Study on Erosion-Corrosion of Titanium and 00Cr25Ni22Mo2 Stainless Steel
Jianyun Wang;Yuying Zhou;;
Cite this article: 

Jianyun Wang; Yuying Zhou. Study on Erosion-Corrosion of Titanium and 00Cr25Ni22Mo2 Stainless Steel. J Chin Soc Corr Pro, 2000, 20(2): 123-127 .

Download:  PDF(156KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Erosion-corrosion of Ti and 00Cr25Ni22Mo2 stainless steel in 1mol/L H2SO4 solution was studied with the aid of a self-designed rotating apparatus. The experimental results showed that the erosion-corrosion rate of Ti and the stainless steel increased with increasing rotating speed and increasing temperature, and it approached the maximum at high rotating speed(>4.18m/s) and at high temperature(83℃、92℃).In the present experimental condition, the electrochemical factor played a more important role than the hydrodynamic factor in erosion-corrosion. The Nyquist plots for Ti and 00Cr25Ni22Mo2 stainless steel in 1mol/L H2SO4 solution presented single capacitive loops. Increase in rotating speed reduced the value of polarization resistance of both the materials, but did not change their characteristics of EIS,showing that erosion effect did not change their corrosion mechanism.
Key words:  erosion-corrosion      stainless steel      impendance      titanium      
Received:  28 June 1999     
ZTFLH:  TG172.8  

URL: 

https://www.jcscp.org/EN/     OR     https://www.jcscp.org/EN/Y2000/V20/I2/123

[1 ]徐明林 .钛在尿素生产中的应用 [J].化工腐蚀与防护 ,1 988,1 6 ( 3) :1 8 2 5 .
[2 ]秦平刚 ,裴经昱 .NH3 汽提法尿素生产装置中汽提塔的腐蚀 [A].全国大型尿素装置第十届技术年会文集[C].1 998.73 75
[3]黄嘉琥 .钛在我国尿素设备中的应用 [J].化工腐蚀与防护 ,1 987,1 5 ( 3) ,2 3 2 8.
[4 ]王健云 ,周清木 ,秦平刚 ,张建丽 ,周育英 .工业纯钛和 0 0Cr2 5Ni2 2Mo2不锈钢的缝隙腐蚀 [J].北京化工大学学报 ,1 999,2 6 ( 2 ) :86 88.
[5 ]曹楚南 ,腐蚀电化学 [M].北京 :化学工业出版社 ,1 985 1 41
[1] ZHENG Kai, WANG Yitao, WANG Dongsheng, LIU Wei, JIANG Yingchang, HUANG Rong, CHANG Xueting. Influence of Corrosion-stress Coupling Effect on Corrosion and Failure of Low-carbon Martensitic Stainless Steel for Polar Marine Propellers[J]. 中国腐蚀与防护学报, 2026, 46(5): 1452-1462.
[2] DONG Shaoyang, LIU Chaokun, LI Yutong, XIA Zhonghu, GAN Lang, LI Cong, REN Yanjie. Cyclic Oxidation Behavior in Air at 900 ℃ of NiCrAlY Coatings Applied by High-speed Laser Cladding[J]. 中国腐蚀与防护学报, 2026, 46(5): 1463-1474.
[3] YE Haifeng, SHEN Shucheng, CHEN Jianghua. Corrosion Behavior of Additively Manufactured 316L Stainless Steel in Artificial Seawater at Different Temperatures[J]. 中国腐蚀与防护学报, 2026, 46(5): 1569-1578.
[4] HE Zhangping, YUAN Yukun, DU Yingzhe, LIN Peng, XU Jian. Crevice Corrosion Behavior of 316LN Stainless Steel in Simulated Electric Heater Overheating Conditions[J]. 中国腐蚀与防护学报, 2026, 46(5): 1579-1587.
[5] ZHANG Honglei, ZHENG Ziqi, DONG Kaihui, WANG Zhengbin, SONG Yingwei, ZHENG Yugui. Performance Variation of Ni-P Coatings on Inner Wall of B30 Cu-Ni Alloy Tube Prepared with Chemical Plating Solution of Varying Flow Rates[J]. 中国腐蚀与防护学报, 2026, 46(5): 1588-1594.
[6] LIU Xiacheng, ZOU Jianrong, GAO Liangwen, ZHOU Long, TAN Jibo, WU Xinqiang, ZHANG Ziyu. Corrosion Fatigue Model for Stainless Steel Weld Seam Used in Pressurized Water Reactor Nuclear Power Plants[J]. 中国腐蚀与防护学报, 2026, 46(5): 1613-1618.
[7] SUN Xin, QU Jiawei, GAO Zilin, ZHENG Yue, MA Aili, YAO Lin, ZHANG Lianmin, ZHENG Yugui. Mechanism and Response Surface Model for Effect of Mn2+ on 304L and C25 Stainless Steels in High-temperature Nitric Acid[J]. 中国腐蚀与防护学报, 2026, 46(4): 1015-1030.
[8] ZHANG Jingjing, ZHANG Zhen, ZHAO Zhanyong, BAI Peikang, ZHOU Jie. Effect of NaHSO3 Addition on Corrosion Behavior of 445J2 Ferritic Stainless Steel in NaCl Solution[J]. 中国腐蚀与防护学报, 2026, 46(4): 1197-1206.
[9] WANG Yanfeng, WANG Liuhuo, SUN Shida, LIU Qi, LI Yamei, WANG Xianzong. Research Progress on Failure of Key Materials and Mitigation Measures for Cooling System of Flexible DC Converter Valve[J]. 中国腐蚀与防护学报, 2026, 46(3): 653-662.
[10] ZHANG Xinrui, XUE Baoquan, TAN Jibo, ZHANG Ziyu, GAO Jun, WU Xinqiang. A Review on environmental degradation of Alumina-forming Austenitic Stainless Steel in Liquid Lead-bismuth Eutectic[J]. 中国腐蚀与防护学报, 2026, 46(3): 671-679.
[11] CHEN Xu, LIU Yuhang, GUO Jian, WANG Qishan, LIU Chang, LIU Bin. Crevice Corrosion Behavior of Super 13Cr Stainless Steel in Saturated CO2 Oilfield Produced Fluids[J]. 中国腐蚀与防护学报, 2026, 46(2): 523-532.
[12] ZHANG Jinyu, LI Xin, ZHANG Lei, CHEN Zhihua, DU Yuxin, FENG Hexin, ZHANG Xue, ZHANG Yangpeng, LIN Rushan, LI Ying, RONG Lijian. Corrosion Behavior of Several 17Cr-type Stainless Steels in Chloride Salts Vapor[J]. 中国腐蚀与防护学报, 2026, 46(2): 576-582.
[13] HU Zongwu, LIU Jianguo, WANG Yu, LI Kai. Erosion-corrosion Failure Mechanism of 90° Elbow in 3.5%NaCl Solution Containing Sand[J]. 中国腐蚀与防护学报, 2026, 46(2): 611-619.
[14] LAN Botao, WU Bin, MING Hongliang, WANG Jianqiu, HAN En-Hou. Research Progress of Stress Corrosion Crack Behavior of Selected Laser Melted Austenitic Stainless Steel in High Temperature Pressurized Water[J]. 中国腐蚀与防护学报, 2026, 46(1): 1-14.
[15] SU Baoxian, GAO Ruxin, ZHU Guoqiang, JIANG Botao, WANG Binbin, LIU Chen, YU Yongsheng, WANG Liang, SU Yanqing. Effects of Post Heat Treatment on Microstructure and Corrosion Behavior of Ti-6Al-3Nb-2Zr-1Mo Alloy Fabricated by Electron Beam Freeform Fabrication[J]. 中国腐蚀与防护学报, 2026, 46(1): 81-91.
No Suggested Reading articles found!