模拟高温海洋环境中铝化物/搪瓷复合涂层腐蚀行为研究 |
程玉贤1(), 曹超2, 蒋成洋2, 陈明辉2, 王福会2 |
1.中国航发沈阳黎明航空发动机有限责任公司 沈阳 110043 2.沈阳材料科学国家研究中心东北大学联合研究分部 沈阳 110819 |
|
Corrosion Behavior of Enamel/aluminide Composite Coating in a Simulated High Temperature Marine Environment |
CHENG Yuxian1(), CAO Chao2, JIANG Chengyang2, CHEN Minghui2, WANG Fuhui2 |
1.AECC Shenyang Liming Aero-Engine Co. Ltd. , Shenyang 110043, China 2.Shenyang National Laboratory for Materials Science, Northeastern University, Shenyang 110819, China |
引用本文:
程玉贤, 曹超, 蒋成洋, 陈明辉, 王福会. 模拟高温海洋环境中铝化物/搪瓷复合涂层腐蚀行为研究[J]. 中国腐蚀与防护学报, 2022, 42(3): 410-416.
Yuxian CHENG,
Chao CAO,
Chengyang JIANG,
Minghui CHEN,
Fuhui WANG.
Corrosion Behavior of Enamel/aluminide Composite Coating in a Simulated High Temperature Marine Environment. Journal of Chinese Society for Corrosion and protection, 2022, 42(3): 410-416.
链接本文:
https://www.jcscp.org/CN/10.11902/1005.4537.2021.223
或
https://www.jcscp.org/CN/Y2022/V42/I3/410
|
1 |
Bu W X. The study on quantitative phase analysis method and application of GH169 alloy [D]. Harbin: Harbin University of Science and Technology
|
1 |
卜文学. GH169合金定量相分析方法及其应用的研究 [D]. 哈尔滨: 哈尔滨理工大学)
|
2 |
Greene G A, Finfrock C C. Oxidation of Inconel 718 in air at high temperatures [J]. Oxid. Met., 2001, 55: 505
|
3 |
Cui T, Wang J Q, Wang X X, et al. High temperature oxidation of superalloy GH4169 [J]. Corros. Sci. Prot. Technol., 2004, 16: 192
|
3 |
崔彤, 王介强, 王晓轩等. GH4169合金高温氧化特征 [J]. 腐蚀科学与防护技术, 2004, 16: 192
|
4 |
Saladi S, Menghani J, Prakash S. A study on the cyclic oxidation behavior of detonation-gun-sprayed Ni-5Al coatings on Inconel-718 at 900 ℃ [J]. J. Mater. Eng. Perform., 2014, 23: 4394
|
5 |
Saladi S, Menghani J, Prakash S. Hot corrosion behaviour of detonation-gun sprayed Cr3C2-NiCr coating on Inconel-718 in molten salt environment at 900 ℃ [J]. Trans. Indian Ins. Met., 2014, 67: 623
|
6 |
Koech P K, Wang C J. High-Temperature corrosion behaviour of aluminized-coated and uncoated alloy 718 under cyclic oxidation and corrosion in NaCl vapour at 750 ℃ [J]. Oxid. Met., 2018, 90: 713
|
7 |
Kumar S, Satapathy B, Pradhan D, et al. Effect of surface modification on the hot corrosion resistance of Inconel 718 at 700 ℃ [J]. Mater. Res. Express, 2019, 6: 086549
|
8 |
Yang S S, Yang L L, Chen M H, et al. Understanding of failure mechanisms of the oxide scales formed on nanocrystalline coatings with different Al content during cyclic oxidation [J]. Acta Mater., 2021, 205: 116576
|
9 |
Jiang C Y, Qian L Y, Feng M, et al. Benefits of Zr addition to oxidation resistance of a single-phase (Ni,Pt) Al coating at 1373 K [J]. J. Mater. Sci. Technol., 2019, 35: 1334
|
10 |
Jiang C Y, Yang Y F, Zhang Z Y, et al. A Zr-doped single-phase Pt-modified aluminide coating and the enhanced hot corrosion resistance [J]. Corros. Sci., 2018, 133: 406
|
11 |
Liao Y M, Zhang B, Chen M H, et al. Self-healing metal-enamel composite coating and its protection for TiAl alloy against oxidation under thermal shock in NaCl solution [J]. Corros. Sci., 2020, 167: 108526
|
12 |
Feng M, Chen M H, Yu Z D, et al. Comparative study of thermal shock behavior of the arc ion plating NiCrAlY and the enamel based composite coatings [J]. Acta Metall. Sin., 2017, 53: 1636 丰敏, 陈明辉, 余中狄等,多弧离子镀NiCrAlY涂层与搪瓷基复合涂层的抗热震行为对比研究 [J]. 金属学报. 2017, 53: 1636
|
13 |
Chen K, Chen M H, Yu Z D, et al. Simulating sulfuric acid dew point corrosion of enamels with different contents of silica [J]. Corros. Sci., 2017, 127: 201
|
14 |
Yang Y F, Jiang C Y, Bao Z B, et al. Effect of aluminisation characteristics on the microstructure of single phase β-(Ni,Pt) Al coating and the isothermal oxidation behaviour [J]. Corros. Sci., 2016, 106: 43
|
15 |
Yang Y F, Jiang C Y, Yao H R, et al. Preparation and enhanced oxidation performance of a Hf-doped single-phase Pt-modified aluminide coating [J]. Corros. Sci., 2016, 113: 17
|
16 |
Jiang C Y, Yang Y F, Zhang Z Y, et al. Preparation and enhanced hot corrosion resistance of a Zr-doped PtAl2+(Ni, Pt) Al dual-phase coating [J]. Acta Metall. Sin., 2018, 54: 581
|
16 |
蒋成洋, 阳颖飞, 张正义等. 一种Zr改性双相PtAl2+(Ni, Pt)Al涂层的制备及热腐蚀行为研究 [J]. 金属学报, 2018, 54: 581
|
17 |
Li M S. High Temperature Corrosion of Metal [M]. Beijing: Beijing Industry Press, 2001
|
17 |
李美栓. 金属的高温腐蚀 [M]. 北京: 北京工业出版社, 2001
|
18 |
Yang L L, Chen M H, Wang J L, et al. A duplex nanocrystalline coating for high-temperature applications on single-crystal superalloy [J]. Corros. Sci., 2016, 102: 72
|
19 |
Wang J L, Chen M H, Cheng Y X, et al. Hot corrosion of arc ion plating NiCrAlY and sputtered nanocrystalline coatings on a nickel-based single-crystal superalloy [J]. Corros. Sci., 2017, 123: 27
|
20 |
Chen M H, Zhu S L, Shen M L, et al. Effect of NiCrAlY platelets inclusion on the mechanical and thermal shock properties of glass matrix composites [J]. Mater. Sci. Eng., 2011, 528A: 1360
|
21 |
Chen M H, Zhu S L, Wang F H. Strengthening mechanisms and fracture surface characteristics of silicate glass matrix composites with inclusion of alumina particles of different particle sizes [J]. Physica, 2013, 413B: 15
|
22 |
Chen K, Chen M H, Yi A H, et al. Thermal shock and sulfuric acid corrosion behavior of enamel-nano-Ni composite/enamel-nano-nickel composite coating [J]. Int. J. Appl. Glass Sci., 2020, 11: 784
|
23 |
Yu Z D, Chen M H, Chen K, et al. Corrosion of enamel with and without CaF2 in molten aluminum at 750 ℃ [J]. Corros. Sci., 2019, 148: 228
|
24 |
Padture N P, Gell M, Jordan E H. Thermal barrier coatings for gas-turbine engine applications [J]. Science, 2002, 296: 280
|
25 |
Chen M H, Zhu S L, Wang F H. Crystallization behavior of SiO2-Al2O3-ZnO-CaO glass system at 1123-1273 K [J]. J. Am. Ceram. Soc., 2010, 93: 3230
|
26 |
Shu Y H, Wang F H, Wu W T. Corrosion behavior of Ti60 alloy coated with a solid NaCl deposit in O2 plus water vapor at 500~700 ℃ [J]. Oxid. Met., 1999, 52: 463
|
27 |
Wang F H, Geng S J, Zhu S L. Corrosion behavior of a sputtered K38G nanocrystalline coating with a solid NaCl deposit in wet oxygen at 600 to 700 ℃ [J]. Oxid. Met., 2002, 58: 185
|
28 |
Cao M, Liu L, Yu Z F, et al. Studies on the corrosion behavior of Fe-20Cr alloy in NaCl solution spray at 600 ℃ [J]. Corros. Sci., 2018, 133: 165
|
29 |
Xiong Y X, Zhu S L, Wang F H. Synergistic corrosion behavior of coated Ti60 alloys with NaCl deposit in moist air at elevated temperature [J]. Corros. Sci., 2008, 50(1): 15
|
30 |
Barin I. Thermochemical Data of Pure Substance [M]. 3rd ed. Weinheim, Germany: Wiley-VCH, 1995
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|