Please wait a minute...
中国腐蚀与防护学报  2008, Vol. 28 Issue (4): 219-224          
  研究报告 本期目录 | 过刊浏览 |
镁合金表面微弧氧化陶瓷膜的腐蚀失效机理
王立世;潘春旭;蔡启舟;魏伯康
武汉大学物理科学与技术学院
Study on Corrosion Failure Mechanism of Microarc Oxidation Coatings Formed on AZ91D Magnesium Alloy
;;;
引用本文:

王立世; 潘春旭; 蔡启舟; 魏伯康 . 镁合金表面微弧氧化陶瓷膜的腐蚀失效机理[J]. 中国腐蚀与防护学报, 2008, 28(4): 219-224 .
, , , . Study on Corrosion Failure Mechanism of Microarc Oxidation Coatings Formed on AZ91D Magnesium Alloy[J]. J Chin Soc Corr Pro, 2008, 28(4): 219-224 .

全文: PDF(1442 KB)  
摘要: 本文评价了镁合金两类微弧氧化(Microarc Oxidation-MAO)膜层的耐蚀性,并分析了其在5wt.%NaCl水溶液中的腐蚀失效机理。研究发现:磷酸盐系膜层(P-film)和硅酸盐系膜层(Si-film)均可极大提高AZ91D合金的耐蚀性能,但硅酸盐系膜层的耐蚀性要优于磷酸盐系膜层的耐蚀性;依据Si-film和P-film在在5wt.%NaCl溶液中不同浸泡时间的自腐蚀电位(OCP)、腐蚀形貌和交流阻抗谱(EIS)数据的变化,MAO膜层的腐蚀失效主要经历了以下四个阶段:溶液渗入多孔层的孔隙;一些孔隙内被腐蚀产物充满;微孔底部的阻挡层逐渐被腐蚀;阻挡层失效,腐蚀过程趋于稳定。
关键词 : 微弧氧化,  镁合金,  腐蚀失效    
Abstract:The corrosion resistance of the two types of microarc oxidation (MAO) coatings was evaluated by virtue of total immersion test and salt spray. Then the mechanism of the coating corrosion failure in 5wt.%NaCl aqueous solution was studied through the impedance and open-circuit potential (OCP) measurements. The results showed that both phosphate coating (P-film) and silicate coating (Si-film) could enhance the corrosion resistance of AZ91D alloy significantly and that the later was more effective. Based on the variations of OCP and corrosion morphology of P-film and Si-film immersed in 5wt.%NaCl aqueous solution with different time, the analytic results of electrochemical impedance spectroscopy (EIS) data for Si-film showed the corrosion failure process had experienced the following four steps: the rapid initial penetration of the solution into the porous outer layer; the filling of corrosion products in certain pores; the gradual corrosion of the barrier layer located in the bottom of pores; the stable corrosion process with the failure of barrier layer.
Key words: microarc oxidation    magnesium alloy    corrosion failure
收稿日期: 2006-11-22     
ZTFLH:  TG146.2  
[1]Yerokhin AL,Nie X,Leyland A,et al.Plasma electrolysis for sur-face engineering[J].Surf.Coat.Technol.,1999,122:73-79
[2]Jiang B L,Zhang S F,Wu G J.The study of the corrosion resis-tance of the ceramic coatings formed by micro-arc oxidation onthe Mg-base alloy[J].J.Chin.Soc.Corros.Prot.,2002,22(5):300-303(蒋百灵,张淑芬,吴国建.镁合金微弧氧化陶瓷层耐蚀性的研究[J].中国腐蚀与防护学报,2002,22(5):300-303)
[3]Wang Y H,Wang J,Zhang J B.Influence of micro-arc oxidationtreatment on the corrosion behavior of AZ91D magnesium alloy[J].J.Chin.Soc.Corros.Prot.,2006,26(4):216-220(王燕华,王佳,张际标.微弧氧化处理对镁合金腐蚀行为的影响[J].中国腐蚀与防护学报,2006,26(4):216-220)
[4]Emley E F.Principles of Magnesium Technology[M].New York:Pergamon Press,1966:670-735
[5]Barton T F,Johnson C B.The effect of electrolyte on the anodizedfinish of a magnesium alloy[J].Plat.Surf.Finish.,1995,(5):138-141
[6]Khaselev O,Weiss D,Yahalom J.Anodizing of pure magnesiumin KOH-aluminate solutions under sparking[J].J.Electrochem.Soc.,1999,146(5):1757-1761
[7]Khaselev O,Weiss D,Yahalom J.Structure and composition ofanodic film formed on binary Mg-Al alloys in KOH-aluminate so-lutions under continuous sparking[J].Corros.Sci.,2001(7),43:1295-1307
[8]Shi Z M,Song G L,Atrens A.Influence of theβphase on thecorrosion performance of anodised coatings on magnesium-alu-minium alloys[J].Corros.Sci.,2005,47(11):2760-2777
[9]Wang L S,Cai Q Z,Wei B K.Introduction of several foreign mi-cro-arc oxidation processes on magnesium alloys[J].Mater.Prot.,2004,(7):61(王立世,蔡启舟,魏伯康.国外几个镁合金微弧氧化工艺介绍[J].材料保护,2004,37(7):61)
[10]Cai Q Z,Wang L S,Wei B K.Electrochemical performance ofmicroarc oxidation films formed on AZ91D magnesium alloy in sil-icate and phosphate electrolytes[J].Surf.Coat.Technol.,2006,200(12-13):3727-3733
[11]Zao S P,Lu S K,Hao W J.Titanium Alloy and Its Surface Treat-ment[M].Haerbin:Haerbin Institute of Technology Press,2003:183-257(赵树萍,吕双坤,郝文杰.钛合金及其表面处理[M].哈尔滨:哈尔滨工业大学出版社,2003:183-257)
[12]Birss V,Xia S,Yue R,et al.Characterization of oxide filmsformed on Mg-based WE43 alloy using AC/DC anodization in sili-cate solutions[J].J.Electrochem.Soc.,2004,B151(1):1-10a
[1] 曾崎, 虞文军, 门向南, 冯保净, 杨耀, 朱凯, 葛玉麟, 应韬, 曾小勤. 高强耐蚀稀土镁合金研究进展[J]. 中国腐蚀与防护学报, 2026, 46(5): 1415-1424.
[2] 张春艳, 张瑜心, 陈必秀, 于宝兴, 周鹏. 铸造缺陷对AZ91D镁合金Mn-P系化学转化膜耐蚀性能的影响[J]. 中国腐蚀与防护学报, 2026, 46(5): 1475-1484.
[3] 张晓晨, 杨闯, 姜旭, 陈永生, 赵佳祥, 赵阳, 周鹏, 张涛, 王福会. 镁合金的一种致密微弧氧化涂层工艺及性能的研究[J]. 中国腐蚀与防护学报, 2026, 46(4): 1218-1226.
[4] 张云, 张宇鹏, 董泽华, 张欣欣. 再生镁合金表面微弧氧化/水滑石复合膜层的一步法制备及其耐蚀性能研究[J]. 中国腐蚀与防护学报, 2026, 46(2): 441-449.
[5] 施艳, 饶智航, 缪程平, 张洋, 陈赵扬, 屠晓华, 李加友, 褚有群. 铜封端负载8-HQ埃洛石纳米管镁合金微弧氧化自修复涂层的制备及耐蚀性能[J]. 中国腐蚀与防护学报, 2026, 46(2): 511-522.
[6] 许诗源, 孟鑫, 杨亚璋, 刘辰, 张昭, 方晓祖. 腐蚀形貌对镁合金电化学阻抗谱特征的影响研究[J]. 中国腐蚀与防护学报, 2025, 45(6): 1589-1598.
[7] 何江海, 杨子钰, 刘琦, 马子骅, 何伟, 陈飞. 在电解液中添加陶瓷颗粒对钛合金表面微弧氧化膜层改性的研究进展[J]. 中国腐蚀与防护学报, 2025, 45(5): 1175-1186.
[8] 蔡科涛, 季磊, 张震, 冯强, 邓伟林, 兰贵红, 何莎, 赵占勇, 白培康. Mg-Gd-Y-Zn-Zr合金在NaCl和Na2SO4 溶液中腐蚀行为研究[J]. 中国腐蚀与防护学报, 2025, 45(5): 1289-1299.
[9] 张雄斌, 党恩, 于晓婧, 汤玉斐, 赵康. 油气田用马氏体不锈钢腐蚀性能研究现状与进展[J]. 中国腐蚀与防护学报, 2025, 45(4): 837-848.
[10] 翟亚如, 熊金平, 赵景茂. 3.5%NaCl溶液中硝基巴比妥酸对AZ31B与AZ91D镁合金腐蚀的缓蚀作用及机理研究[J]. 中国腐蚀与防护学报, 2025, 45(4): 916-926.
[11] 魏然, 蒋全通, 孙琛, 王伟伟, 段继周, 侯保荣. 镁合金在海洋环境中的腐蚀与防护研究[J]. 中国腐蚀与防护学报, 2025, 45(3): 533-547.
[12] 张超, 陈俊航, 邹士文, 张欢, 李曌亮, 肖葵. Mg-Gd-Y-Zr合金在模拟沿海贮存环境下的腐蚀行为与机理研究[J]. 中国腐蚀与防护学报, 2025, 45(3): 731-738.
[13] 魏珂正, 蒋文龙, 龚奕维, 裘欣, 丁汉林, 项重辰, 王子健. 时效时间对锻态AZ80镁合金第二相析出及柱面取向表面腐蚀性能的影响[J]. 中国腐蚀与防护学报, 2024, 44(6): 1557-1565.
[14] 刘元海, 李玉珠, 郁大照, 慕仙莲, 刘杰. 印制电路板在服役环境中的腐蚀失效行为研究进展[J]. 中国腐蚀与防护学报, 2024, 44(5): 1145-1156.
[15] 尹洁, 高永浩, 易芳. Ag微合金化对Mg-Zn-Ca合金微观组织及腐蚀行为的影响[J]. 中国腐蚀与防护学报, 2024, 44(5): 1274-1284.