Comparison on the Failure Behaviour of the LPG Spherical Tank Manufactured from Different Steels under the Wet H2S Environment |
;; |
南京工业大学205# |
|
|
Abstract Comparative studies on the failure behaviour of the liquefied petroleum gas(LPG) spherical tanks,which were manufactured from 16MnR steel and SPV50Q steel respectively and working under the wet H2S environment,were conducted.By observing the crack feature of the samples cut from the severely corroded shell plates removed from the integral 16MnR spherical tank and the crack morphologies of the metallurgical replica photos made on the internal surface of SPV50Q tank on site,as well as analysing the hardness and welding residual stress measured on site,it was found that the failure of 16MnR tank was attributed to hydrogen-induced cracking(HIC) and the damages occurred on the base metal.While for SPV50Q tank,the failure was attributed to sulfide stress corrosion cracking(SSCC) and cracks mainly appeared in the heat-affected zone(HAZ) around the welded joints.
|
Received: 05 December 2005
|
|
[1]Merick R D.Refinery experience with cracking in wet H2S environ-ment[J].Mater.Perf.,1988,27(1):30-36 [2]Cantwell J E.LPG storage vessel cracking experience[J].Mater.Perf.,1988,27(10):79-82 [3]Trivedi D K,Gupta S C.Cracking in liquid petroleum gas Hortonspheres[J].Mater.Perf.,1997,36(7):59-61 [4]Zhang Y L,Wang J,Shan X P,et al.Critical crack size of CNGcylinder steel in H2S environment[J].J.Chin.Soc.Corros.Prot.,2005,25(5):285-290(张亦良,王晶,陕小平等.CNG气瓶在不同H2S浓度中的临界裂纹尺寸[J].中国腐蚀与防护学报,2005,25(5):285-290) [5]Wang J,Chen J J,Li X B,et al.The concentration distribution ofH2S in the waste water from oil platform and its influences on thecorrosion behavior of the steel structure of platform[J].J.Chin.Soc.Corros.Prot.,2003,23(1):38-45(王佳,陈家坚,李相波等.油田排污水中H2S的分布及其对平台钢结构设施腐蚀行为的影响[J].中国腐蚀与防护学报,2003,23(1):38-45) [6]Zhang Y L,Li L S,Wang M,et al.Criteria to avoid sulfide stresscracking provided by EFC and its verification[J].J.Chin.Soc.Cor-ros.Prot.,2002,22(3):138-143(张亦良,李林生,王慕等.防止硫化氢应力腐蚀失效的EFC准则应用及验证[J].中国腐蚀与防护学报,2002,22(3):138-143) [7]Ikeda A,Kaneko T,Ando Y.On the evaluation methods of sulfidestress cracking susceptibility of carbon and low alloy steels[J].Cor-ros.Sci.,1987,27:1099-1115 [8]Garber R.Higher hardenability low alloy steels for H2S resistant oilcountry tubular[J].Corrosion,1983,39(3):83-91 [9]NACE Standard RP0472.Methods and controls to prevent in-ser-vice environmental cracking of carbon steel weldments in corrosivepetroleum refining environments[S].1987 [10]Adam Mazur.Segregation bands’role in H2S cracking of steels[J].Mater.Perf.,1995,34(7):52-54 [11]Maria Sozańka,Jaroslav Sojka,Petra Bet′ákov,áet al.Examinationof hydrogen interaction in carbon steel by means of quantitativemicrostructure and fracture descriptions[J].Mate.Charact.,2001,46:239-241 [12]Snape E.Sulfide stress corrosion cracking of some medium and lowalloy steel[J].Corrosion,1967,23(6):154-172 [13]Albarran J L,Martinez L,Lopez H F.Effect of heat treatment onthe stress corrosion resistance of microalloyed pipeline steel[J].Corros.Sci.,1999,41:1037-1049 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|