埋地管线剥离覆盖层下阴极保护的有效性
闫茂成;王俭秋;韩恩厚;柯伟
中国科学院金属研究所
Effectiveness of Cathodic Protection under Simulated Disbonded Coating on Pipelines
;;;
中国科学院金属研究所
引用本文:

闫茂成; 王俭秋; 韩恩厚; 柯伟 . 埋地管线剥离覆盖层下阴极保护的有效性[J]. 中国腐蚀与防护学报, 2007, 27(5): 257-262 .
, , , . Effectiveness of Cathodic Protection under Simulated Disbonded Coating on Pipelines[J]. J Chin Soc Corr Pro, 2007, 27(5): 257-262 .

全文: PDF(389 KB)  
摘要: 由微小缝隙模拟管线剥离覆盖层(涂层)下的局部电化学环境,用微电极技术测量了缝隙内局部电位及pH的分布,研究了缝口阴极保护电位、剥离区几何形状、溶液电导率等因素对剥离区内部局部环境及阴极保护水平的影响。结果表明,剥离区内电位降(电位梯度)主要集中在破损口附近,而剥离区深处接近自然腐蚀状态;剥离区内有效保护距离随缝口保护电位负移而增加,但缝口过保护并不能有效提高剥离区保护效果。阴极保护可使剥离区局部电化学环境pH升高、电导率增大。
关键词 : 阴极保护,  管道,  涂层,  缝隙腐蚀,  微电极,  电位    
Abstract:The local potential and pH along a crevice simulating disbonded coating on pipelines were measured using microelectrodes.The effectiveness of cathodic protection (CP) in the local environment and the effects of applied cathodic potential, geometry of the crevice and solutio conductivity were investigated. The results showed that the IR drop in the disbondment mainly occurred in the vicinity of the opening. The distance effectively protected by CP increased with the decreasing applied potential. However, hydrogen evolution had a reverse effect when an overprotection potential was applied. The additional effct of CP was shown to be the modification of the local environment , such as increase of pH and conductivity of solution, which was beneficial to corrosion controlling as well as direct polarization of the exposed steel at the holiday.
Key words: cathodic protection    pipeline    coating    crevice corrosion    microelectrode    IR drop
收稿日期: 2006-04-12     
ZTFLH:  TG174.41  
[1]Toncre A C.On achieving polarization beneath unbonded pipe coat-ings[J].Mater.Performance,1984,22-27
[2]Song F M,Kirk D W,Graydon J W,et al.Corrosion under dis-bonded coatings having cathodic protection[J].Mater.Performance,2003,42(9):24-26
[3]Beavers J A,Thompson N G.Corrosion beneath disbonded pipelinecoatings[J].Mater.Performance,1997,36(4):13-19
[4]Sabde G,Gan F,Chin D T.Cathodic protection of undergroundpipeline against crevice corrosion:a review[J].J.Chin.Inst.Chem.Eng.,1993,24(6):417-429
[5]Li Z F,Mao X H,Gan F X.Potential distribution inside a ca-thodic protection crevice[J].J.Chin.Soc.Corros.Prot.,2000,20(3):129-134(李正奉,毛旭辉,甘复兴.阴极保护下缝隙内的电位分布[J].中国腐蚀与防护学报,2000,20(3):129-134)
[6]Brousseau R,Qian S.Distribution of steady-state cathodic cur-rents underneath a disbonded coating[J].Corrosion,1994,50(12):907-911
[7]Gan F,Sun Z W,Sabde G,et al.Cathodic protection to mitigateexternal corrosion of underground steel pipe beneath disbondedcoating[J].Corrosion,1994,50(10):804-816
[8]Li S Y,Kim Y G,Kho Y T,et al.Statistical approach to corro-sion under disbonded coating on cathodically protected line pipesteel[J].Corrosion,2004,60(11):1058-1071
[9]Parkins R,Belhimer E,Blanchard W.Stress-corrosion crackingcharacteristics of a range of pipeline steels in carbonate-bicarbon-ate solution[J].Corrosion,1993,49(12):951-966
[10]Charles E A,Parkins R N.Generation of stress-corrosion crack-ing environments at pipeline surfaces[J].Corrosion,1995,51(7):518-527
[11]Wang M,Yao S.Carbonate-melt oxidized iridium wire for pH sens-ing[J].Electroanalysis,2003,15(20):1606-1615
[12]Fessler R R,Markworth A J,Parkins R N.Cathodic protectionlevels under disbonded coatings[J].Corrosion,1983,39(1):20-25
[13]Husock B,Wilson R.Potentials and hydrogen evolution on coatedpipe[J].Mater.Performance,1984,9:26-30
[14]Perdomo J J,Song I.Chemical and electrochemical conditions onsteel under disbonded coatings:the effect of applied potential,so-lution resistivity,crevice thickness and holiday size[J].Corros.Sci.,2000,42(8):1389-1415
[15]Kajiyama F,Okamura K.Evaluating cathodic protection reliabili-ty on steel pipe in microbiologically active soils[J].Corrosion,1999,55(1):74-80
[16]Yan M C,Weng Y J.High pH environment under disbonded coat-ing on cathodic protected pipelines[J].J.Chin.Soc.Corros.Prot.,2004,24(2):95-99(闫茂成,翁永基.阴极保护管线破损涂层下高pH环境形成规律[J].中国腐蚀与防护学报,2004,24(12):95-99)
[1] 李岩, 高科, 张伟, 陈信斌, 隋显杰, 陈洪生, 王晓雅, 冷雪松, 武俊伟. 深海装备涂层功能强化设计及性能调控机制研究进展[J]. 中国腐蚀与防护学报, 2026, 46(5): 1305-1325.
[2] 董少阳, 刘朝坤, 李昱彤, 夏忠虎, 甘浪, 李聪, 任延杰. 高速激光熔覆NiCrAlY涂层在900 ℃空气中的高温氧化行为[J]. 中国腐蚀与防护学报, 2026, 46(5): 1463-1474.
[3] 齐晓涵, 翟海民, 李文生, 洪昊, 曹元, 俞雷, 陈博瀚. Al2O3 磨加量对铝合金搪瓷涂层组织结构及腐蚀性能的影响[J]. 中国腐蚀与防护学报, 2026, 46(5): 1497-1507.
[4] 赵先锐, 戴中国, 李战江, 徐育烺, 张会霞, 李旺. 添加Y、Hf对AlCoCrFeNi高熵合金涂层在NaCl溶液中的腐蚀行为的影响[J]. 中国腐蚀与防护学报, 2026, 46(5): 1549-1559.
[5] 何章平, 袁誉坤, 杜颖哲, 林鹏, 徐健. 在模拟电加热器过热条件下316LN奥氏体钢缝隙腐蚀行为的研究[J]. 中国腐蚀与防护学报, 2026, 46(5): 1579-1587.
[6] 俞春林, 顾铭飞, 孙一昂, 袁可鑫, 杨静, 王丽熙, 朱承飞, 朱海奎. 海洋环境中316不锈钢表面喷涂粉末涂层的耐久性评估[J]. 中国腐蚀与防护学报, 2026, 46(5): 1627-1633.
[7] 雍兴跃, 董晓梅, 高新华, 李卓玄, 陈燕飞, 纪灏天. 电化学阻抗谱在有机涂层研究中的应用[J]. 中国腐蚀与防护学报, 2026, 46(4): 945-961.
[8] 吴昉赟, 乔睿鑫, 李旭宁, 尚浩杰, 陆丰华, 周澄, 王欣, 董亮. 管道内海水流动特性对碳钢阴极保护影响的试验与数值模拟研究[J]. 中国腐蚀与防护学报, 2026, 46(4): 1081-1094.
[9] 柯定芳, 吴芳芳, 朱兆彬, 谢声益, 洪静, 陈悦, 李亮, 李昊, 曹发和. 氧化石墨烯/铈基金属有机框架构筑高稳定长耐蚀防护涂层[J]. 中国腐蚀与防护学报, 2026, 46(4): 1095-1106.
[10] 程孟, 李晓伟, 胡松青. 基于纳米催化剂耗氧机制的主动防腐环氧涂层构筑及性能研究[J]. 中国腐蚀与防护学报, 2026, 46(4): 1117-1128.
[11] 苗乔智, 易芮熙, 张永龙, 蔡云飞, 杨扉雁, 张超宇, 张子晗, 李雯, 孙瑞, 尹月, 王文波. 混维凹凸棒石纳米容器-有机涂层的耐腐蚀性能研究[J]. 中国腐蚀与防护学报, 2026, 46(4): 1169-1176.
[12] 王流火, 孙强, 祁含, 胡苏凯, 叶欢欢, 刘家含, 汪大洋, 张涛. 海上换流站用DH460钢盐雾腐蚀及陶瓷涂层防护[J]. 中国腐蚀与防护学报, 2026, 46(4): 1257-1268.
[13] 周吉, 帅若辉, 杨继凯, 娄丽艳, 刘伊, 鲁俊豪, 蔡志海, 王海斗, 李成新. 21CrMoV钢表面激光熔覆Stellite合金涂层的组织及高温氧化性能[J]. 中国腐蚀与防护学报, 2026, 46(4): 1269-1278.
[14] 成杰, 商永滨, 张沨喜, 卢锋, 刘建国. 原油储罐自修复涂层适应性分析与展望[J]. 中国腐蚀与防护学报, 2026, 46(3): 641-652.
[15] 刘素云, 李婉婷, 周润琪, 刘叡, 董志君, 刘莉, 王福会. 聚多巴胺改性多尺寸氮化硼环氧复合涂层导热防腐性能研究[J]. 中国腐蚀与防护学报, 2026, 46(3): 767-776.