Please wait a minute...
中国腐蚀与防护学报  2005, Vol. 25 Issue (3): 142-148          
  研究报告 本期目录 | 过刊浏览 |
金属材料长周期海水腐蚀规律研究
朱相荣;黄桂桥;林乐耘;刘大扬
山东青岛小麦岛海洋腐蚀所
RESEARCH PROGRESS ON THE LONG PERIOD CORROSION LAW OF METALLIC MATERIALS IN SEAWATER
;;;Dayang Liu
山东青岛小麦岛海洋腐蚀所
引用本文:

朱相荣; 黄桂桥; 林乐耘; 刘大扬 . 金属材料长周期海水腐蚀规律研究[J]. 中国腐蚀与防护学报, 2005, 25(3): 142-148 .
, , , . RESEARCH PROGRESS ON THE LONG PERIOD CORROSION LAW OF METALLIC MATERIALS IN SEAWATER[J]. J Chin Soc Corr Pro, 2005, 25(3): 142-148 .

全文: PDF(209 KB)  
摘要: 对常用金属材料在我国的青岛、舟山、厦门和榆林4个海域的飞溅、潮差、全浸3个海洋区带中暴露1、4、8和16年的长周期腐蚀试验工作进行了研究,得到了长周期的海水腐蚀数据及其腐蚀规律.提出了一种海水腐蚀性的评价方法和一种综合评价材料耐蚀性的方法.
关键词 : 金属,  海水腐蚀,  腐蚀规律    
Abstract:This paper summarized that 16 years' corrosion law and character of 50 kinds metallic materials that were exposed 1,2,4,8 and 16 years in splash zone,tidal zone,full immersion zone of Qingdao,Zhoushan,Xiamen and Yulin in China sea areas.Many data and law for long period and character of seawater corrosion for metallic materials have been obtained.An evaluation method of the seawater corrosiveness and a comprehensive evaluation method of corrosion resistance are proposed.
Key words: metal    seawater corrosion    corrosion law
收稿日期: 2003-10-30     
ZTFLH:  TG172.5  
[1]HuangGQ.Corrosionbehaviourofcarbonsteelsimmersedinsea areasofChina[J].Corros.Sci.Prot.Technol.,2001,13(2):81-86(黄桂桥.碳钢在我国不同海域的海水腐蚀行为[J].腐蚀科学与防护技术,2001,13(2):81-86)
[2]HuangGQ.Corrosionofstainlesssteelsinmarineenvironment[J].Corros.Prot.,1999,20(9):392-395(黄桂桥.不锈钢在海洋环境中的腐蚀[J].腐蚀与防护,1999,20(9):392-395)
[3]LinLY.AbnormalcorrosionbehaviorofAl-MgandAl-Mnalloy inseawater[J].Corros.Sci.Prot.Technol.,2000,12(4):198~202(林乐耘.实海暴露防锈铝合金局部腐蚀敏感性研究[J].腐蚀科学与防护技术,2000,12(4):198-202)
[4]LinLY.Studyonmarinecorrosionandantifoulingbehaviorsof copperalloyexposedtoseaareasinChina[J].RareMetals,2000,(2):96-100
[5]SouthwellCR,AlexanderAL.Corrosionofmetalsintropicalwater-structuralferrousmetals[J].Mater.Prot.,1970,(1):14-23
[6]LiuDY.Analysisforthereasonofcorrosionresistance“reversion”ofcontainingchromiumlowalloysteelinseawater[J].J.Chin.Soc.Corros.Prot.,2003,23(1):7-12(刘大扬.含铬低合金钢在海水中耐蚀性”逆转”原因分析[J].中国腐蚀与防护学报,2003,23(1):7-12)
[7]ZhuXR,HuangGQ.Astudyonthecorrosionpeakofcarbonsteel inmarinesplashzone[A].13thInter.Corr.Cong.[C].Nov.1996,Melbourne,Australia
[8]ZhuXR,HuangGQ.Corrosivebehaviourofsteelinmarinesplash zone[J].Corros.Sci.Prot.Technol.,1995,7(3):246-24(朱相荣,黄桂桥.钢在海洋飞溅带腐蚀行为探讨[J].腐蚀科学与防护技术,1995,7(3):246-248)
[9]HuangGQ.AStudyofCorrosionPotentialofStainlessSteels ProgressofCorrosionScienceandProtectionEngineeringTechnol ogy[M].Beijing:ChemicalIndustryPress,1999,10:242(黄桂桥.不锈钢在海水中的腐蚀电位研究腐蚀科学与防护工程技术进展[M].北京:化学工业出版社1999,10:242)
[10]LinLY.Studyofcorrosionbehaviorofhome-madeCu-Nial loyinseawater[J].J.Chin.Soc.Corros.Prot.,2000,20(6):361-367(林乐耘.国产B10铜镍合金海水腐蚀行为研究[J].中国腐蚀与防护学报,2000,20(6):361-367)
[11]LiuZC,LinLY,LiuSF,ZhaoYH.Diffusionmechanismofdez incificatonindouble-phasebrassexposedtoseawater[J].Journal ofMaterialResearch,2000,(1):145-149(刘增才.实海暴露双相黄铜脱锌的扩散机制[J].材料研究学报,2000(1):145-149)
[12]ZhuXL.Corrosionlowandmeaninfluencefactorsinseawateren vironmental[J].TheChineseJournalofNonferrousMetals,1998,8(9):210-217(朱小龙.铜合金在海水环境中的腐蚀规律及主要影响因素[J].中国有色金属学报,1998,8(9):210-217)
[13]ShaoYuehong.ThecorrosionofLF6Al-MgalloywithdifferentprocessingandsurfacetreatmentindeepMarineCorrosionand Contral[M].Changsha:ChinaOceanPress,2000,7:544
[14]SongWS.Thecorrosionbehaviorofthelongperiodofaluminum alloyinthefullimmersionandtidalzoneofXimanseaarea[A].ProceedingoftheSecondCorrosionandProtectionConferenceof TwoCoastofChannel[C].Tainan:Cheng-kungUniversityPub lishingHouse,2000,383(宋文桑.铝合金在厦门海域全浸/潮差区长周期的腐蚀行为[A].第二届海峡两岸材料腐蚀与防护研讨会论文集[C].台南:成功大学出版社,2000,383)
[15]LinZJ.Theinfluenceofenvironmentalfactorsoncorrosionsensi tivityofAl-MgalloyinXiamenseaarea[A].Proceedingofthe FirstCorrosionandProtectionConferenceofTwoCoastofChan nel[C].Xiamen:XiamenUniversityPublishingHouse,2000,593(林志坚.厦门海域环境因素对铝镁合金腐蚀敏感性影响的研究[A].第一届海峡两岸材料腐蚀与防护研讨会论文集[C].厦门:厦门大学出版社,2000,593)
[16]ZhuXR,HuangGQ.Evaluationmethodofseawatercorrosivity bymeansofdoubleenvironmentalfactors[J].MarineSciences,2003,(1):65-68(朱相荣.海水腐蚀性双因素环境评价法[J].海洋科学,2003(1):65-68)
[17]DengJuliong.GreyLinerProgrammingInternationalConference onInformationProcessingandManagementofUncertaintyin Knowledge-BasedSystems[M].Qingdao:ParisBasedPress,1986.
[18]LinZJ.Syntheticalevaluationofseawatercorrosionresistantfor somesteels[A].ProceedingoftheSecondCorrosionandProtec tionConferenceofTwoCoastofChannel[C].Tainan:Cheng-kungUniversityPublishingHouse,2000,378(林志坚.几种钢的耐海水腐蚀性能综合评价[A].第二届海峡两岸材料腐蚀与防护研讨会论文集[C].台南:成功大学出版社,2000,378)
[19]LinZJ.Syntheticalevaluationofseawatercorrosionresistanceof carbonsteelsandlowalloysteels[J].MaterialDevelopmentand Application(accepted)(林志坚.碳钢及低合金钢海水耐蚀性综合评价[J].材料开发与应用,待发表)
[1] 周书宇, 刘昌璞, 杨留洋, 耿杰, 范海明, 张大磊, 鞠虹. 在超临界CO2 工况和典型环境因素共影响下的管线钢腐蚀及防护技术研究进展[J]. 中国腐蚀与防护学报, 2026, 46(5): 1353-1368.
[2] 王兴斌, 李家民, 伍登骏, 唐伟能, 杨静, 郭嘉成, 杨欣宇, 侯娟. Al含量对Mg-xAl-Zn合金耐腐蚀性能的影响[J]. 中国腐蚀与防护学报, 2026, 46(5): 1560-1568.
[3] 黄绘, 李树丽, 邓书端, 李向红. MOFs作为防腐蚀材料的研究进展及展望[J]. 中国腐蚀与防护学报, 2026, 46(4): 971-988.
[4] 柯定芳, 吴芳芳, 朱兆彬, 谢声益, 洪静, 陈悦, 李亮, 李昊, 曹发和. 氧化石墨烯/铈基金属有机框架构筑高稳定长耐蚀防护涂层[J]. 中国腐蚀与防护学报, 2026, 46(4): 1095-1106.
[5] 吴健, 姚锡文, 许开立, 许克强. 生物质飞灰粒度与浓度对电站锅炉协同腐蚀损伤特性研究[J]. 中国腐蚀与防护学报, 2026, 46(4): 1148-1158.
[6] 李亮, 殷文昌, 郜阿旺, 韩小乐, 杨延格. 寒带海洋环境下金属材料腐蚀与防护研究进展[J]. 中国腐蚀与防护学报, 2026, 46(3): 629-640.
[7] 张新瑞, 薛宝权, 谭季波, 张兹瑜, 高军, 吴欣强. 含铝奥氏体不锈钢液态铅铋环境相容性研究进展[J]. 中国腐蚀与防护学报, 2026, 46(3): 671-679.
[8] 高金彪, 刘怡, 赵海波, 高清河, 吴禹沈, 于鑫. 超声波调控下聚合物缓蚀剂对金属腐蚀行为的作用机制研究[J]. 中国腐蚀与防护学报, 2026, 46(3): 883-892.
[9] 刘凡, 刘凤莲, 范松海, 邵千秋, 周凯, 李泽瑞, 陈熠东, 文柯成, 张静. 自由基对高压电缆中间接头析氢腐蚀过程的影响[J]. 中国腐蚀与防护学报, 2026, 46(3): 919-930.
[10] 张彭辉, 赵建仓, 姜浩, 彭文山, 丁康康. 极端海域海水环境特征及腐蚀性对比研究[J]. 中国腐蚀与防护学报, 2026, 46(3): 931-937.
[11] 郑彬彬, 周宇航, 朱琦, 张涛, 王福会. 蒸汽锅炉与蒸汽管路异种金属焊接的腐蚀机理研究[J]. 中国腐蚀与防护学报, 2026, 46(2): 381-392.
[12] 陈宇, 魏高飞, 邓书端, 李向红. 碳点缓蚀剂的研究进展及展望[J]. 中国腐蚀与防护学报, 2025, 45(6): 1474-1492.
[13] 孙士斌, 高浩, 常雪婷, 王东胜. 细晶FH40船用低温钢在海水-海冰中耦合失效行为研究[J]. 中国腐蚀与防护学报, 2025, 45(6): 1659-1668.
[14] 史轩铭, 谭季波, 张兹瑜, 吴欣强. 铅冷快堆候选结构材料液态铅铋共晶环境中疲劳行为研究进展[J]. 中国腐蚀与防护学报, 2025, 45(5): 1187-1195.
[15] 方焕杰, 周鹏, 郁健浩, 王永欣, 于波, 蒲吉斌. Ti80合金与船用金属的电偶腐蚀行为研究[J]. 中国腐蚀与防护学报, 2025, 45(4): 905-915.