The synergetic effect of chloride and fluoride on the critical pitting temperature of 316 stainless steel
;;;;;
Cite this article: 

;. The synergetic effect of chloride and fluoride on the critical pitting temperature of 316 stainless steel. J Chin Soc Corr Pro, 2008, 28(1): 30-33 .

Download:  PDF(867KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The influence of concentration of fluoride ion on the pitting corrosion behavior of 316SS has been in?鄄vestigated by means of measuring the critical pitting temperature (CPT) in 0.1 mol/L NaCl solution. The results showed that the CPT decreased and the open circuit potential also decreased with increasing concentration of flu?鄄oride ion. Metastable pitting occurred just below the CPT, while stable pits could only be formed above the CPT. The morphologies of the pits below and above the CPT had been obtained by scanning electron microscope (SEM).
Key words:  stainless steel      critical pitting temperature      fluoride ion      chloride ion      
Received:  17 May 2006     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.jcscp.org/EN/     OR     https://www.jcscp.org/EN/Y2008/V28/I1/30

[1]Brigham R J,Tozer E W.Temperature as a pitting criterion[J].Corrosion-NACE,1973,29:33-42
[2]Qvarfort R.Critical pittingtemperature measurement of stainless steel with an improved electrochemical method[J].Corros.Sci.,1989,29:987-996
[3]Standard test method for electrochemical critical pitting temperature testing of stainless steels,designation:G150-99,Am.Soc.Test.Mater[S].
[4]Moayed M H,Laycock N J,Newman R C.Dependence of the criti-cal pitting temperature on surface roughness[J].Corros.Sci.,2003,45:1203-1216
[5]Moayed M H,Newman R C.Aggressive effects of pitting"inhibitors"on highly alloyed stainless steel[J].Corros.Sci.,1998,40:519-522
[6]Ernst P,Moayed M H,Laycock N J,et al.Passivity of metals and semiconductors VIII,PV99-42[J].Electrochem.Soc.,1999,22:665-679
[7]Abd E I Meguid E A,Abd E I Latif A A.Critical pitting tem-perature for type254SMO stainless steel in chloride solutions[J].Corros.Sci.,2007,2(49):263-275
[8]Bastidas J M,C Fosca C,Chico B,et al.Weight loss and electro-chemical results for two super-austenitic stainless steel in chlo-ride-fluoride mixtures[J].Corros.Sci.,1996,38:559-563
[9]Li M C,Zeng C L,Lin H C.Corrosion behavior of316stainless steel in solutions containing F-/Cl-ions[J].J.Chin.Soc.Corros.Prot.,2002,22(3):162-166(李谋成,曾潮流,林海潮.316不锈钢在F-和Cl-酸性溶液中的腐蚀行为[J].中国腐蚀与防护学报,2002,22(3):162-166)
[10]Cao Z F,Qiao L J,Chu Y W.Study of effect factors to pitting potential of321stainless steel[J].J.Chin.Soc.Corros.Prot.,2006,26(1):22-25(曹占峰,乔利杰,褚武扬.321不锈钢点蚀电位影响因素的研究[J].中国腐蚀与防护学报,2006,26(1):22-25)
[11]WangH T,ZhaoJ M,ZuoY.The effects ofsome anions on metastable pitting of316L stainless steel[J].J.Chin.Soc.Corros.Prot.,2002,22(4):202-206(王海涛,赵景茂,左禹.几种阴离子对316L不锈钢亚稳态孔蚀行为的影响[J].中国腐蚀与防护学报,2002,22(4):202-206)
[12]Ernst P,Newman R C.Pit growth studies in stainless steel foils.I.Introduction and pit growth kinetics[J].Corros.Sci.,2002,44:927-941
[1] ZHENG Kai, WANG Yitao, WANG Dongsheng, LIU Wei, JIANG Yingchang, HUANG Rong, CHANG Xueting. Influence of Corrosion-stress Coupling Effect on Corrosion and Failure of Low-carbon Martensitic Stainless Steel for Polar Marine Propellers[J]. 中国腐蚀与防护学报, 2026, 46(5): 1452-1462.
[2] DONG Shaoyang, LIU Chaokun, LI Yutong, XIA Zhonghu, GAN Lang, LI Cong, REN Yanjie. Cyclic Oxidation Behavior in Air at 900 ℃ of NiCrAlY Coatings Applied by High-speed Laser Cladding[J]. 中国腐蚀与防护学报, 2026, 46(5): 1463-1474.
[3] YE Haifeng, SHEN Shucheng, CHEN Jianghua. Corrosion Behavior of Additively Manufactured 316L Stainless Steel in Artificial Seawater at Different Temperatures[J]. 中国腐蚀与防护学报, 2026, 46(5): 1569-1578.
[4] HE Zhangping, YUAN Yukun, DU Yingzhe, LIN Peng, XU Jian. Crevice Corrosion Behavior of 316LN Stainless Steel in Simulated Electric Heater Overheating Conditions[J]. 中国腐蚀与防护学报, 2026, 46(5): 1579-1587.
[5] LU Yiliang, ZHANG Qiang, JIN Yan, CHEN Yun, YANG Bingkun, WANG Xiaofang, HAN Yu. Effect of Cl--amount on Corrosion Behavior of Cu in Simulated Leaching Solutions of Soil at Korla District of Xinjiang[J]. 中国腐蚀与防护学报, 2026, 46(5): 1605-1612.
[6] LIU Xiacheng, ZOU Jianrong, GAO Liangwen, ZHOU Long, TAN Jibo, WU Xinqiang, ZHANG Ziyu. Corrosion Fatigue Model for Stainless Steel Weld Seam Used in Pressurized Water Reactor Nuclear Power Plants[J]. 中国腐蚀与防护学报, 2026, 46(5): 1613-1618.
[7] SUN Xin, QU Jiawei, GAO Zilin, ZHENG Yue, MA Aili, YAO Lin, ZHANG Lianmin, ZHENG Yugui. Mechanism and Response Surface Model for Effect of Mn2+ on 304L and C25 Stainless Steels in High-temperature Nitric Acid[J]. 中国腐蚀与防护学报, 2026, 46(4): 1015-1030.
[8] ZHANG Jingjing, ZHANG Zhen, ZHAO Zhanyong, BAI Peikang, ZHOU Jie. Effect of NaHSO3 Addition on Corrosion Behavior of 445J2 Ferritic Stainless Steel in NaCl Solution[J]. 中国腐蚀与防护学报, 2026, 46(4): 1197-1206.
[9] WANG Yanfeng, WANG Liuhuo, SUN Shida, LIU Qi, LI Yamei, WANG Xianzong. Research Progress on Failure of Key Materials and Mitigation Measures for Cooling System of Flexible DC Converter Valve[J]. 中国腐蚀与防护学报, 2026, 46(3): 653-662.
[10] ZHANG Xinrui, XUE Baoquan, TAN Jibo, ZHANG Ziyu, GAO Jun, WU Xinqiang. A Review on environmental degradation of Alumina-forming Austenitic Stainless Steel in Liquid Lead-bismuth Eutectic[J]. 中国腐蚀与防护学报, 2026, 46(3): 671-679.
[11] CHEN Xu, LIU Yuhang, GUO Jian, WANG Qishan, LIU Chang, LIU Bin. Crevice Corrosion Behavior of Super 13Cr Stainless Steel in Saturated CO2 Oilfield Produced Fluids[J]. 中国腐蚀与防护学报, 2026, 46(2): 523-532.
[12] ZHANG Jinyu, LI Xin, ZHANG Lei, CHEN Zhihua, DU Yuxin, FENG Hexin, ZHANG Xue, ZHANG Yangpeng, LIN Rushan, LI Ying, RONG Lijian. Corrosion Behavior of Several 17Cr-type Stainless Steels in Chloride Salts Vapor[J]. 中国腐蚀与防护学报, 2026, 46(2): 576-582.
[13] LAN Botao, WU Bin, MING Hongliang, WANG Jianqiu, HAN En-Hou. Research Progress of Stress Corrosion Crack Behavior of Selected Laser Melted Austenitic Stainless Steel in High Temperature Pressurized Water[J]. 中国腐蚀与防护学报, 2026, 46(1): 1-14.
[14] GU Qingyu, SONG Yanfei, ZHANG Liangliang, WANG Nan, LEI Xiaowei. Passivation and Pitting Corrosion Behavior of Laser Directed Energy Deposited 17-4PH Stainless Steel[J]. 中国腐蚀与防护学报, 2026, 46(1): 103-114.
[15] FENG Haoxuan, WANG Fuli, LI Jialin, DU Yao, WEI Boxin, ZHU Shenglong. High Temperature Oxidation and Corrosion Behavior of 316L Stainless Steel Prepared by Selected Laser Melting Process[J]. 中国腐蚀与防护学报, 2026, 46(1): 137-144.
No Suggested Reading articles found!