OXIDATION BEHAVIOR AND STRENGTH CHARACTERISTICSOF PARTICLE REINFORCED Al2O3/SiC/(W,Ti)CCOMPOSITE CERAMIC TOOL MATERIALS |
;; |
山东轻工业学院机电工程系 |
|
|
Abstract Oxidation behavior of the particle reinforced Al2 O3/SiC/(W,Ti)C composite ceramic tool materials has been studied in detail,as well as the effect of the oxidation on the flexural strength of the material.It is shown that the weight gains in the static oxidation of the material under ai r atmosphere obey the parabolic law.The energy of activation of the material dec reases with the increase in the content of SiC and (W,Ti)C.Residual stresses in the oxidation film can be released with the form of the viscous flowing at high temperature.Therefore,the speed of the oxidation is lowered,and then the oxidat ion resistance of the material can be enhanced to some extent.It is found that t he appropriate oxidation is effective for the improvement of the flexural streng th of Al2O3/SiC/(W,Ti)C ceramic tool material.
|
Received: 11 November 1999
|
|
[1]“HighTechnologyMaterials”compilingcommittee .HighTechnologyMaterials[M ].Beijing :ChinaScienceandTechnologyPress,1993 :2 39- 2 41(《高技术新材料要览》编辑委员会 .高技术新材料要览 [M ].北京 :中国科技出版社 ,1993:2 39- 2 41) [2 ]RiuDH ,ChoiR ,KimHE ,etal.OxidationbehaviorandstrengthofB4 C - 30wt%SiCcompositematerials[J].JMaterSci,1995 ,30 :3897- 390 2 [3]XuChonghai.Designandsimulationofcompositeceramictoolmaterialsandtheirapplication[D].Jinan :ShandongUniversityofTechnology ,1998:10 6 - 118(许崇海 .复相陶瓷刀具材料设计、仿真及其应用研究 [D].济南 :山东工业大学 ,1998:10 6 - 118) [4 ]MinoruMaeda.OxidationresistanceevaluationofSiCceramicswithvariousadditives[J].J .Am .Ceram .Soc.,1989,72 (3) :5 12 - 5 16 [5 ]VinodPareek .OxidationofSiCinenvironmentscontainingpotassiumsaltvapour[J].J .Am .Ceram .Soc .,1991,74(3) :5 5 6 -5 6 0 [6 ]LuJinsheng ,WangBiao ,YaoYingcheng .ManualforthedeterminationofthecommonphasesinsteelsandalloysbyX -ray[M ].Beijing :BeijingInstituteofSteelandIronResearchPress.1990 :78- 80(陆金生 ,王彪 ,姚影澄 .钢和合金中常见相X -射线鉴定手册 [M ].北京 :北京钢铁研究总院出版社 ,1990 :78- 80 ) [7]DengJianxin .DevelopmentofadvancedceramictoolmaterialswiththeadditionofTiB2 andstudyonitsfrictionandwearbe haviorandapplications[D].Jinan :ShandongUniversityofTechnology ,1995 :5 5 - 6 5(邓建新 .添加TiB2 的新型陶瓷刀具材料的开发及其摩擦磨损行为和应用研究 [D].济南 :山东工业大学 ,1995 :5 5 -6 5 ) [8]Erwin .OxidationbehaviorofSiCceramics[J].JAmCeramSoc ,195 8,41(3) :347- 349 [9]KimHE .OxidationbehaviorandflexuralstrengthofAlNexposedtoairatelevatedtemperature[J].J.Am .Ceram .Soc .,1994,77(4 ) :10 37- 10 42 [10 ]BoromMP .Astudyofmechanicalpropertiesof 3Al2 O3·2SiO2 atelevatedtemperature[J].Ceram .Eng .Sci.Proc.,1989,8(7) :6 5 4- 6 5 8 [11]LevinEM ,RobbinsCR ,McMurdieHF ,eds .PhaseDiagramsforCeramists[M ].OH :TheAm .Ceram .Soc.,196 4,Vol1:2 6 1- 2 6 3 [12 ]LangeFF .HealingofsurfacecracksinSiCbyoxidation[J].J.AmCeram .Soc .,1970 ,5 3(2 ) :2 90 - 2 93 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|