Please wait a minute...
中国腐蚀与防护学报  2007, Vol. 27 Issue (4): 233-237          
  研究报告 本期目录 | 过刊浏览 |
电化学噪声和电化学阻抗谱监测1Cr18Ni9Ti不锈钢的初期点蚀行为
王梅丰;杜 楠;胡 丽 华
南昌航空工业学院;北京科技大学
MONITORING THE INITIAL PITTING BEHAVIORS OF 1Cr18Ni9Ti STAINLESS STEEL BY ELECTROCHEMICAL NOISE AND ELECTROCHEMICAL IMPEDANCE SPECTROSCOPY
;;
南昌航空工业学院;北京科技大学
引用本文:

王梅丰; 杜楠; 胡丽华 . 电化学噪声和电化学阻抗谱监测1Cr18Ni9Ti不锈钢的初期点蚀行为[J]. 中国腐蚀与防护学报, 2007, 27(4): 233-237 .

全文: PDF(263 KB)  
摘要: 采用电化学噪声和电化学阻抗谱技术,研究1Cr18Ni9Ti不锈钢在3.5% NaCl溶液中的早期腐蚀行为。研究表明,浸泡初期(0 h~48 h),电化学噪声电位、电流在测量时间范围内漂移较小,电位谱功率(PSDV)曲线的斜率几乎不变;电化学阻抗谱在低频下出现感抗特征,表明研究电极表面发生钝化膜破裂与修复的交替过程,即出现了亚稳态蚀点。浸泡中期(48 h~60 h),电化学噪声出现尖峰波动,谱功率曲线的斜率产生突变,电化学阻抗谱的低频感抗特征消失,表明研究电极表面的亚稳态蚀点转化为稳定蚀点。扫描电镜表面形貌分析表明,浸泡60 h后研究电极表面出现明显蚀点。
关键词 : 1Cr18Ni9Ti不锈钢,  点蚀,  电化学噪声,  电化学    
Abstract:The initial pitting of 1Cr18Ni9Ti stainless steel in 3.5% NaCl solution was studied by electrochemical noise(ECN) and electrochemical impedance spectroscopy(EIS). The results indicated that, the initial immersion stage (to 48 hours), the fluctuation amplitude of potential and current noise were small, the slope of the power spectral density of potential(PSDV)plots changed hardly,and an inductive component was observed on impedance plane, which means the formation of the metastable pitting and continuous reparation of the passive film on the surface of the 1Cr18Ni9Ti stainless steel.When immersed to the stage of 48 hours to 60 hours,noise pulse emerged in the plots of electrochemical noise,the slope of the power spectral density (PSD) plots changed suddenly, on the impedance plane inductive component disappeared, which means the transition from metastable to stable pitting. SEM image showed pitting emerged in the surface after immersion for 60 hours.
Key words: 1Cr18Ni9Ti stainless stee    pitting corrosion    ECN    EIS    SEM
收稿日期: 2006-02-13     
ZTFLH:  TG174.2  
[1]Wei B M.Theory and Application of Metal Corrosion Science[M].Beijing:Chemical Industry Press,1984(魏宝明.金属腐蚀学理论及应用[M].北京:化学工业出版社,1984)
[2]Cheng Y F,Wilmott M,Luo J L.Analysis of the role of electrode capacitance on the initiation of pits for A516carbon steel by elec-trochemical noise measurements[J].Corros.Sci.,1999,41(7):1245-1256
[3]Zhang J Q,Zhang Z,Wang J M,et al.Analysis and application of electrochemical noise technologyⅡ.application of electrochemi-cal noise[J].J.Chin.Soc.Corros.Prot.,2002,22(4):241-248(张鉴清,张昭,王建明等.电化学噪声的分析与应用Ⅱ-电化学噪声的应用.中国腐蚀与防护学报[J].2002,22(4):241-248)
[4]Uruchurtu J C,Dawson J L.Noise analysis of pure aluminum under different pitting conditions[J].Corrosion,1987,43(1):19-26
[5]Dong Z H,Guo X P,Zhen J S,et al.Features of ECN of local-ized corrosion for16Mn steel[J].J.Chin.Soc.Corros.Prot.,2002,22(5):290-293(董泽华,郭兴蓬,郑家等.16Mn钢局部腐蚀中的电化学噪声特征.中国腐蚀与防护学报[J].2002,22(5):290-293)
[6]Cao C N.Corrosion Electrochemistry[M].Beijing:Chemical In-dustry Press,2004(曹楚南.腐蚀电化学原理[M].北京:化学工业出版社,2004)
[7]Mansfled F,Sun Z,Hsu C H.Electrochemical noise analysis(ENA)for active and passive systems in chloride media[J].Electrochim.Acta,2001,46(24/25):3651-3664
[8]Gouveia-caridade C,Pereira M I S,Brett C M A.Electrochemical noise and impedance study of aluminium in weakly acid chloride solution[J].Electrochim.Acta,2004,49(5):785-793
[9]Bertocci U,Gabrielli C,Huet F,et al.Noise resistance applied to corrosion measurements I.theoretical analysis[J].J.Electrochem.Soc.,1997,144(1):31-37
[10]Hashimoto M,Miyajima S,Murata T.An experimental study of potential fluctuation during passive film breakdown and repair on iron[J].Corros.Sci.,1992,33(6):905-915
[11]Mojica J,García E,Rodríguez F J,et al.Evaluation of the pro-tection against corrosion of a thick polyurethane film by electro-chemical noise[J].Org.Coat.,2001,42(3/4):218-225
[12]Lee C C,Mansfeld F.Analysis of data for a passive system in the frequency domain[J].Corros.Sci.,1998,40(6):959-962
[13]Cao C N.Introduction of Electrochemical Impedance Spectroscopy[M].Beijing:Science Press,2002(曹楚南.电化学阻抗谱导论[M].北京:科学出版社,2002)
[1] 黎敏, 魏高飞, 邓书端, 李向红. 扫描电化学显微镜(SECM)在缓蚀剂研究中的进展与展望[J]. 中国腐蚀与防护学报, 2026, 46(5): 1326-1342.
[2] 郑凯, 王艺陶, 王东胜, 刘伟, 蒋颖畅, 黄嵘, 常雪婷. 腐蚀-应力耦合作用对极地船用螺旋桨低碳马氏体不锈钢失效机理影响研究[J]. 中国腐蚀与防护学报, 2026, 46(5): 1452-1462.
[3] 曹天慧, 杨砚淇, 刘雨薇, 吴磊, 郭泉忠, 贾志刚, 曹公望, 汪川. 23MnNiMoCr54钢在不同pH的模拟高矿化水中腐蚀机理研究[J]. 中国腐蚀与防护学报, 2026, 46(5): 1537-1548.
[4] 王兴斌, 李家民, 伍登骏, 唐伟能, 杨静, 郭嘉成, 杨欣宇, 侯娟. Al含量对Mg-xAl-Zn合金耐腐蚀性能的影响[J]. 中国腐蚀与防护学报, 2026, 46(5): 1560-1568.
[5] 叶海锋, 沈书成, 陈江华. 增材制造316L不锈钢在不同温度海水环境中的腐蚀行为研究[J]. 中国腐蚀与防护学报, 2026, 46(5): 1569-1578.
[6] 黄胡灵彤, 王成, 程学群, 杨小佳, 张占武, 黎亮. Q235碳钢在模拟南疆土壤中的腐蚀行为[J]. 中国腐蚀与防护学报, 2026, 46(5): 1595-1604.
[7] 俞春林, 顾铭飞, 孙一昂, 袁可鑫, 杨静, 王丽熙, 朱承飞, 朱海奎. 海洋环境中316不锈钢表面喷涂粉末涂层的耐久性评估[J]. 中国腐蚀与防护学报, 2026, 46(5): 1627-1633.
[8] 雍兴跃, 董晓梅, 高新华, 李卓玄, 陈燕飞, 纪灏天. 电化学阻抗谱在有机涂层研究中的应用[J]. 中国腐蚀与防护学报, 2026, 46(4): 945-961.
[9] 柯定芳, 吴芳芳, 朱兆彬, 谢声益, 洪静, 陈悦, 李亮, 李昊, 曹发和. 氧化石墨烯/铈基金属有机框架构筑高稳定长耐蚀防护涂层[J]. 中国腐蚀与防护学报, 2026, 46(4): 1095-1106.
[10] 黄涛, 朱宇, 邓宇, 王岐山, 田一晨, 陈旭. 氢对X65钢及其焊缝力学性能及腐蚀行为影响[J]. 中国腐蚀与防护学报, 2026, 46(4): 1107-1116.
[11] 徐慧强, 赖长清, 王茜茜, 王子明. 基于海水循环模拟系统的牺牲阳极材料对B30传热管腐蚀行为影响研究[J]. 中国腐蚀与防护学报, 2026, 46(4): 1139-1147.
[12] 周炜龙, 郭玉冰, 胡梦茹, 沈凯杰, 杨正桓, 谢林君. 磷酸钠浓度对40Cr钢耐蚀性能的影响[J]. 中国腐蚀与防护学报, 2026, 46(4): 1185-1196.
[13] 陆海峰, 缪强, 梁文萍, 姚志猛, 魏少翀, 陈国星. 激光清洗对不锈钢表面耐腐蚀性能的影响[J]. 中国腐蚀与防护学报, 2026, 46(4): 1227-1237.
[14] 林莉, 毕诗浩, 付磊, 蹇科, 张千. D-酪氨酸增强AH36船体钢四羟甲基硫酸磷杀菌腐蚀防护效用研究[J]. 中国腐蚀与防护学报, 2026, 46(4): 1238-1248.
[15] 李自立, 王欣纪, 田春洋, 叶沛聪, 刘海乔, 何成刚, 刘吉华. NaCl溶液温度和含量对热处理后钢轨腐蚀行为的影响[J]. 中国腐蚀与防护学报, 2026, 46(4): 1279-1288.