全文: PDF(158 KB)  
摘要: 利用原子力显微镜、电子探针和电化学测试等技术,研究了Ca2+离子对碳钢表面生物膜的形成、微生物腐蚀程度以及杀菌剂杀菌效果的影响。结果表明:Ca2+离子促进了硫酸盐还原菌(SRB)的生长,增加了生物膜的致密性,降低了碳钢微生物腐蚀的敏感性。但同时也增加了SRB对杀菌剂的敏感性,给防治SRB带来更大困难。
关键词 Ca2+离子硫酸盐还原菌微生物腐蚀杀菌剂    
Abstract:In this paper, the effect of Ca2+ in the form of bilfilm on the surface of carbon steel, the corrosion extent of MIC and the efficacy of bactericide were investigated via AFM, EPMA and EIS. The result shows that Ca2+ can promote the growth of SRB, increase the compact of bilfil and decrease the sensitiveness of carbon metal to MIC. But at the same time Ca2+ also decreases the sensitiveness of SRB to biocide which brings many difficulties to the prevention and cure of SRB.
Key wordscalcium ion    SRB    MIC    biocide
收稿日期: 2003-01-13     
ZTFLH:  TG172.7  
通讯作者: 许立铭   
Corresponding author: Liming Xv   

引用本文:

刘宏芳; 汪梅芳; 许立铭; 郭兴蓬 . Ca2+离子对碳钢微生物腐蚀的影响[J]. 中国腐蚀与防护学报, 2004, 24(1): 45-51 .
Hongfang Liu, Meifang Wang, Liming Xv, Xingpeng Guo. The Role of Ca2+ on the Microbiologically Induced Corrosion of Carbon Steel. J Chin Soc Corr Pro, 2004, 24(1): 45-51 .

链接本文:

https://www.jcscp.org/CN/      或      https://www.jcscp.org/CN/Y2004/V24/I1/45

[1]FlemmingHC .MicrobiallyInfluencedCorrosionofMaterials[M ].1sted.,HeitzE ,FlemmingHC ,SandW ,editors.Berlin:Heidelberg,Sp inger,1996,5
[2]BeerD ,StoodleyP ,RoeF ,LewandowskiZ .Effectsofbiofilmstructuresonoxygendistributionandmasstransport[J].BiotechnolBioeng,1994,43:1131
[3]LiuHongfang,HuangZhuo,XuLiming,ZhengJiashen.Identificationofvarioussulfatereducingbacteriaspeciesbygaschromatography-massspectrometry[J].Chin.J.AnalyticalChemistry,,2000,2:194-196(刘宏芳,黄茁,许立铭,郑家焱木.气相色谱/质谱在不同种类硫酸盐还原菌的鉴定中应用探讨[J].分析化学,2000,2:194-196)
[4]LiuHongfang,QinQihua,XuLiming,ZhengJiashen.EffectsoffiveSRBstrainsoncorrosionofcarbonsteel[J].Chemic.Eng.OilandGas,2000,29(1):30-32(刘宏芳,覃启华,许立铭,郑家焱木.不同种群硫酸盐还原菌腐蚀行为研究[J].石油与天然气化工,2000,29(1):30-32)
[5]LiuHongfang,XuLiming,ZhengJiashen,LiuJing.Newbactericideforbiocide-resistantsulfate-reducingbacteria[J].MaterialPerformance,2000,39(4):52-55
[6]LiuHongfang,XuLiming,ZhengJiashen.InfluenceofSRBbiofilmoncorrosionofcarbonsteel[J].J.Chin.Soc.Corros.Prot.,2000,20(1):41-46(刘宏芳,许立铭,郑家焱木.SRB生物膜与碳钢腐蚀的关系[J].中国腐蚀与防护学报,2000,20(1):41-46)
[7]XuLichong,HerbertHPFang,ChanKwongyu.Atomicforcemicroscopyofmicrobiologicallyinfluencedcorrosionofmildsteel[J].J.Electroche mi.Soc.,1999,146(12):4455-4460
[8]LiuHongfang,LiuLiewei,XuLiming,ZhengJiashen.Effectsofbiofilmoncorrosionofcarbonsteel[J].J.Chin.Soc.Corros.Prot.,1999,19(5):291-295(刘宏芳,刘烈炜,许立铭,郑家焱木.生物膜对碳钢腐蚀的影响[J].中国腐蚀与防护学报,1999,19(5):291-295)
[1] 董续成, 管方, 徐利婷, 段继周, 侯保荣. 海洋环境硫酸盐还原菌对金属材料腐蚀机理的研究进展[J]. 中国腐蚀与防护学报, 2021, 41(1): 1-12.
[2] 张雨轩, 陈翠颖, 刘宏伟, 李伟华. 铝合金霉菌腐蚀研究进展[J]. 中国腐蚀与防护学报, 2021, 41(1): 13-21.
[3] 王欣彤, 陈旭, 韩镇泽, 李承媛, 王岐山. 硫酸盐还原菌作用下2205双相不锈钢在3.5%NaCl溶液中应力腐蚀开裂行为研究[J]. 中国腐蚀与防护学报, 2021, 41(1): 43-50.
[4] 王玉, 吴佳佳, 张盾. 海水环境中异化铁还原菌所致金属材料腐蚀的研究进展[J]. 中国腐蚀与防护学报, 2020, 40(5): 389-397.
[5] 陈旭, 李帅兵, 郑忠硕, 肖继博, 明男希, 何川. X70管线钢在大庆土壤环境中微生物腐蚀行为研究[J]. 中国腐蚀与防护学报, 2020, 40(2): 175-181.
[6] 胥聪敏,罗立辉,王文渊,赵苗苗,田永强,宋鹏迪. D-tyrosine对碳钢表面铁细菌生物膜的杀菌增强作用机理研究[J]. 中国腐蚀与防护学报, 2020, 40(1): 63-69.
[7] 陈旭,马炯,李鑫,吴明,宋博. 温度与SRB协同作用下X70钢在海泥模拟溶液中应力腐蚀行为研究[J]. 中国腐蚀与防护学报, 2019, 39(6): 477-483.
[8] 卫晓阳,杨丽景,吕战鹏,郑必长,宋振纶. 磁场对纯Cu微生物腐蚀行为的影响[J]. 中国腐蚀与防护学报, 2019, 39(6): 484-494.
[9] 戚鹏, 万逸, 曾艳, 郑来宝, 张盾. 海洋环境中硫酸盐还原菌的快速测定方法研究[J]. 中国腐蚀与防护学报, 2019, 39(5): 387-394.
[10] 吴堂清,周昭芬,王鑫铭,张德闯,尹付成,孙成. 微生物致裂的热力学和动力学分析[J]. 中国腐蚀与防护学报, 2019, 39(3): 227-234.
[11] 史显波,杨春光,严伟,徐大可,闫茂成,单以银,杨柯. 管线钢的微生物腐蚀[J]. 中国腐蚀与防护学报, 2019, 39(1): 9-17.
[12] 李鑫,陈旭,宋武琦,杨佳星,吴明. pH值对X70钢在海泥模拟溶液中微生物腐蚀行为的影响[J]. 中国腐蚀与防护学报, 2018, 38(6): 565-572.
[13] 管方, 翟晓凡, 段继周, 侯保荣. 阴极极化对硫酸盐还原菌腐蚀影响的研究进展[J]. 中国腐蚀与防护学报, 2018, 38(1): 1-10.
[14] 于利宝, 闫茂成, 王彬彬, 舒韵, 许进, 孙成. 酸性土壤环境中Q235钢的微生物腐蚀行为[J]. 中国腐蚀与防护学报, 2018, 38(1): 10-17.
[15] 梅朦, 郑红艾, 陈惠达, 张鸣, 张大全. 硫酸盐还原菌对Cu在循环冷却水中腐蚀行为的影响[J]. 中国腐蚀与防护学报, 2017, 37(6): 533-539.