Please wait a minute...
中国腐蚀与防护学报  2007, Vol. 27 Issue (3): 172-175          
  研究报告 本期目录 | 过刊浏览 |
铝合金表面不同硅烷化预处理的耐蚀性研究
郭增昌;王云芳;王汝敏
西北工业大学化工系
Study on anti-resistance of various silanization pretreatment on aluminium alloys surface
;;
西北工业大学化工系
引用本文:

郭增昌; 王云芳; 王汝敏 . 铝合金表面不同硅烷化预处理的耐蚀性研究[J]. 中国腐蚀与防护学报, 2007, 27(3): 172-175 .

全文: PDF(283 KB)  
摘要: 采用浸涂工艺,用pH=4~5,体积分数<3%的3种硅溶胶即γ-缩水甘油醚丙基三甲氧基硅烷(GPTMS)、双-(三乙氧基硅)乙烷(BTSE)、双-[γ-(三乙氧基硅)丙基]四硫化分别采用100℃×60min和130℃×60min工艺固化,并用动电位(PDS)和电化学阻抗谱(EIS)测试了不同硅烷化膜层在3.5mass%NaCl溶液中的耐蚀性并与铬酸盐处理的耐蚀性进行了比较。结果表明,双功能硅烷化膜层的耐蚀性优于功能性硅烷化膜层的耐蚀性,BTSPS硅烷化膜层的耐蚀性最优。
关键词 : 硅烷化,  预处理,  耐蚀性,  双硅烷    
Abstract:In order to see about anti-corrosion of silanization pretreatment on aluminium alloys surface, YL12 Al aloys surface were treated with γ- glycidoxypropyltrimentoxysilane(GPTMS),bis- [triethoxysilylpropyl] tetrasulfide(BTSPS) and bis-1,2-(triethoxysilyl) - ethane (BTSE)by dip-coating process. GPTMS and bis - silane films layer were cured at 100 ℃ for 60min and 130℃ for 60min respectively. Corrosion resistance of various silane silanization films layer were tested with potentiodynamic scan (PDS) and electrochemical impedance spectroscopy (EIS)in 3.5mass% NaCl solution and compared with that of chromated conversion coatings. The results show that the corrosion resistance of bis - silanization film layer exceeded that of organofunctional silane, the antiresistance of BTSPS silanization film layer exceeded that of all others.
Key words: silanization    pretreatment    anti-resistance    bis-silane
收稿日期: 2005-11-25     
ZTFLH:  TG17  
[1]Aramaki K.The inhibition e.ects of chromate-free,anion inhibitorson corrosion of zinc in aerated 0.5 mol/L NaCl[J].Corros.Sci.,2001,43:591~604
[2]Aramaki K.The inhibition effects of cation inhibitors on corrosion ofzinc in aerate 0.5mol/L NaCl[J].Corros.Sci.,2001,43:1573~1588
[3]Underhill P R,Goring G,Du QD.Astudy of the curing of3-glyci-doxypropyltrimethoxy silane films on aluminum[J].InternationalJournal Adhesion&Adhesives,1998,18:313-317
[4]Underhill P R,Goring G,Du Q D.A study of the deposition of 3-glycidoxypropyltrimethoxysilane on aluminum[J].International Jour-nal Adhesion&Adhesives,1998,18:308-311
[5]Underhill P R,Goring G,Du QD.The drying of3-glycidoxypropyl-trimethoxy silane[J].Appl.Surf.Sci.,1998,134:247-253
[6]Sang I S,Kim J H,Choi K H,et al.Preparation of corrosion protec-tive coatings on galvanized iron from aqueous inorganic-organic hy-brid sols by sol-gel method[J].Surf.Coat.Technol.,2006,200(11):3468-3472
[7]Franquet A,Laet J D,Schram T,et al.Determination of the thicknessof thin silane films on aluminium surfaces by means of spectroscopicellipsometry[J].Thin Solid Films,2001,384:37-45
[8]Susac D,Sun X,Mitchell K A R.Adsorption of BTSE andγ-APSorganosilanes on different microstructural regions of2024-T3 alumi-num alloy[J].Appl.Surf.Sci.,2003,207:40-50
[9]Teo M,Kim J,Wong P C,et al.Investigations of interfaces formedbetween bis-1,2-(triethoxysilyl)ethane(BTSE)and aluminumafter different forest product laboratory pre-treatment times[J].Ap-pl.Surf.Sci.,2004,221:340-348
[10]Teo M,Kim J,Wong P C,et al.Pre-treatments applied to oxidizedaluminum surfaces to modify the interfacial bonding with bis-1,2-(triethoxysilyl)ethane(BTSE)Part I.High-purity Al with n-ative oxide[J].Appl.Surf.Sci.,2005,252(15):1293-1304
[11]Kim J,Teo M,Wong P C,et al.Pre-treatments applied to oxidizedaluminum surfaces to modify the interfacial bonding with bis-1,2-(triethoxysilyl)ethane(BTSE)Part II.Anodized 7075-T6 Alalloy[J].Appl.Surf.Sci.,2005,252(15):1305-1312
[12]Van Ooij W J,Zhu D.Electrochemical impedance spectroscopy ofbis-[triethoxysilypropyl]tetrasulfide on Al 2024-T3 substrates[J].Corrosion,2001,57(5):413-427
[13]Zhu D Q,Van Ooij W J.Corrosion protection of AA 2024-T3 bybis-[3-(triethoxysilyl)propyl]tetrasulfide in sodium chloridesolution.Part 1 corrosion of AA2024-T3[J].Corros.Sci.,2003,45:2163-2175
[14]Zhu D Q,Van Ooij W J.Corrosion protection of AA 2024-T3 bybis-[3-(triethoxysilyl)propyl]tetrasulfide in sodium chloridesolution.Part 2:mechanism for corrosion protection[J].Corros.Sci.,2003,345:2177-2197
[15]Cabral A,Duarte R G,Montemor M F,et al.Analytical characteri-sation and corrosion behaviour of bis-[triethoxysilylpropyl]tetra-sulphide pre-treated AA2024-T3[J].Corros.Sci.,2005,47:869-881
[16]Franquet A,Le P C,Terryn H,et al.Effect of bath concentrationand curing time on the structure nonfunctional thin organosilanelayers on aluminium[J].Electrochim.Acta,2003,48:1245~1255
[17]Cao C N,Zhang J Q.An Introduction to EIS for Electrode Proces-ses[M].Beijing:Science Press,2002,7(曹楚南,张鉴清著.电化学阻抗谱导论[M].北京:科学出版社,2002,7)
[1] 郑凯, 王艺陶, 王东胜, 刘伟, 蒋颖畅, 黄嵘, 常雪婷. 腐蚀-应力耦合作用对极地船用螺旋桨低碳马氏体不锈钢失效机理影响研究[J]. 中国腐蚀与防护学报, 2026, 46(5): 1452-1462.
[2] 张春艳, 张瑜心, 陈必秀, 于宝兴, 周鹏. 铸造缺陷对AZ91D镁合金Mn-P系化学转化膜耐蚀性能的影响[J]. 中国腐蚀与防护学报, 2026, 46(5): 1475-1484.
[3] 徐慧强, 赖长清, 王茜茜, 王子明. 基于海水循环模拟系统的牺牲阳极材料对B30传热管腐蚀行为影响研究[J]. 中国腐蚀与防护学报, 2026, 46(4): 1139-1147.
[4] 张晓晨, 杨闯, 姜旭, 陈永生, 赵佳祥, 赵阳, 周鹏, 张涛, 王福会. 镁合金的一种致密微弧氧化涂层工艺及性能的研究[J]. 中国腐蚀与防护学报, 2026, 46(4): 1218-1226.
[5] 刘状, 乔创, 姜金利, 车欣, 代春丽, 沈勇, 郝龙. 电镀锡板表面Cr2O3 钝化膜结构及耐蚀性演化的电化学阻抗谱研究[J]. 中国腐蚀与防护学报, 2026, 46(3): 756-766.
[6] 赖漾, 徐清亮, 罗群, 李谦. 酸洗致基板表面状态变化对镀锡板耐蚀性的影响[J]. 中国腐蚀与防护学报, 2026, 46(2): 393-404.
[7] 张云, 张宇鹏, 董泽华, 张欣欣. 再生镁合金表面微弧氧化/水滑石复合膜层的一步法制备及其耐蚀性能研究[J]. 中国腐蚀与防护学报, 2026, 46(2): 441-449.
[8] 李勇, 王靖超, 胡勇, 高尧, 李贵铭, 陈少武, 柴利强, 缪星旭. 激光熔凝表面改性铁基粉末冶金材料腐蚀防护机理[J]. 中国腐蚀与防护学报, 2026, 46(2): 590-600.
[9] 丁昊, 杜凌霄, 舒琴, 曹甫洋, 谢云, 彭晓. WC含量对激光熔覆AlCoCrFeNi2.1 共晶高熵合金涂层磨损和腐蚀性能的影响[J]. 中国腐蚀与防护学报, 2026, 46(1): 126-136.
[10] 王立芳, 商孟超, 高希钰, 刘贵昌, 孙文. B30铜镍合金原始膜对其腐蚀的影响[J]. 中国腐蚀与防护学报, 2025, 45(6): 1575-1588.
[11] 黄泽邦, 刘光明, 范文学, 徐睿中, 朱炎彬, 刘晨辉. 钝化时间对304不锈钢耐蚀性能的影响[J]. 中国腐蚀与防护学报, 2025, 45(6): 1741-1747.
[12] 何燕, 刘燕, 田华, 陈晔. 低温扩散预处理对含B超级奥氏体不锈钢S31254析出相及耐蚀性的影响[J]. 中国腐蚀与防护学报, 2025, 45(6): 1773-1778.
[13] 郭耀威, 艾士民, 房大然, 林小娉, 杨连威, 郑哲皓. 高压凝固Mg-xAl (x = 3, 5, 7, 9, 12)合金组织结构及耐腐蚀性能[J]. 中国腐蚀与防护学报, 2025, 45(5): 1265-1276.
[14] 冯宇芹, 郭同翰, 余韦汉, 吴伟, 张大全. Sb对高强结构钢在东海环境中腐蚀行为的影响[J]. 中国腐蚀与防护学报, 2025, 45(5): 1300-1308.
[15] 张雄斌, 党恩, 于晓婧, 汤玉斐, 赵康. 油气田用马氏体不锈钢腐蚀性能研究现状与进展[J]. 中国腐蚀与防护学报, 2025, 45(4): 837-848.