HIGH TEMPERATURE CORROSION OF NF616 AND 12CrMoV IN SIMULATED WASTE-GASIFICATION ENVIROMENTS
PAN Taijun1, CHEN Degui1, ZHANG Ke2, HU Jing1
1. Key Laboratory of Advanced Metallic Materials of Changzhou, School of Material Science and Engineering, Changzhou University, Changzhou 213164
2. Department of Chemistry, Shenyang Normal University, Shenyang, 110034
Download:  PDF(932KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The corrosion behavior of two commercial steels NF616 and 12CrMoV was comparatively investigated at 600℃ in H2-CO2, H2-HCl-CO2 and H2-HCl-H2S-CO2 reducing atmospheres. In comparison with corrosion behavior of the same-type steels in H2-CO2 and H2-HCl-CO2 reducing atmosphere, NF616 and 12CrMoV suffered from accelerated corrosion in the H2-HCl-H2S-CO2 atmosphere, particularly the degradation of chromia formed on 12CrMoV. The kind of accelerated corrosion was mainly attributed to formation of metal chlorides and sulfides during corrosion procedure. The mechanism on accelerated corrosion is illuminated on the basis of thermodynamic diagrams.
Key words:  sulfur      chlorine      high temperature corrosion      internal oxidation     
Received:  30 August 2010     
ZTFLH: 

TG172

 

Cite this article: 

PAN Taijun, CHEN Degui, ZHANG Ke, HU Jing. HIGH TEMPERATURE CORROSION OF NF616 AND 12CrMoV IN SIMULATED WASTE-GASIFICATION ENVIROMENTS. J Chin Soc Corr Pro, 2011, 31(6): 457-461.

URL: 

https://www.jcscp.org/EN/     OR     https://www.jcscp.org/EN/Y2011/V31/I6/457

[1] Spiegel M, Grabke H J.High temperature corrosion of high alloy steels in simulated waste incineration environments[J]. Mater. Corros., 1996,47:179-189

[2] Miller P D, Krouse H H. The mechanism in high temperature corrosion in municipal incinerators[J]. Corrosion, 1972, 28: 274-281

[3] Pan T J, Lin Y F, Hu J. Accelerated corrosion behavior of Fe-Al alloys under KCl-ZnCl2 deposits[J].J. Chin. Soc. Corros.Prot., 2010, 30: 58-61

    (潘太军, 林一凡, 胡静. Fe-Al合金在KCl-ZnCl2沉积盐作用下的加速腐蚀行为,中国腐蚀与防护学报, 2010, 30: 58-61)

[4] Li Y S,  Niu Y, Wu W T. Corrosion behavior of pure Cr and two Cr-containing alloys beneath ZnCl2 and KCl-ZnCl2 deposits [J]. J. Chin. Soc. Corros. Prot., 2002, 22: 27-31

    (李远士, 牛焱,吴维tao.纯Cr和两种含Cr合金在ZnCl2及KCl-ZnCl2盐膜下的腐蚀,中国腐蚀与防护学报, 2002, 22: 27-31)

[5] Zahs A, Spiegel M, Grabke H J. Chlorination and oxidation of iron, chromium, nickel, and their alloys in chloridizing and oxidizing atmospheres at 400-700℃[J]. Corros. Sci., 2000, 42:1093-1122

[6] Schulte M, Rahmel A, Schutze M. The sulfidation behavior of several commercial ferritic and austenitic steels[J]. Oxid. Met.,1998, 49: 33-70

[7] Pan T J, Al-Omary M, Zeng C L, et al. The corrosion of three commercial steels in reducing atmospheres containing HCl and H2S at 873 K[J]. High Temp. Mater. Proc., 2005, 24: 193-203

[8] Pan T J, Gesmundo F, Niu Y. Corrosion behavior of three iron based model alloys in reducing atmospheres containing HCl and H2S at 600℃[J]. Corros. Sci., 2007, 49: 1362-1377

[9] Li Y S, Niu Y, Liu G. High temperature corrosion of metallic materials in waste incineration  environment[J]. Corros. Sci. Prot. Technol., 2000, 12: 224-227

    (李远士, 牛焱, 刘刚等.金属材料在垃圾焚烧环境中的高温腐蚀, 腐蚀科学与防护技术, 2000, 12:224-227)

[10] Hou P Y, Pruner K, Fairbrother D H, et al. Sulfur segregation to deposited Al2O3 film/alloy interface at 1000SDC[J]. Scr. Mater., 1999, 40: 241-247

[11] Hou P Y, Zhang X F, Cannon R M. Impurity distribution in Al2O3 formed on an FeCrAl alloy[J]. Scr. Mater., 2004, 50:45-49
[1] JIANG Xuguang, LIU Xiaobo. Research Progress and Direction Thinking on Corrosion of Key Heat Transfer Components in Waste Incineration Boilers[J]. 中国腐蚀与防护学报, 2020, 40(3): 205-214.
[2] LI Xianghong, DENG Shuduan, XU Xin. Inhibition Action of Cassava Starch Ternary Graft Copolymer on Steel in H2SO4 Solution[J]. 中国腐蚀与防护学报, 2020, 40(2): 105-114.
[3] Zhifeng LIU,Zhiping ZHU,Chun SHI,Zhaoxin HUANG. Preparation of Sulfuric Acid Vapor for Simulation of Sulfuric Acid Dew Point Corrosion by Inert Gas Carrying Method[J]. 中国腐蚀与防护学报, 2020, 40(1): 1-9.
[4] XU Xunhu,HE Cuiqun,XIANG Junhuai,WANG Ling,ZHANG Honghua,ZHENG Xiaodong. High Temperature Oxidation Behavior of Co-20Re-25Cr-1Si Alloy in 0.1 MPa Pure Oxygen[J]. 中国腐蚀与防护学报, 2020, 40(1): 75-80.
[5] YU Renqiang,HE Jianjun,LI Wei,REN Yanjie,YANG Wang. Erosive Wear of Cr30A High Chromium Cast Iron in a Simulated Circulating Pump Operation Condition with Slurry Related to Wet DesulfurationProcess in Thermal Power Plant[J]. 中国腐蚀与防护学报, 2019, 39(4): 353-358.
[6] Changgang WANG,Jie WEI,Xin WEI,Xin MU,Fang XUE,Junhua DONG,Wei KE,Guoping LI. Crevice Corrosion Behavior of Several Super Stainless Steels in a Simulated Corrosive Environment of Flue Gas Desulfurization Process[J]. 中国腐蚀与防护学报, 2019, 39(1): 43-50.
[7] Gaohong CHEN,Yuansen HU,Mei YU,Jianhua LIU,Guoai LI. Effect of Sulfuric Acid Anodizing on Mechanical Properties of 2E12 Al-alloy[J]. 中国腐蚀与防护学报, 2018, 38(6): 579-586.
[8] Taotao XU, Zhuqiao CHEN, Weiping TIAN, Cheng WANG, Shenglong ZHU, Fuhui WANG, Tao ZHANG, Minghui CHEN. Protective Performance of a Novel Silicone Coating ES150 Modified with Nano-particulate of Metal for AZ91D Mg-alloy[J]. 中国腐蚀与防护学报, 2018, 38(4): 373-380.
[9] Mingming ZHANG,Li XIN,Xueyong DING,Shujiang GENG,Shenglong ZHU,Fuhui WANG. Corrosion Resistance of Alternately Multilayered Coating Ti/TiAlN on Ti-alloy Ti-6Al-4V Beneath a Solid NaCl Film in Atmosphere of Water Vapor and Oxygen at 600 ℃[J]. 中国腐蚀与防护学报, 2017, 37(1): 29-35.
[10] Yan LI,Jintao LU,Zhen YANG,Ming ZHU,Yuefeng GU. Effect of Sulfur Content on Corrosion Behavior of Candidate Alloys Used for 700 ℃ Level A-USC Boiler in Simulated Coal Ash and Flue Gas Environments[J]. 中国腐蚀与防护学报, 2016, 36(5): 505-512.
[11] Qiuyan SHEN,Hongfang LIU,Liewei LIU. Influence of Sulfur Deposition on Corrosion Behavior of Carbon Steel L360 Covered with FeS- or FeCO3-film[J]. 中国腐蚀与防护学报, 2016, 36(1): 79-86.
[12] HUANG Bensheng,YIN Wenfeng,WANG Xiaohong,SHI Yijun. Corrosion Behavior of Steels Used in Making Crude Oil Distillation Unit in High Temperature Crude Oil Fractions[J]. 中国腐蚀与防护学报, 2013, 33(5): 377-382.
[13] ZENG Hongtao,XIANG Song,LIU Songlin,HE Yonggang. Corrosion Behaviors of 904L Austenite Stainless Steel in Concentrated Sulfuric Acid Containing Hydrofluoric Acid[J]. 中国腐蚀与防护学报, 2013, 33(3): 182-187.
[14] GUO Yong'an, LI Bosong, LAI Wanhui, GUO Jianting, ZHOU Lanzhang. OXIDATION BEHAVIOR OF Ni-BASED SUPERALLOY K444 AT 900℃ IN AIR DURING LONG TERM[J]. 中国腐蚀与防护学报, 2012, 32(4): 285-290.
[15] HU Chunlian, HOU Shanglin. FAILURE ANALYSIS OF PLUNGERS SPRAYED BY  Ni-BASE ALLOY ON HYDRAULIC FEEDBACK SUBSURFACE PUMP[J]. 中国腐蚀与防护学报, 2012, 32(1): 80-84.
No Suggested Reading articles found!