis and sintering [J]. J. Funct. Mater., 2009, 40: 1215
|
| [27] |
李晓东, 柏立飞, 赵恒和 等. 氯离子对氧化镁纳米粉体合成及烧结性能的影响研究 [J]. 功能材料, 2009, 40: 1215
|
| [28] |
Sharifi-Viand A, Mahjani M G, Jafarian M. Investigation of anomalous diffusion and multifractal dimensions in polypyrrole film [J]. J. Electroanal. Chem., 2012, 671: 51
doi: 10.1016/j.jelechem.2012.02.014
|
| [29] |
Cao C N, Zhang J Q. An Introduction to Electrochemical Impedance Spectroscopy [M]. Beijing: Science Press, 2002
|
| [29] |
曹楚南, 张鉴清. 电化学阻抗谱导论 [M]. 北京: 科学出版社, 2002
|
| [30] |
Hwang Y S, Rapp R A. Synergistic dissolution of oxides in molten sodium sulfate [J]. J. Electrochem. Soc., 1990, 137: 1276
doi: 10.1149/1.2086647
|
| [31] |
Rapp R A, Zhang Y S. Hot corrosion of materials: Fundamental studies [J]. JOM, 1994, 46: 47
|
| [32] |
Li Y S, Niu Y, Wu W T. Chlorination of metallic materials at high temperature [J]. Corros. Sci. Prot. Technol., 2000, 12: 41
|
| [32] |
李远士, 牛 焱, 吴维㞵. 金属材料的高温氯化腐蚀 [J]. 腐蚀科学与防护技术, 2000, 12: 41
|
|
Viewed |
|
|
|