Please wait a minute...
中国腐蚀与防护学报
  技术报告 本期目录 | 过刊浏览 |
十八硫醇自组装膜对电偶腐蚀的抑制作用
万俐1,杜伟李佳佳2,丁毅2,陈步荣2
1. 南京博物院
2. 南京工业大学
Inhibition effect of the odtadecanethiol self-assembled monolayers for bronze-silver galvanic Corrosion
全文: PDF(408 KB)  
摘要: 

针对错银铜器的青铜-银电偶腐蚀问题,采用十八硫醇(ODT)的乙醇溶液在青铜和银表面制备了自组装膜(SAMs)。通过测量青铜-银的电偶对电流,研究了自组装前后的电偶腐蚀性能,并且采用X光电子能谱(XPS)、Tafel极化曲线法和微分电容法初步研究了ODT SAMs的作用机理。结果表明:ODT分子通过硫原子与基体形成硫醇盐,吸附在青铜和银表面形成自组装膜,该自组装膜在3.5%NaCl溶液中具有良好的电化学稳定性,能够有效抑制青铜和银之间的电偶腐蚀,属于混和抑制型缓蚀剂。

Abstract

In order to solve the galvanic corrosion problem between bronze and silver , the self-assemble monolayers(SAMs) of odtadecanrthiol(ODT) was prepared on the surfaces of bronze and silver. Corrosion inhibition and function mechanism of ODT SAMs were investigated by couple corrosion current, XPS, polarization curves and differential capacity methods. The results show that ODT molecular adsorbs on the surface of bronze and silver to form SAMs through the formation of thiolate. In NaCl solution of 3.5% concentration, the ODT SAMs have a good electrochemical stability and prohibit the galvanic corrosion between bronze and silver effectively. ODT SAMs are a kind of mixed inhibition inhibitors.

收稿日期: 2012-06-26     
ZTFLH:  TG172.3  
通讯作者: 陈步荣   

引用本文:

万俐 杜伟 李佳佳 丁毅 陈步荣. 十八硫醇自组装膜对电偶腐蚀的抑制作用[J]. 中国腐蚀与防护学报, .

链接本文:

https://www.jcscp.org/CN/Y0/V0/I0/0

[1]Nuzzo R G, Allara D L, Ralph G N. Adsorption of bifunction arganic disulfides on gold sufaces[J]. Journal of the American Chemical Society, 1983,105(13):4481-4483.

[2] Metikos-Hukovic M, Babic R, Petrovic. Copperprotection by a self-assembled monolayer of alkanethiol: Comparison with benzotriazole[J].Journal of the Electrochemical Society,2007,154(2):138-143

[3] LI Degang, Yu Xianjin, Dong Yunhui. The different self-assembled way of n-andt-dodecyl mercaptan on the surface of copper[J].Applied Surface Science, 2007, 253(9):4182-4187.

[4]Magali E, Michel K, Hisasi T. The formation of self-assembleing membrane of hexadecane-thiol on silver to prevent the tarnishing[J]. Electrochi Acta, 2004,49:1937

[5]Burleigh T D, Shi C, Kilic S. Self-assembled monolayers of perfluoroalkyl amideethanethiols, fluoroalkythios, and alkylthiols for the prevention of silver tarnish[J]. Corrosion , 2002, 58 (1):49

[6]Y. Feng, W. K. Teo, K. S. Siow, Z. Gao, K. L. Tan, A. K. Hsieh. Corrosion protect of copper by a self-assembled monolayer of alkanethiol [J] .J Electeochem Soc. 1997, 144(1): 55-64.

[7] Schweize M, Hagenstrom H, Kolb D M. Potential-induced structure transitions in self-assembled monolayer: ethanrthiol Au(100)[J]. Surface Science, 2001,490(3): 627-636.

[8] Xun Qunjie,Wang Zhongyao, Yin Renhe et al. Inhibition Action of the Self-Assembled Monolayers of 3-Amino-1,2,4-triazole on Brass[J]. Acta Phys. –Chim. Sin.,2008, 24(1):115-120

(徐群杰,万宗跃,印仁和,朱律均,曹为民,周国定,林昌健。3-氨基-1,2,4-三氨基自组装膜对黄铜的缓蚀作用。物理化学学报,2008,24(1):115-120)

[9] Wang Xianqun,Liu Ruiquan,Zhu Liqin. Inhibition action and adsorption behaviors of BIT,BIOHT and BIMMT on Copper in alkaline mediume[J]. Acta Phys-Chim Sin,2007,23(1):21-26

(王献群,刘瑞泉,朱丽琴,宫建伟.碱性介质中BIT, BIOHT和BIMMT对铜的缓蚀作用和吸附行为[J].物理化学学报,2007,23(1):21-26)

[10] Elsayed M S,Erasmus R M, Comins J D. Effects of 3-amino-1,2,4-triazole on the inhibition of copper in acidic chloride solutions[J]. J Colloid Interface Sci,2007,311(1):144-151.

[11] Liao Qiangqiang,Yue Zhongwen,Zhu Zhongwei et al,,Corrosion Inhibition Effect of Self-Assembled Monolayers of Ammonium Pyrrolidine Dithiocarbamate on Copper[J]. Acta Physico-Chimica Sinica, 2009,25(08):1658

(廖强强; 岳忠文; 朱忠伟等. 吡咯烷二硫代氨基甲酸铵自组装膜对铜的缓蚀作用[J].物理化学学报, 2009,25(08):1658)

[12] Ralph G. Nuzzo, Bernard R. Zegarski, Lawrence H. Dubois. Fundamental Studies of the Chemisorption of Oranosulfur Compoumds on Au(1 1 1). Implication for Molecular Self-Assembly on Gold Surfaces[J].J Am Chem Soc, 1987,109(3):733-740

[13]Chenhao Liang, Changjiang Yang, Naibao Huang. Tarnish protection of silver by octadecanethiol self-assembled monolayers prepared in aqueous micellar solution y[J].Surface &Cotaings Technolog,2009,203:1034-1044

[14]Paul E Laibinis, George M Whitesides, David L Allara et al. Comparison of the structres and wetting properties of self-assembled monolayer of n-alkanethiols on the coinage metal surface,Cu,Ag,Au[J]. Journal of the American Chemical Socirty,1991,113(19):7151-7167.

[15] B.V. Appa Rao ,Md. Yakub Iqbal, B. Sreedhar. Self-assemble monolayer of 2-(octadecythio)benzothiazole for corrosion protection of copper[J]. Corrosion Science. 2009,51:1441-1452.

[16] Yang Zhangjiang, Liang Chenghao, Zhang Xu. Self-Assembled Monolayers Prepared on Silver Surface in Aqueous Micellar Solution [J] .Rare Metal Materials and Engineering. 2010,39(9):1676-1681.

(杨长江,梁成浩,张旭. 水溶液中银表面组装膜工艺. 稀有金属材料与工程. 2010,39(9):1676-1681).

[1] 赵海洋 高多龙 张童 吕由 张宇鹏 张欣欣 石鑫 魏晓静 刘冬梅 董泽华. 电弧增材制造航空AA2024铝合金的微观结构及其腐蚀行为研究[J]. 中国腐蚀与防护学报, 0, (): 0-0.
[2] 陈文娟, 方莲, 潘刚. O3/SO2复合大气环境中Q235B钢的腐蚀演化特性[J]. 中国腐蚀与防护学报, 2021, 41(4): 450-460.
[3] 李子运, 王贵, 罗思维, 邓培昌, 胡杰珍, 邓俊豪, 徐敬明. 热带海洋大气环境中EH36船板钢早期腐蚀行为研究[J]. 中国腐蚀与防护学报, 2020, 40(5): 463-468.
[4] 赵博儒, 孙志, 赵健伟, 陈智栋. 正十六硫醇分子在Ag表面的自组装动力学及其保护作用[J]. 中国腐蚀与防护学报, 2020, 40(3): 281-288.
[5] 范益,陈林恒,蔡佳兴,代芹芹,马宏驰,程学群. 热轧AH36船板钢在室内仓储条件下的腐蚀行为研究[J]. 中国腐蚀与防护学报, 2020, 40(1): 10-16.
[6] 冯亚丽,白子恒,陈利红,魏丹,张东玖,姚琼,吴俊升,董超芳,肖葵. Corten-A耐候钢在模拟污染海洋大气环境中的加速腐蚀相关性研究[J]. 中国腐蚀与防护学报, 2019, 39(6): 519-526.
[7] 郭铁明,张延文,秦俊山,宋志涛,董建军,杨新龙,南雪丽. 桥梁钢Q345q在3种模拟大气环境中的腐蚀行为研究[J]. 中国腐蚀与防护学报, 2019, 39(4): 319-330.
[8] 邓俊豪,胡杰珍,邓培昌,王贵,吴敬权,王坤. 氧化皮对SPHC热轧钢板在热带海洋大气环境中初期腐蚀行为的影响[J]. 中国腐蚀与防护学报, 2019, 39(4): 331-337.
[9] 郭铁明 张延文 秦俊山 宋志涛 董建军 杨新龙. 桥梁钢Q345q在三种模拟大气环境中的腐蚀行为研究[J]. 中国腐蚀与防护学报, 0, (): 0-0.
[10] 姚望, 周和荣, 肖葵, 刘鹏洋, 但佳永, 吴润. 中性盐雾环境中DC06超深冲钢的腐蚀行为研究[J]. 中国腐蚀与防护学报, 2018, 38(3): 241-247.
[11] 夏大海, 宋诗哲, 王吉会, 高志明, 胡文彬. 食品包装用镀锡薄钢板的腐蚀机理研究进展[J]. 中国腐蚀与防护学报, 2017, 37(6): 513-518.
[12] 罗睿, 吴军, 柳鑫龙, 周学杰, 郑鹏华, 张三平. Q235和09CuPCrNi-A钢在两种不同大气环境中腐蚀早期锈层演化研究[J]. 中国腐蚀与防护学报, 2014, 34(6): 566-573.
[13] 刘雨薇, 王振尧, 王军, 胡波涛. 输电塔杆用热浸镀锌钢在模拟酸雨大气环境中的腐蚀行为[J]. 中国腐蚀与防护学报, 2014, 34(5): 426-432.