Abstract Abstract: In this paper, the corrosion behaviors of three kinds of titanium alloys (TC4、TC18、TC21) in 3.5%NaCl solution were studied by means of Cyclic voltammetry, wedge loaded WOL pre-crack sample method combined with scanning electron microscope. The results showed that the broken potential of the three titanium alloys were 1.625V, 1.671V and 1.842V for TC4,TC18 and TC21, respectively, which representing the excellent pitting corrosion resistance, and pitting corrosion susceptibility in the following sequence: TC4>TC18>TC21. Furthermore, TC21 had the highest broken potential and the best self-healing ability of passive film when pitting happened among the three titanium alloys, while the self-healing ability of TC4 is a little better than that of TC18. KISCC for TC4, TC18 and TC21 were 62.92MPa.m0.5、66.82MPa.m0.5 and 71.99MPa.m0.5 respectively and the SCC susceptibility of the three kinds of titanium alloys in the following sequence: TC4>TC18>TC21. They have better stress corrosion resistance and the TC21 was the best in stress corrosion resistance. TC18 was better than that of TC4. The fracture surface of SCC zone was inspected using SEM and the fracture surface of test specimens showed the characteristics of dimple.
|
|
Received: 30 October 2013
|
|
|
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|