FACTORS EFFECTING ON THE HYDROGEN EVOLUTION ON Al-ANODES IN STRONG ALKALINE SOLUTION
Yusu Song;Yan Zhang;Liqing Zhou
武汉海军工程大学兵器工程系
Download:  PDF(222KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  By means of the constant current gathering volumes of hydrogen evolution,potentiodynamic and the surface corrosion morphology observed,the effect factors of the hydrogen evolution on Al anodes in strong alkaline solution were studied.The factors includes the alloying elements,the concentration of KOH solution,the temperature and the anti-hydrogen evolution agents.The aluminum alloy anode which contains mixed rare earth elements(RE) had the lower se lf-corrosion property and the hydrogen evolution rate in its surface also decreased greatly.When the concentration of KOH solution was 4 mol/L,the anode had the better activity and the lowest H2-evolution rate,The higher the temperature,the faster the H2-evolution rate.The anti-hydrogen evolution agents (eg.aminophenol) could reduce the H2-evolution rate.The results showed that the mixed rare earth(RE) aluminum alloy,4 mol/L KOH solution and the 0.4 mol/L o-aminophenol additive were suitable conditions to reduce the hydrogen evolution rate on the surface of A l-anodes,especially at the high temperature.
Key words:  hydrogen evolution      Al anode      the alkaline solution      
Received:  21 January 2005     
ZTFLH:  TG174.42  
Corresponding Authors:  Yusu Song     E-mail:  caosys@263.net

Cite this article: 

Yusu Song; Yan Zhang; Liqing Zhou. FACTORS EFFECTING ON THE HYDROGEN EVOLUTION ON Al-ANODES IN STRONG ALKALINE SOLUTION. J Chin Soc Corr Pro, 2006, 26(4): 237-240 .

URL: 

https://www.jcscp.org/EN/     OR     https://www.jcscp.org/EN/Y2006/V26/I4/237

[1]Ma Z Q,Li W X,Wang R C.Study on the electro-chemical perfor-mance of aluminum anodes in alkaline electrolytes[J].Journal ofPower Sources,2002,26(3):365-368(马正青,黎文献,王日初.铝合金阳极在碱性介质中的电化学性能研究[J].电源技术,2002,26(3):365-368)
[2]Wilhelmsenw,Arnesent,Hasvold,et al.,The electrochemical behav-ior of Al in alloys in alkaline electrolytes[J].Electrochemica Acta,1991,36(1):79-85
[3]MacDonald D D,Silvia Real.Evaluation of alloy anodes for alu-minum-air batteries[J].J.Electrochem.Soc.,1988,135(10):2410-2411
[4]Song Y S,Zhang Y,Wang S Z.Electrochemical behavior of alu-minum alloy anodes with the mixed rare earth elements in KOH so-lution[J].J.Yunnan University,2004,26(4A):213-215(宋玉苏,张燕,王树宗.稀土铝阳极在KOH溶液中的电化学行为[J].云南大学学报,2004,26(4A):213-215)
[5]MacDonald D D,Silvia Real.Development of anodes for aluminum/air batteries-solution phase inhibition of corrosion[J].J.AppliedElectrochemistry,1990,20:405-408
[6]Shao H B,Wang J M,Zhang Z,et al.The cooperative of calciumions on the corrosion inhibition of pure aluminum in an alkaline solu-tion[J].Mater.Chem.Phy.,2002,77:305-309
[7]Zhang Y.Research on the rare earth aluminum anode and inhibitionof hydrogen evolution for the aluminum high energy battery[D].Wuhan:Naval University of Engineering,2003(张燕.强碱性介质铝阳极材料和抑氢剂的研究[D].硕士学位论文,武汉:海军工程大学,2003)
[1] SUN Haijing, QIN Ming, LI Lin. Performance of Al-Zn-In-Mg-Ti Sacrificial Anode in Simulated Low Dissolved Oxygen Deep Water Environment[J]. 中国腐蚀与防护学报, 2020, 40(6): 508-516.
[2] JIA Yizheng, WANG Baojie, ZHAO Mingjun, XU Daokui. Effect of Solid Solution Treatment on Corrosion and Hydrogen Evolution Behavior of an As-extruded Mg-Zn-Y-Nd Alloy in an Artificial Body Fluid[J]. 中国腐蚀与防护学报, 2020, 40(4): 351-357.
[3] Mingyuan JIAO, Weiliang JIN, Jianghong MAO, Teng LI, Jin XIA. Effect of Concrete Inner Environment on Hydrogen Evolution of Rebar During ElectrochemicalRemediation[J]. 中国腐蚀与防护学报, 2018, 38(5): 463-470.
[4] Teng LI, Weiliang JIN, Chen XU, Jianghong MAO. Determination of Steady Critical Current Density of Hydrogen Evolution During Electrochemical Repair Process of Reinforced Concrete[J]. 中国腐蚀与防护学报, 2017, 37(4): 382-388.
[5] ZHAO Guoqiang, WEI Yinghua, LI Jing. Current Efficiency and Corrosion Mechanism of Al-Zn-In Sacrificial Anode at Different Current Densities[J]. 中国腐蚀与防护学报, 2015, 35(1): 69-74.
[6] HOU Juncai, LIANG Guojun, QIAO Jinhua, ZHANG Qiumei. LOW Mn CONTENT MAGNISIUM SACRIFICIAL ANODE[J]. 中国腐蚀与防护学报, 2012, 32(5): 403-406.
[7] HU Shengnan, ZHANG Tao, SHAO Yawei, MENG Guozhe, WANG Fuhui. EFFECT OF CYCLIC HYDROSTATIC PRESSURE ON SACRIFICIAL ANODE CATHODIC PROTECTION[J]. 中国腐蚀与防护学报, 2012, 32(3): 241-246.
[8] HUANG Yanbin, SONG Gaowei, LIU Xuebin1 DING Huadong, YAN Yonggui, SHAO Xinhai. CORROSION PROTECTION OF Al-Zn-In-Mg-Ga-Mn ALUMINOUS SACRIFICIAL ANODE[J]. 中国腐蚀与防护学报, 2012, 32(1): 44-47.
[9] HOU Juncai, ZHANG Qiumei. CURRENT STATUS OF HIGH POTENTIAL MAGNESIUM SACRIFICIAL ANODES[J]. 中国腐蚀与防护学报, 2011, 31(2): 81-85.
[10] MA Li, LI Weili, ZENG Hongjie, YAN Yonggui,HOU Baorong. LOW DRIVING VOLTAGE Al-Ga SACRIFICIAL ANODE AND ITS ACTIVATION MECHANISM[J]. 中国腐蚀与防护学报, 2010, 30(4): 329-332.
[11] KONG Xiaodong; DING Zhenbin; ZHU Meiwu. EFFICIENCY AND EFFECTING FACTORS OF Mg CONTAINING Al ALLOY SACRIFICIAL ANODES[J]. 中国腐蚀与防护学报, 2010, 30(1): 6-10.
[12] . Activation behavior of aluminum sacrificial anodes in sea water[J]. 中国腐蚀与防护学报, 2008, 28(3): 186-192 .
[13] ;. EFFECT OF SMALL ADDITION OF STRONTIUM ONMICROSTRUCTURE AND ELECTROCHEMICALPERFORMANCE OF Mg-Mn SACRIFICIAL ANODE[J]. 中国腐蚀与防护学报, 2006, 26(3): 166-170 .
[14] ;. EVALUATION PERFORMANCE OF SACRIFICIAL ANODE USING GALVANIC CURRENT[J]. 中国腐蚀与防护学报, 2005, 25(3): 176-178 .
[15] . Corrosion Behavior of AZ91D Magnesium Alloy in Hand Sweat 1.Effect of hand sweat composition on the corrosion behavior of AZ91D magnesium alloy[J]. 中国腐蚀与防护学报, 2004, 24(5): 276-279 .
No Suggested Reading articles found!