Study on Preparation and Corrosion Resistance of Conductive Polyaniline Coating on Aluminum by Electropolymerization
;;;
湖南科技大学南校区化学化工学院;中南大学化学化工学院
Cite this article: 

;. Study on Preparation and Corrosion Resistance of Conductive Polyaniline Coating on Aluminum by Electropolymerization. J Chin Soc Corr Pro, 2008, 28(1): 11-15 .

Download:  PDF(1205KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Polyaniline (PANI) films are deposited on aluminum substrate through electrochemical process and the corrosion resistance of PANI films is studied. The results show metallic nickel of nonelectrolytic deposition on the aluminum surface can catalyze electropolymerization of aniline.The proper upper scanning potential through cyclic voltammetry is not more than 0.7 V(vs. Hg/Hg2SO4); the polymerization potential range through potentio?鄄static is between 0 and 0.45 V(vs. Hg/Hg2SO4); the current density through galvanostatic is not more than 0.3 mA/cm2;the proper electrolytic pH value is at range of 2 to 3.The potentiodynamic polarization curves in 0.5 mol/L sodium chloride solution show that the pitting corrosion potentials of aluminum electrodes coated with PANI through cyclic voltammetry,potentiostatic or galvanostatic method shift toward positive direction as compared with pure aluminum electrode.The PANI coating could improve the pitting corrosion resistance of aluminum and its alloy.
Key words:       
Received:  18 July 2006     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.jcscp.org/EN/     OR     https://www.jcscp.org/EN/Y2008/V28/I1/11

[1]Zhang H,Yu Z M,Sun W C.Interface microstructure and corro-sion resistance of electrodeposited Cr coating on aluminum over-laid LY12[J].Corros.Sci.Prot.Technol.,2003,23(6):352-355(张慧,于志明,孙伟成.包铝LY12铝合金表面镀铬层的界面显微组织及耐蚀性能[J].腐蚀科学与防护技术,2003,23(6):352-355)
[2]Li G Q,Li D,Li J Q,et al.Cerium conversion coatings formed on anodized aluminum by cathodic electrolysis[J].J.Chin.Soc.Corros.Prot.,2001,21(3):150-157(李国强,李荻,李久青.铝阳极氧化膜上阴极电解沉积的稀土铈转化膜[J].中国腐蚀与防护学报,2001,21(3):150-157)
[3]Long X Q,Shao R K.Investigation of corrosion-resistance of chemical conversion film and phosphating primer on2024Alu-minium alloy[J].J.Chin.Soc.Corros.Prot.,2003,23(3):56-159(隆小庆,邵荣宽.2024铝合金化学转化膜与磷化底漆耐蚀性的研究[J].中国腐蚀与防护学报,2003,23(3):157-159)
[4]Xin T Z,Zhao W S,Liu J C,Characteristics and principle analysis of micro arc oxidation on Al alloy surface[J].Surf.Technol.2006,35(1):14-17(辛铁柱,赵万生,刘晋春.铝合金微弧氧化过程的特性研究及机理分析[J].表面技术,2006,35(1):14-17)
[5]Deberry D W.Modification of the electrochemical and corrosion behavior of stainless steel with electroactive coating[J].J.Elec-trochem.Soc.,1985,132(5):1022-1026
[6]Jing X L,Wang Y Y,Qiang J F.Anti-corrosion property of e-meraldine base form of polyaniline[J].J.Chin.Soc.Corros.Prot.,2004,24(5):301-305(井新利,王杨勇,强军锋.本征态聚苯胺的防腐性能[J].中国腐蚀与防护学报,2004,24(5):301-305)
[7]Jiang Y F,Zhai C Q,Guo X W,et al.Growth of polyaniline film on AZ91magnesium alloy surface[J].Mater.Rev.,2003,17(4):70-72(蒋永锋,翟春泉,郭兴伍等.聚苯胺膜在AZ91镁合金表面的生长过程[J].材料导报,2003,17(4):70-72)
[8]Wang S L,Long J M,Wang J.Corrosion resistance of polyaniline coating on low carbon steel[J].Corros.Prot.,2004,25(4):142-145(王少龙,龙晋明,王静.低碳钢基体上电沉积聚苯胺膜及耐蚀性研究[J].腐蚀与防护,2004,25(4):142-145)
[9]Pournaghi-Azar M H,Ramzmi-Nerbin H.Voltammetric behaviour and electrocatalytic activity of the aluminum electrode modified with nickel and nickel hexacyanoferrate films,prepared by elec-troless deposition[J].J.Electroanal.Chem.,1998,456:83-90
[10]Thompson G E.Porous anodic alumina:fabrication,characteriza-tion and applications[J].Thin Solid Films,1997,297:192-201
[11]Lai X J,Zuo L Cui.One-step synthesis of oriented polyaniline nanorods through electrochemical deposition[J].Polym.Bull.,2006,online
[12]Wen J B,Zhou H H,Li S L,et al.Growth process of nano-fibrous polyaniline film on stainless Steel[J].Acta Phys.Chim.Sin.,2006,22(1):106-109(温靖邦,周海晖,李松林等.纳米纤维聚苯胺膜在不锈钢电极表面的生长过程[J].物理化学学报,2006,22(1):106-109)
[13]Dong P,Zhou J Z,Xi Y Y,et al.The growth mechanism of elec-trosynthesized polyaniline nanotubules in aluminua template[J].Acta Phys.Chim.Sin.,2004,20(5):454-458(董平,周剑章,席燕燕等.聚苯胺纳米管在阳极氧化铝模板中电聚合的生长机理[J].物理化学学报,2004,20(5):454-458)
[1] SUN Xiaoguang, WANG Rui, ZHANG Zhiyi, HAN Xiaohui, LI Gangqing. On-line Corrosion Monitoring Technology for High-speed Train in Dynamic Service Circumstance[J]. 中国腐蚀与防护学报, 2022, 42(3): 441-446.
[2] LUAN Hao, MENG Fandi, LIU Li, CUI Yu, LIU Rui, ZHENG Hongpeng, WANG Fuhui. Preparation and Anticorrosion Performance of M-phenylenediamine-graphene Oxide/Organic Coating[J]. 中国腐蚀与防护学报, 2021, 41(2): 161-168.
[3] YAN Zhu, ZHANG Chenyang, WANG Lixin, YUAN Guo, ZHANG Yuanxiang, FANG Feng, WANG Yang, KANG Jian. Effect of Structural Stability on Electrochemical Corrosion Properties of Zr-based Amorphous Alloy[J]. 中国腐蚀与防护学报, 2022, 42(1): 79-84.
[4] Chun-Yu WANG Hao-Zhe JIN. Study on the Corrosion Mechanism of Air Cooler in a CO2 Removal System with Amine Solution[J]. 中国腐蚀与防护学报, 0, (): 0-0.
[5] WAN Hongxia, LIU Chonglin, WANG Zian, LIU Ru, CHEN Changfeng. Corrosion Behavior of P110S Oil Casing Steel in Sulfur Containing Environment[J]. 中国腐蚀与防护学报, 2023, 43(2): 371-376.
[6] CHENG Qidong, WANG Yanhua. Effect of Surface Scratches on Corrosion Behavior of 304 Stainless Steel Beneath Droplets of Solution (0.5 mol/L NaCl+0.25 mol/L MgCl2)[J]. 中国腐蚀与防护学报, 2022, 42(1): 99-105.
[7] YANG Haifeng, YUAN Zhizhong, LI Jian, ZHOU Naipeng, GAO Feng. Effect of Ni Content on Corrosion Behavior of Cu-bearing Aged Weldable Steels in a Simulated Tropical Marine Atmosphere[J]. 中国腐蚀与防护学报, 2023, 43(5): 1022-1030.
[8] MEI Jiaxue, DU Zunfeng, ZHU Haitao. Ultimate Bearing Capacity of Ship Structure Based on Random Corrosion[J]. 中国腐蚀与防护学报, 2022, 42(4): 662-668.
[9] LIAO Minxing, LIU Jun, DONG Baojun, LENG Xuesong, CAI Zelun, WU Junwei, HE Jianchao. Effect of Salt Spray Environment on Performance of 1Cr18Ni9Ti Brazed Joint[J]. 中国腐蚀与防护学报, 2023, 43(6): 1312-1318.
[10] XIE bin. Corrosion Inhibition Performance of Diethylammonium O,O'-Di(2-phenylethyl)dithiophosphate for Q235 Steel in HCl Solution[J]. , 0, 0(0): 0-0.
[11] wan hongxia. Comparative study on the corrosion of X65 pipeline steel welded joint in shallow and deep sea[J]. , 0, 0(0): 0-0.
[12] YI Junda, LENG Ao, GONG Delun, WEI Boxin. Microstructureand Properties of Low Modulus Corrosion-resistant Metastable β-Ti Alloy Prepared by Electron Beam Melting[J]. 中国腐蚀与防护学报, 2026, 46(1): 49-59.
[13] LI Jiayuan, ZENG Tianhao, LIU Youtong, WU Xiaochun. Corrosion Behavior of 4Cr16Mo Martensite Stainless Steel with 1% Cu Addition by Applied Stress[J]. 中国腐蚀与防护学报, 2023, 43(5): 1094-1100.
[14] JI Yuefei, HAO Long, WANG Jianqiu, LI Qinghua, ZHENG Yue, YU Pei, KE Wei. Research Progress on Compatibility Between Alkalizing Agents and Materials in PWR Secondary Circuit[J]. 中国腐蚀与防护学报, 2024, 44(2): 267-277.
[15] LIU Jing, CHEN Xuandong, YU Aiping, GONG Xinzhi. Multi-phase Mesoscopic Numerical Simulation of Chloride Ion Diffusion in Recycled Aggregate Concrete[J]. 中国腐蚀与防护学报, 2023, 43(5): 1111-1118.
No Suggested Reading articles found!