The Electrochemical Characteristics of Pitting of X70 Pipeline Steel
Jian Peng Mao;Yuming Tang;Yu Zuo
北京化工大学材料科学与工程学院
Cite this article: 

Jian Peng Mao; Yuming Tang; Yu Zuo. The Electrochemical Characteristics of Pitting of X70 Pipeline Steel. J Chin Soc Corr Pro, 2006, 26(2): 80-84 .

Download:  PDF(167KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The Electrochemical Characteristics of pitting of X70 Pipeline Steel in Phosphate Buffer Solution are studied in this paper. It is found that the effect of Cl- ions on pitting protection potential is neglectable. PO43- ions show strong inhibition on nucleation and the growth of pitting. Impurity and the surface grooves left by polishing result in the nucleation and the growth of metastable pitting. The nucleation frequency increases at first and then decreases with potential, while peak current increases continually. In the potential range of metastable pitting, the impedance of passive film keeps almost unchanged with potential. However, the impedance shows an obvious decrease when potential is above pitting potential Eb.
Key words:  pitting      metastable pitting      current fluctuations      X70 steel      EIS      
Received:  13 January 2005     
ZTFLH:  TG174  

URL: 

https://www.jcscp.org/EN/     OR     https://www.jcscp.org/EN/Y2006/V26/I2/80

[1]Frankel G S,Stockert L,Hunkeler F,et al.Metastable pitting ofstainless steel[J].Corrosion,1987,43(7):429-436
[2]Pistorius P C,Burstein G T.Growth of corrosion pits on stainlesssteel in chloride solution containing dilute sulphate[J].Corros.Sci.,1992,33(12):1885-1897
[3]Pistorious P C,Burstein G T.Aspects of the effects of electrolytecomposition on the occurrence of metastable pitting on stainlesssteel[J].Corros.Sci.,1994,36(3):255-261
[4]Cheng Y F,Luo J L.Metastable pitting of carbon steel under potentio-static control[J].J.Electrochem.Soc.,1999,146(3):970-978
[5]Cheng Y F,Wilmott M,Luo J L.Analysis of the role of electrodecapacitance on the initiation of pits for A516 carbon steel by elec-trochemical noise measurements[J].Corros.Sci.,1999,41:1245-1256
[6]Dong Z H,Guo X P,Zheng J S.Electrochemical noise characteris-tics of metastable pitting of 16Mn mild steel[J].Corros.Sci.Prot.Technol.,2001,13(4):195-201(董泽华,郭兴蓬,郑家焱木.用电化学噪声研究16Mn钢的亚稳态孔蚀特征[J].腐蚀科学与防护技术,2001,13(4):195-201)
[7]Tang Y M,Zuo Y.The metastable pitting of mild steel in bicar-bonate solutions[J].Materials Chemistry and Physics,2004,88(3):221-226
[8]Fujioka E,Nishihara H,Aramaki K.The inhibition of pit nucle-ation and growth on the passive surface of iron in a borate buffersolution coataining Cl-by oxidizing inhibitors[J].Corros.Sci.,1996,38(11):1915-1933
[9]Pistorius P C,Burstein G T.Surface roughness and the metastablepitting of stainless steel in chloride solutions[J].Corrosion,1995,51(5):380-385
[10]Wang H,Zuo Y,Mao J P.Metastable pitting and related morphol-ogy of pure iron in NaNO2+NaCl solution[J].J.Beijing Universi-ty of Chemical Technology,2004,31(5):41-43(王虎,左禹,毛健鹏.工业纯铁在NaNO2+NaCl溶液中的亚稳态孔蚀及其腐蚀形貌[J].北京化工大学学报,2004,31(5):41-43)
[11]Wei B M,Hao L.Physical characteristic of some non-semi-cricle AC depeadances[J].Total Corrosion Control,1990,4(3):9-15(魏宝明,郝凌.几种非正半圆交流阻抗图谱的物理意义[J].全面腐蚀控制,1990,4(3):9-15)
[1] YU Chunlin, GU Mingfei, SUN Yi'ang, YUAN Kexin, YANG Jing, WANG Lixi, ZHU Chengfei, ZHU Haikui. Durability Assessment of Powder Spraying Coating on Surface of 316 Stainless Steel in Artificial Marine Environments[J]. 中国腐蚀与防护学报, 2026, 46(5): 1627-1633.
[2] YONG Xingyue, DONG Xiaomei, GAO Xinhua, LI Zuoxian, CHEN Yanfei, JI Haotian. Application of Electrochemical Impedance Spectroscopy in Research of Organic Coatings[J]. 中国腐蚀与防护学报, 2026, 46(4): 945-961.
[3] MA Huanhuan, LV Shengdong, QIAN Yixin, LIN Yong, HAO Xiangping, ZHANG Dawei, WANG Luning. Localized Corrosion and Service Life Prediction of Copper Heat Exchange Tubes in a Sodium Acetate Trihydrate Phase Change Thermal Energy Storage System[J]. 中国腐蚀与防护学报, 2026, 46(4): 1045-1057.
[4] LU Haifeng, MIAO Qiang, LIANG Wenping, YAO Zhimeng, WEI Shaochong, CHEN Guoxing. Effect of Laser Surface Cleaning on Corrosion Resistance of Stainless Steel[J]. 中国腐蚀与防护学报, 2026, 46(4): 1227-1237.
[5] LIU Zhuang, QIAO Chuang, JIANG Jinli, CHE Xin, DAI Chunli, SHEN Yong, HAO Long. Structure- and Corrosion Resistance-evolution of Cr2O3 Passivation Film on Tinplate Surface in Neutral NaCl- and Acidic NaCl + Na2SO3-solution[J]. 中国腐蚀与防护学报, 2026, 46(3): 756-766.
[6] GU Qingyu, SONG Yanfei, ZHANG Liangliang, WANG Nan, LEI Xiaowei. Passivation and Pitting Corrosion Behavior of Laser Directed Energy Deposited 17-4PH Stainless Steel[J]. 中国腐蚀与防护学报, 2026, 46(1): 103-114.
[7] XU Shiyuan, MENG Xin, YANG Yazhang, LIU Chen, ZHANG Zhao, FANG Xiaozu. Effect of Corrosion Morphology on Electrochemical Impedance Spectroscopy Characteristics of Mg-alloy[J]. 中国腐蚀与防护学报, 2025, 45(6): 1589-1598.
[8] GUO Yujie, LI Yanhui, XIA Da-Hai, HU Wenbin. Data Analysis and Physical Model of Electrochemical Impedance Spectroscopy for Corrosion Systems: Progresses and Challenges[J]. 中国腐蚀与防护学报, 2025, 45(5): 1143-1160.
[9] HE Wuhao, LIU Yang, YANG Siyi, ZHANG Shaodong, WU Wei, ZHANG Junxi. Effect of Sensitization Treatment on Electrochemical Behavior and Intergranular Corrosion of Conventional and Additively Manufactured 316L Stainless Steels[J]. 中国腐蚀与防护学报, 2025, 45(5): 1331-1340.
[10] HONG Xiaomu, WANG Yongqiang, LI Na, TIAN Kai, DU Juan. Effect of Aging on Microstructures and Localized Corrosion of Custom455 Martensitic Age-hardening Stainless Steel[J]. 中国腐蚀与防护学报, 2024, 44(5): 1285-1294.
[11] YANG Cheng, YANG Guangming, WANG Jianjun, MIAO Xueliang, ZHANG Yi, SUN Baozhuang, LIU Zhiyong. Effect of Temperature on Corrosion Behavior of 42CrMoE Low-alloy Steel in Boric Acid Solution[J]. 中国腐蚀与防护学报, 2024, 44(5): 1345-1352.
[12] XU Guizhi, DU Xiaoze, HU Xiao, SONG Jie. Effect of Pt Coating on Electrochemical Behavior and Interfacial Conductivity of TA4 Bipolar Plate in Anode Side Environment of Proton Exchange Membrane Water Electrolyzer for Hydrogen Production[J]. 中国腐蚀与防护学报, 2024, 44(5): 1370-1376.
[13] FU Jiangyue, GUO Jianxi, YANG Yange, LENG Zhe, WANG Wen. Erosion-corrosion Behavior of a High Strength Low Alloy Steel in Flowing 3.5%NaCl Solution[J]. 中国腐蚀与防护学报, 2024, 44(3): 585-600.
[14] MA Heng, TIAN Huiyun, LIU Yuxi, WANG Yuexiang, HE Kang, CUI Zhongyu, CUI Hongzhi. Corrosion Behavior of S420 Steel in Different Marine Zones[J]. 中国腐蚀与防护学报, 2024, 44(3): 635-644.
[15] XING Shaohua, PENG Wenshan, QIAN Yao, LI Xiangbo, MA Li, ZHANG Dalei. Effect of Seawater Flow Velocity on Pitting Corrosion of 2205 Stainless Steel with Different Surface Treatments[J]. 中国腐蚀与防护学报, 2024, 44(3): 658-668.
No Suggested Reading articles found!