动载荷条件下紫铜/铬青铜受流摩擦磨损性能
胡道春;孙乐民;上官宝
河南科技大学材料科学与工程学院 洛阳 471003
TRIBOLOGICAL CHARACTERISTICS OF T2/QCr0.5 RUBBING PAIRS WITH ELECTRIC CURRENT AND DYNAMIC LOAD
HU Daochun;SUN Lemin;SHANGGUAN Bao
Institute of Materials Science and Engineering;Henan University of Science and Technology;Luoyang 471003
全文: PDF(1565 KB)  
摘要: 

以紫铜/铬青铜摩擦副为研究对象模拟受电弓与导线的服役条件,在HST100型销盘式高速载流试验机上考察了该材料在动载荷(按正弦规律加载)条件下受流摩擦磨损性能。结果表明:在动载荷条件下,电流是影响其摩擦磨损性能的重要因素。摩擦系数、磨损率均随电流的增大递增,但随着电流的进一步增加其增大趋势减缓;粘着磨损、电弧侵蚀、塑性变形是其主要的磨损形式。

关键词 动载荷受流摩擦磨损性能摩擦系数磨损率粘着磨损电弧侵蚀塑性变形    
Abstract

The tribological characteristics of T2/QCr0.5 rubbing pairs under the load of sine shock pulse and in the electrical current of various intensities, which simulated working conditions of the pantograph-wire system used in electrical railway, were examined on the pin-on-disc friction and wear tester of HST100.The results show that the electrical current is the important effect factor on tribological properties with electrical current, friction coefficient and wear rate increase with current intensity whereas the tendency is slow up with the further increasing of electrical current. The most wear form is adhesive wear, arc erosion and plastic deformation.

Key wordsdynamic load    current-carrying    tribological characteristics    friction coefficient    wear rate    adhesive wear    arc erosion    plastic deformation
收稿日期: 2007-05-14     
ZTFLH: 

TG146.1

 
基金资助:

国家重点基础研究发展规划项目(2007CB607603);国家自然科学基金项目(50775066);河南省高校科技创新人才项目(2009HASTIT008);河南省创新团队项目

 

 

通讯作者: 孙乐民     E-mail: sunlm@mail.haust.edu.cn
Corresponding author: SUN Lemin     E-mail: sunlm@mail.haust.edu.cn

引用本文:

胡道春 孙乐民 上官宝. 动载荷条件下紫铜/铬青铜受流摩擦磨损性能[J]. 中国腐蚀与防护学报, 2009, 29(1): 35-39.
LI Yun-Chun, PAN Qing-Lin, LIANG Wen-Jie, HE Yun-Bin, LUO Cong-Ge. TRIBOLOGICAL CHARACTERISTICS OF T2/QCr0.5 RUBBING PAIRS WITH ELECTRIC CURRENT AND DYNAMIC LOAD. J Chin Soc Corr Pro, 2009, 29(1): 35-39.

链接本文:

https://www.jcscp.org/CN/      或      https://www.jcscp.org/CN/Y2009/V29/I1/35

[1] Paul G Hegda,Gordon J Thackray. Computer evaluation of electric railway catenary equipment by the method of normal modes[J]. IEEE Trans. Ind.,1981,17(9):139-145
[2] Yu D. Analysis on catenary current-carrying theory of high-speed railway [J]. J. Chin. Railway Soc.,1998, 20(5):58-64
(于涤. 高速接触网受流的理论分析[J].铁道学报,1998,20(5): 58-64)
[3] He D H,Rafael R Manory,Norm Grady. Wear of railway contact wires against current collector materials [J].Wear,1998,215(1-2):146-155
[4] Shunichi Kubo,Koji Kato. Effect of arc discharge on wear rate of Cu-impregnated carbon strip in unlubricated sliding against Cu trolley under electric current[J]. Wear, 1998,216:179-183
[5] Chang Q Y,Meng Y G,Wen S Z. The influence of electrode potential on the friction behavior of silicon nitride ball/brass plate sliding couple [J]. Tribology,2002,22 (5):373-376
(常秋英,孟永钢,温诗铸.电极电势对氮化硅/黄铜滑动摩擦副摩擦磨损性能的影响研究[J]. 摩擦学学报,2002,22(5): 373-376)
[6] Senouci A,Zaidi H,Frene J,et al. Damage of surface in sliding electrical contact copper/steel.[J]. Appl. Surf.Sci.,1999,144-145: 287-291
[7]  Tian X L,Lin Y Z,Liu J J,et al. Electrochemical behavior in erosion-corrosion of carbon steel in liquid-solid double phase flow loop [J]. J. Chin. Soc. Corros. Prot.,2004, 24(1):48-51
(田兴玲,林玉珍,刘景军等. 碳钢在液/固双相管流中磨损腐蚀的电化学行为[J]. 中国腐蚀与防护学报,2004,24(1):48-51)
[8] Yu L. Study on the wear mechanism of Au-Rare earth alloy wires[J].Tribology,2002,22(4):282-285
(虞澜.金-稀土合金电刷丝的磨损机理研究[J].摩擦学学报, 2002,22(4):282-285)
[9] He D H,Manory R,Sinkis H. A sliding wear tester for overhead wires and current collectors in light rail systems[J].Wear,2000,239(1):10-20
[10] Azevedo C R F,Sinatora A. Failure analysis of a railway copper contact strip.[J].Eng.Fail. Anal.,2004,11:829-841

[1] 陈磊,裴志亮,肖金泉,宫骏,孙超. 磁过滤电弧离子镀制备TiAlN涂层的结构与性能表征[J]. 中国腐蚀与防护学报, 2017, 37(3): 241-246.
[2] 李靖,马志瀛,黄绍平,李建明,许利战. 400 Hz低压阻性小电流电弧对银石墨触头材料的侵蚀研究[J]. 中国腐蚀与防护学报, 2010, 30(3): 231-235.
[3] 王蕾 胡道春. C/C复合材料抗电弧侵蚀性能研究[J]. 中国腐蚀与防护学报, 2009, 29(3): 235-240.
[4] 王燕斌; 王胜; 颜练武 . 塑性变形在氢致断裂中的作用[J]. 中国腐蚀与防护学报, 2000, 20(4): 248-252 .