Please wait a minute...
中国腐蚀与防护学报  2010, Vol. 30 Issue (6): 433-436    
  研究报告 本期目录 | 过刊浏览 |
稀硫酸中丙烯基硫脲对纳米工业纯铁腐蚀作用
沈长斌1,杨怀玉2,王胜刚3,龙康2,王福会2
1. 大连交通大学材料科学与工程学院 大连 116028
2. 中国科学院金属研究所金属腐蚀与防护国家重点实验室 沈阳 110016
3. 中国科学院金属研究所 沈阳材料科学国家(联合)实验室 沈阳 110016
CORROSIVE EFFECT BY ALLYLTHIOUREA OF BULK NANOCRYSTALLINE INGOT IRON IN AMBIENT DILUTED ACIDIC SULPHATE SOLUTION
SHEN Changbin1, YANG Huaiyu2, WANG Shenggang3, LONG Kang2, WANG Fuhui2
1. School of Materials Science & Engineering, Dalian Jiaotong University, Dalian 116028
2. State Key Laboratory for Corrosion and Protection, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
3. Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
全文: PDF(626 KB)  
摘要: 在室温0.1 mol/L H2SO4+0.25 mol/L Na2SO4 溶液中,研究了添加不同浓度丙烯基硫脲(ATU)对块体纳米晶工业纯铁(BNII)(通过严重塑性变形获得)和普通工业纯铁(CPII)电化学腐蚀行为的影响。当浸泡5 min后, CPII 的 Nyquist谱图上出现感抗弧,而BNII的Nyquist谱图为单阻抗谱。随着时间延长至2 h,BNII的Nyquist 谱图上出现两个时间常数;CPII的阻抗复平面上出现一圆心下偏的单阻抗谱。
关键词 块体纳米晶工业纯铁(BNII)丙烯基硫脲(ATU)硫酸    
Abstract:In the corrosive solution 0.1 mol/L H2SO4+0.25 mol/L Na2SO4, the effect of allyl-thiourea (ATU) on the corrosion behaviors of bulk nanocrystalline ingot iron (BNII) was studied. Inhibited by ATU at ambient temperature, for CPII, when immersion time as short as 5 min, an inductive loop appeared at different concentrations at the Nyquist complex planes; for BNII, only a simple capacitance loop appeared in the Nyquist plot at the same period. With the elongation of the immersion time, for BNII, two time constants appeared in the Nyquist plot; For CPII, the impedance spectrum shows a slightly depressed semicircular shape.
Key wordsbulk nanocrystalline ingot iron (BNIN)    allyl-thiourea (ATU)    acidic sulphate solution
收稿日期: 2009-03-18     
基金资助:

国家自然科学基金项目(50501023)资助

通讯作者: 沈长斌     E-mail: shencb@djtu.edu.cn
作者简介: 沈长斌,男,1972出生,副教授,研究方向为金属材 料腐蚀与防护

引用本文:

沈长斌,杨怀玉,王胜刚,龙康,王福会. 稀硫酸中丙烯基硫脲对纳米工业纯铁腐蚀作用[J]. 中国腐蚀与防护学报, 2010, 30(6): 433-436.
CHEN Zhang-Bin, YU Fu-Hui, YANG Huai-Yu, YU Qing-Gang, MANG Kang. CORROSIVE EFFECT BY ALLYLTHIOUREA OF BULK NANOCRYSTALLINE INGOT IRON IN AMBIENT DILUTED ACIDIC SULPHATE SOLUTION. J Chin Soc Corr Pro, 2010, 30(6): 433-436.

链接本文:

https://www.jcscp.org/CN/      或      https://www.jcscp.org/CN/Y2010/V30/I6/433

[1] Bentiss F, Lebrini M, Lagrenee M.Thermodynamic characterization of metal dissolution and inhibitor adsorption processes in mild steel/2,5-bis(n-thienyl)-1,3,4-thiadiazoles/hydrochloric acid system [J]. Corros. Sci., 2005, 47(12): 2915-2931

[2] Lukovits I, Shaban A, Kalman E. Thiosemicarbazides and thiosemicarbazones: non-linear quantitative structure-efficiency model of corrosion inhibition [J]. Electrochim. Acta, 2005, 50(20): 4128-4133

[3] Baddini Q, Cardoso S, Hollauer E, et al. Statistical analysis of a corrosion inhibitor family on three steel surfaces (duplex, super-13 and carbon) in hydrochloric acid solutions [J]. Electrochim. Acta,2007, 53(2): 434 -446

[4] Thompson I, Campbell D. Interpreting Nyquist responses from defective coatings on steel substrates [J].Corros. Sci., 1994, 36(1): 187-198

[5] Wang S G, Shen C B, Long K, et al. The electrochemical corrosion of bulk nanocrystalline ingot iron in acidic sulphate solution [J]. J. Phys. Chem.,2006, 110B: 377-382

[6] Pardo A, Otero E, Merino M C, et al. The influence of Cr addition on the corrosion resistance of Fe73.5Si13.5B9Nb3-Cu1 metallic glass in marine environments [J]. Corros. Sci., 2002, 44(6): 1193-1211

[7] Wang S G, Long K, Long Q W. Refinement of pure iron grain by severe rolling technology [J]. Acta Metall. Sin., 2003, 39: 1247-1250

    (王胜刚, 龙康, 龙期威. 深度轧制细化工业纯铁晶粒 [J]. 金属学报,2003, 39: 1247-1250)

[8] Lopez M, Arce M. Characterization of Co-Cu mechanical alloys by linear sweep voltammetry [J]. Electrochim. Acta, 1997, 42(1): 61-65

[9] Shen C B, Wang S G, Yang H Y, et al. Electrochemical corrosion behavior of bulk nanostructured industrial pure iron in hydrochloric acid solution [J]. Mater. Sci. Technol., 2006, 14(3), 316-319

    (沈长斌, 王胜刚, 杨怀玉等. 块体纳米晶工业纯铁在盐酸溶液中的电化学腐蚀行为[J]. 材料科学与工艺, 2006, 14(3), 316-319)

[10] Shen C B, Wang S G, Long K, et al. Corrosion inhibition of bulk nanocrystallized industrial pure iron by thiourea in HCl [J]. Acta Phys-Chem. Sin., 2004, 20(6), 664-667

     (沈长斌, 王胜刚, 杨怀玉等. 硫脲对纳米晶工业纯铁在盐酸溶液中的缓蚀行为 [J]. 物理化学学报, 2004, 20(6), 664-667)

[11] Cao C N, Zhang J Q. The Introduction to Electrochemical Impedance Spectrum [M]. Beijing:Science Press, 2002: 135

     (曹楚南, 张鉴清. 电化学阻抗谱导论 [M]. 北京: 科学出版社, 2002: 135)

[12] Tan Y J, Bailey S, Kinsella B. An investigation of the formation and destruction of corrosion inhibitor films using electrochemical impedance spectroscopy (EIS) [J]. Corros. Sci., 1996, 38(9): 1545-1561
[1] 董续成, 管方, 徐利婷, 段继周, 侯保荣. 海洋环境硫酸盐还原菌对金属材料腐蚀机理的研究进展[J]. 中国腐蚀与防护学报, 2021, 41(1): 1-12.
[2] 王欣彤, 陈旭, 韩镇泽, 李承媛, 王岐山. 硫酸盐还原菌作用下2205双相不锈钢在3.5%NaCl溶液中应力腐蚀开裂行为研究[J]. 中国腐蚀与防护学报, 2021, 41(1): 43-50.
[3] 李向红, 邓书端, 徐昕. 木薯淀粉三元接枝共聚物对钢在H2SO4溶液中的缓蚀性能研究[J]. 中国腐蚀与防护学报, 2020, 40(2): 105-114.
[4] 陈旭, 李帅兵, 郑忠硕, 肖继博, 明男希, 何川. X70管线钢在大庆土壤环境中微生物腐蚀行为研究[J]. 中国腐蚀与防护学报, 2020, 40(2): 175-181.
[5] 刘志峰,朱志平,石纯,黄赵鑫. 载流法制备硫酸露点腐蚀模拟气体的试验研究[J]. 中国腐蚀与防护学报, 2020, 40(1): 1-9.
[6] 陈旭,马炯,李鑫,吴明,宋博. 温度与SRB协同作用下X70钢在海泥模拟溶液中应力腐蚀行为研究[J]. 中国腐蚀与防护学报, 2019, 39(6): 477-483.
[7] 戚鹏, 万逸, 曾艳, 郑来宝, 张盾. 海洋环境中硫酸盐还原菌的快速测定方法研究[J]. 中国腐蚀与防护学报, 2019, 39(5): 387-394.
[8] 吴堂清,周昭芬,王鑫铭,张德闯,尹付成,孙成. 微生物致裂的热力学和动力学分析[J]. 中国腐蚀与防护学报, 2019, 39(3): 227-234.
[9] 李鑫,陈旭,宋武琦,杨佳星,吴明. pH值对X70钢在海泥模拟溶液中微生物腐蚀行为的影响[J]. 中国腐蚀与防护学报, 2018, 38(6): 565-572.
[10] 陈高红,胡远森,于美,刘建华,李国爱. 硫酸阳极化对2E12铝合金力学性能的影响[J]. 中国腐蚀与防护学报, 2018, 38(6): 579-586.
[11] 管方, 翟晓凡, 段继周, 侯保荣. 阴极极化对硫酸盐还原菌腐蚀影响的研究进展[J]. 中国腐蚀与防护学报, 2018, 38(1): 1-10.
[12] 于利宝, 闫茂成, 王彬彬, 舒韵, 许进, 孙成. 酸性土壤环境中Q235钢的微生物腐蚀行为[J]. 中国腐蚀与防护学报, 2018, 38(1): 10-17.
[13] 马双忱, 焦坤灵, 张立男, 孙尧, 吴文龙, 张小霓. 高温气相条件下硫酸氢铵与硫酸铵对20#碳钢的腐蚀行为研究[J]. 中国腐蚀与防护学报, 2017, 37(6): 605-612.
[14] 梅朦, 郑红艾, 陈惠达, 张鸣, 张大全. 硫酸盐还原菌对Cu在循环冷却水中腐蚀行为的影响[J]. 中国腐蚀与防护学报, 2017, 37(6): 533-539.
[15] 滕彧,陈旭,何川,王义闯,王冰. 显微组织对X70钢在含有硫酸盐还原菌的3.5%NaCl溶液中腐蚀行为的影响[J]. 中国腐蚀与防护学报, 2017, 37(2): 168-174.