Abstract  To understand the application of copper for anti-fouling the dissolution mechanism of copper was investigated in 3% NaCl solution by means of potentiodynamic polarization and electrochemical impedance spectroscopy as well as cyclic voltammetry.Copper in active region dissolved in the form of CuCl2- complex,and the rate of dissolution was controlled by its diffusion from the copper surface to the bulk of the solution.The kinetics mechanism of copper dissolution in active region was suggested.The galvanostatic experiments showed that copper was electrolyxed and than transferred to the surface to be protected against fouling in the form of cuprous species,and that the divergent reaction of cuprous ions to cupric ions had not been found.
Key words:  copper      anticathode      electrolysis      seawater      anti-fouling      electrochemistry      
Received:  25 December 1997     

URL: 

https://www.jcscp.org/EN/     OR     https://www.jcscp.org/EN/Y1999/V19/I1/27

1梁成浩,顾谦农,吴青镐.化工腐蚀与防护,1996,4:15
2Deslouis C, Thibollet B, Mengoli G, Musiani M M.J. Appl. Electrochem, 1988, 18: 374
3Deslouis C, Thibollet B; Mengoli G, Musiani M M.J. Appl. Electrochem, 1988, 18: 384
4Elsner CI, Salvarezza R C, Arvia A J. Electrochim.Acta, 1988, 33(12): 1735
5Benedetti A V, Sumodjo P T A, Nobe K, etal. Electrochim. Acta, 1995; 40(16): 2657
6Tromans D, Silva J C.J. Electrochem. soc.; 1996, 143(2): 458
7Fleischmann M, Hill I R, Mengoli G, Musiani M M, Akhavan J. Electrochim. Acta, 1985; 30(7): 879
8Crousier J; Pardessus L, Crousier J P. Electrochim. Acta.; 1988, 33(8): 1039
[1] CAO Tianhui, YANG Yanqi, LIU Yuwei, WU Lei, GUO Quanzhong, JIA Zhigang, CAO Gongwang, WANG Chuan. Corrosion Behavior of 23MnNiMoCr54 Steel in Artificial High-mineralized Mine Waters of Different pH Values[J]. 中国腐蚀与防护学报, 2026, 46(5): 1537-1548.
[2] WANG Xingbin, LI Jiamin, WU Dengjun, TANG Weineng, YANG Jing, HOU Juan, GUO Jiacheng, YANG Xinyu. Effect of Al-Contents on Corrosion Resistance of Mg-xAl-Zn Alloys[J]. 中国腐蚀与防护学报, 2026, 46(5): 1560-1568.
[3] MA Huanhuan, LV Shengdong, QIAN Yixin, LIN Yong, HAO Xiangping, ZHANG Dawei, WANG Luning. Localized Corrosion and Service Life Prediction of Copper Heat Exchange Tubes in a Sodium Acetate Trihydrate Phase Change Thermal Energy Storage System[J]. 中国腐蚀与防护学报, 2026, 46(4): 1045-1057.
[4] KE Dingfang, WU Fangfang, ZHU Zhaobin, XIE Shengyi, HONG Jing, CHEN Yue, LI Liang, LI Hao, CAO Fahe. Composite of Graphene Oxide/Cerium-based Metal Organic Frameworks for Preparing Protective Coatings with High Stability and Long-term Corrosion Resistance[J]. 中国腐蚀与防护学报, 2026, 46(4): 1095-1106.
[5] LI Zili, WANG Xinji, TIAN Chunyang, YE Peicong, LIU Haiqiao, HE Chenggang, LIU Jihua. Influence of NaCl Temperature and Content on Corrosion Behavior of Heat Treated Rail Steel[J]. 中国腐蚀与防护学报, 2026, 46(4): 1279-1288.
[6] TANG Zhijie, XIE Dongbai, DUO Shuwang, LAI Tian, HONG Hao, SHAN Guo. Influence of Pyrolysis Products of Polyvinyl Chloride on Oxidation Behavior of Cu in Ethanol Combustion Atmosphere[J]. 中国腐蚀与防护学报, 2026, 46(4): 1289-1295.
[7] ZHANG Qiang, LI De, XIAO Diaobin, XIONG Zhuang, SUN Wen. Research on Monitoring and Evaluation Model for Sacrificial Anodes in Seawater Pipelines[J]. 中国腐蚀与防护学报, 2026, 46(4): 1296-1304.
[8] LI Yongkun, ZHOU Jiashun, WANG Youbin, GAO Feng, WANG Xinpeng, TANG Hongqun. Influence of Corrosion Products on Corrosion Behavior of Cut Edges of Galvanized Coatings/Q235 Carbon Steel[J]. 中国腐蚀与防护学报, 2026, 46(3): 703-716.
[9] LU Huayi, LI Ruoyu, CHENG Yufei, BAI Yingxiong, WANG Yanli. Corrosion Behavior of NiCrMoNb and NiCoFeCrMoNb Alloys in Molten NaCl-KCl-MgCl2 at 700 ℃[J]. 中国腐蚀与防护学报, 2026, 46(3): 730-742.
[10] LIU Chenhui, LIU Guangming, ZHU Yanbin, LU Yiliang, ZHANG Lingling, HUANG Zebang. Corrosion Behavior of Pure Zinc in Simulated Underground Seawater Infiltrated Saline-alkali Soils[J]. 中国腐蚀与防护学报, 2026, 46(3): 864-874.
[11] GAO Jinbiao, LIU Yi, ZHAO Haibo, GAO Qinghe, WU Yushen, YU Xin. Mechanistic Investigation in Controlling Metal Corrosion by Synegistic Effect of Ultrasonic and Polymer Corrosion Inhibitors[J]. 中国腐蚀与防护学报, 2026, 46(3): 883-892.
[12] LIU Fan, LIU Fenglian, FAN Songhai, SHAO Qianqiu, ZHOU Kai, LI Zerui, CHEN Yidong, WEN Kecheng, ZHANG Jing. Influence of Radicals on Hydrogen Evolution Corrosion Process of High Voltage Cable Intermediate Joints[J]. 中国腐蚀与防护学报, 2026, 46(3): 919-930.
[13] ZHANG Penghui, ZHAO Jiancang, JIANG Hao, PENG Wenshan, DING Kangkang. Comparative Study on Characteristics and Corrosivity of Seawater Environments in Extreme Marine Areas[J]. 中国腐蚀与防护学报, 2026, 46(3): 931-937.
[14] LIAN Longjiang, CHEN Simin, HUANG Yansong, ZEN Lanxiang, ZHENG Zhong, LEI Bing, MENG Guozhe. Effect of Alternating Dissolved Oxygen Content on Corrosion Behavior of B30 Cu-Ni Alloy in a Simulated Sulfide-polluted Seawater Environment[J]. 中国腐蚀与防护学报, 2026, 46(2): 405-416.
[15] WANG Song, LIU Xuewu, ZHAO Jian, LI Zhong, YANG Jike. Corrosion Inhibition Efficiency of Honeysuckle Extract as an Eco-friendly Inhibitor for Acid Corrosion on Mild Steel[J]. 中国腐蚀与防护学报, 2026, 46(2): 541-548.
No Suggested Reading articles found!