Please wait a minute...
中国腐蚀与防护学报  2005, Vol. 25 Issue (4): 245-249     
  研究报告 本期目录 | 过刊浏览 |
铜银系导电复合材料腐蚀失效研究
朱华;甘复兴
武汉大学资源与环境科学学院
CORROSION FAILURE OF COMPLEX ELECTRICAL CONDUCTIVE MATIERALS FILLED WITH COPPER AND SILVER POWDERS
;
武汉大学资源与环境科学学院
全文: PDF(165 KB)  
摘要: 采用无氰化学镀工艺,研制出一种导电性良好的镀银铜粉,粉末体积电阻率小于2×10-4Ω·cm,用该粉末为填料制成的导电胶,导电率高(导电填料与树脂的重量比为75:25时,体积电阻率为5×10-4Ω·cm)、抗迁移能力强(比银粉导电胶提高近百倍)、导电稳定(经60℃ 相对湿度100%湿热试验1000h,体积电阻率升高小于20%).采用粉末微电极技术研究了导电胶抗迁移的机理,结果表明电偶效应是该导电胶具有抗迁移作用的主要原因,铜作为阳极抑制作为阴极的银的溶解,从而降低银形成枝晶的几率.
关键词 镀银铜粉导电胶腐蚀失效粉末微电极    
Abstract:One new kind of silver-plated copper powder with high conductivity (volume resistivity of the powder is less than 2×10-4Ω·cm) was developed by the electroless plating without cyanide.The ECAs filled with this silver-plated copper powder exhibit high conductivity ( the volume resistivity of ECAs is less than 5×10-4Ω·cm when the mixing proportion of the resin to powder is 25:75 by weight) ,high migration-resistance (the shortcut time is 100 time longer than silver-filled ECAs in the migration test ) and high electric conductive stability (the volume esistivity increase is not more than 20% after 1000 hours humid-heat test in the condition of 60℃and RH100%).The mechanism of anti-migration was studied using powder microelectrode technique and other electrochemical methods.The results show galvanic coupling effect plays an important role in the anti-migration.Copper as anode restrains cathodic silver dissolved during dissolution then decreases the probability of dendritic growth.
Key wordssilver-plated copper    electrical conductive adhesive    corrosion failure    powder microelectrode
收稿日期: 2004-02-23     
ZTFLH:  TG172  
通讯作者: 朱华     E-mail: zhuhua67@sohu.com

引用本文:

朱华; 甘复兴 . 铜银系导电复合材料腐蚀失效研究[J]. 中国腐蚀与防护学报, 2005, 25(4): 245-249 .
. CORROSION FAILURE OF COMPLEX ELECTRICAL CONDUCTIVE MATIERALS FILLED WITH COPPER AND SILVER POWDERS. J Chin Soc Corr Pro, 2005, 25(4): 245-249 .

链接本文:

https://www.jcscp.org/CN/      或      https://www.jcscp.org/CN/Y2005/V25/I4/245

[1]SteppanJJ,RothJA.Areviewofcorrosionfailuremechanisms duringacceleratedtests[J].J.Electrochem.Soc.,1987,134(1):175
[2]GaoBJ,JiangHM,etal.Astudyonthemechanismofmicrometer copperpowderplated-silverusingargentaminesolution[J].Chin.J.InorganicChemisity,2000,16(4):669(高保娇,蒋红梅等.用银氨溶液对微米级铜粉镀银反应机理的研究[J].无机化学报,2000,16(4):669)
[3]TanFB,CaiYZ,etal.Chemicallysilveringcopperpowderandits properties[J].PreciousMetals,2000,21(3):8(谭富彬,蔡云卓等.铜粉末化学镀银及其性能[J].贵金属,2000,21(3):8)
[4]ZhaQX.FundamentalsofKineticsofElectrodeProcesses[M].Bei jing:SciencePress,2002,368-376(查全性.电极过程动力学导论[M].北京:科学技术出版社,2002:368-376)
[5]TangH,FangXF,LuoYX.Astudyonconductivemechanismof conductivepolymercompositesandcalculationofresistivity[J].PolymerMater.Sci.Eng.,2000,12(6):1(汤浩,防欣芳,罗云霞.复合型导电高分子材料导电机理研究及电阻率计算[J].高分子材料科学与工程,2000,12(6):1
[6]CharlesGuanY,HanKennethN.Anelectrochemicalstudyonthe dissolutionofcopperandsilverfromsilver-copperalloys[J].J.Electrochem.Soc.,1995,142(6):1819I
[1] 杨根柱,李庆华,刘国帅,王博,刘杰,熊金平,何少平,陆正良. W0714己内酰胺薄膜蒸发器下料管管壁腐蚀减薄失效分析[J]. 中国腐蚀与防护学报, 2011, 31(6): 488-492.
[2] 李春福 王 戎 牛艳花 朱泽华 李天雷. 纳米掺杂对Al2O3+13%TiO2等离子喷涂涂层耐蚀性能的影响[J]. 中国腐蚀与防护学报, 2008, 28(6期): 331-336.
[3] 王立世; 潘春旭; 蔡启舟; 魏伯康 . 镁合金表面微弧氧化陶瓷膜的腐蚀失效机理[J]. 中国腐蚀与防护学报, 2008, 28(4): 219-224 .
[4] 吕小军; 张琦; 项民; 刁鹏; 栗晓飞; 谢国君 . 环境因素对复合材料力学性能的影响[J]. 中国腐蚀与防护学报, 2007, 27(2): 97-100 .
[5] 罗逸; 邓聚龙; 郑家shen . 腐蚀评估中的灰靶方法[J]. 中国腐蚀与防护学报, 2001, 21(6): 374-378 .