AN ANALYSIS OF FAILURE IN CAST IRON SEAWATER BURIED PIPE
;;
华东理工大学;上海应用技术学院
Cite this article: 

. AN ANALYSIS OF FAILURE IN CAST IRON SEAWATER BURIED PIPE. J Chin Soc Corr Pro, 2005, 25(3): 183-186 .

Download:  PDF(246KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  This paper mainly analyses the cause and principle of the failure in cast iron seawater pipe.The pipe is 630 mm of inside diameter and 12 mm of wall thickness.In the inner wall coating was polymer sand plasma.There was a big corroded hole in the pipe.With the help of morphological character and metallographic examination,it was found that on the matrix material there were small holes with different depth and size and only few pearlite matrix was left.With the help of microanalysis,it was found that in the inner wall there were Cl\+- and oxygen.With the help of scanning electron microscope,it was found that in the crack area there was oxide in the shape of line.In the same time it was found the value of rigidity was lower in inner face than in outer face.Through the analysis we can confirm the cause of the failure is the action of electrochemical corrosion and chemical corrosion when the Cl\+- and oxygen were existed.The equation of the electrochemical corrosion is also discussed.
Key words:  seawater      cast iron pipe      corrosion principle      failure analysis      
Received:  12 January 2004     
ZTFLH:  TG172.5  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.jcscp.org/EN/     OR     https://www.jcscp.org/EN/Y2005/V25/I3/183

[1]MakarJM.Apreliminaryanalysesoffailuresofgraycastironwater pipe[J].EngineeringFailureAnalysis,2000,7:43-53
[2]NevilleA,HodgkiessT,XuH.Anelectrochemicalandmicrostruc turalassessmentoferosion-corrosionofcastiron[J].Wear,1999,(233-235):523-534
[3]WangRF,WeiH,XiaLT.There-corrosionofcastironinthe environmentofsea[J].ResearchStudiesonFoundryEquipment,2001,(05):25-27(王荣峰,韦华,夏兰廷.铸铁在海洋腐蚀环境下的防护措施[J].铸造设备研究,2001,(05):25-27)
[4]XiaLT,WeiH.Effectofgraphitemorphologyonthecorrosion propertiesofcastironinthestillsea[J].J.TaiyuanHeavyMachin eryInstitute,2002,23(1):532-534,547(夏兰廷,韦华.石墨形态对铸铁静海腐蚀性能的影响[J].太原重型机械学院学报,2002,23(1):532-534,547)
[1] ZHANG Qiang, LI De, XIAO Diaobin, XIONG Zhuang, SUN Wen. Research on Monitoring and Evaluation Model for Sacrificial Anodes in Seawater Pipelines[J]. 中国腐蚀与防护学报, 2026, 46(4): 1296-1304.
[2] LIU Chenhui, LIU Guangming, ZHU Yanbin, LU Yiliang, ZHANG Lingling, HUANG Zebang. Corrosion Behavior of Pure Zinc in Simulated Underground Seawater Infiltrated Saline-alkali Soils[J]. 中国腐蚀与防护学报, 2026, 46(3): 864-874.
[3] ZHANG Penghui, ZHAO Jiancang, JIANG Hao, PENG Wenshan, DING Kangkang. Comparative Study on Characteristics and Corrosivity of Seawater Environments in Extreme Marine Areas[J]. 中国腐蚀与防护学报, 2026, 46(3): 931-937.
[4] MA Xiao, XU Xuelei, TONG Hongtao, WANG Xin, ZHAO Mingyu, WANG Xuan, SHEN Jie, LIU Guangyi. Erosion-corrosion Characteristics of B10 Cu-Ni Alloy Seawater Control Valve in Flowing Seawater Conditions[J]. 中国腐蚀与防护学报, 2026, 46(1): 283-290.
[5] SUN Shibin, GAO Hao, CHANG Xueting, WANG Dongsheng. Failure Behavior of Fine-grained FH40 Marine Low-temperature Steel in Conditions of Coupling Effect of Seawater-sea Ice[J]. 中国腐蚀与防护学报, 2025, 45(6): 1659-1668.
[6] WEI Ran, JIANG Quantong, SUN Chen, WANG Weiwei, DUAN Jizhou, HOU Baorong. A Review on Corrosion and Protection of Mg-alloy in Marine Environment[J]. 中国腐蚀与防护学报, 2025, 45(3): 533-547.
[7] LIU Jiabing, HUANG Shiyu, GUO Na, GUO Zhangwei, LIU Tao. Corrosion Behavior of EH40 Marine Steel in Artificial Seawater at Low- and Ambient-Temperatures[J]. 中国腐蚀与防护学报, 2025, 45(3): 620-630.
[8] XIE Wenzhen, WANG Zhenyu, HAN En-Hou. Passivation Behavior of Corrosion Resistant Rebar Steels as Bare Steels in a Simulated Concrete Pore Fluid and as Rebar Steels Embedded in Concrete Made of Cement and Sea-sand in a Simulated Seawater[J]. 中国腐蚀与防护学报, 2024, 44(6): 1454-1464.
[9] ZHAO Lianhong, WANG Yingqin, LIU Yuanhai, HE Weiping, WANG Haowei. Corrosion Behavior of Four Steels for Landing Gear of Amphibious Aircraft in Simulated Seawater[J]. 中国腐蚀与防护学报, 2024, 44(5): 1263-1273.
[10] MA Xiaowei, XUE Rongjie, WANG Taotao, YANG Liang, LIU Zhenguang. Comparison of Corrosion Resistance of Zr-based Amorphous Alloys and Traditional Alloys in Seawater[J]. 中国腐蚀与防护学报, 2024, 44(4): 949-956.
[11] PENG Wenshan, XING Shaohua, QIAN Yao, LIN Cunguo, HOU Jian, ZHANG Dalei. Effect of Flowing Seawater on Corrosion Characteristics of Passivation Film on TA2 Pure-Ti Pipes[J]. 中国腐蚀与防护学报, 2024, 44(4): 1038-1046.
[12] XING Shaohua, PENG Wenshan, QIAN Yao, LI Xiangbo, MA Li, ZHANG Dalei. Effect of Seawater Flow Velocity on Pitting Corrosion of 2205 Stainless Steel with Different Surface Treatments[J]. 中国腐蚀与防护学报, 2024, 44(3): 658-668.
[13] SUN Jiayu, PENG Wenshan, XING Shaohua. Combined Effect of Stress and Dissolved Oxygen on Corrosion Behavior of Ni-Cr-Mo-V High Strength Steel[J]. 中国腐蚀与防护学报, 2024, 44(3): 755-764.
[14] XING Shaohua, LIU Zhongye, LIU Jinzeng, BAI Shuyu, QIAN Yao, ZHANG Dalei. Galvanic Corrosion Behavior of ZCuSn5Pb5Zn5/B10 Couple in Flowing Seawater[J]. 中国腐蚀与防护学报, 2023, 43(6): 1339-1348.
[15] DENG Chengman, LIU Zhe, XIA Da-Hai, HU Wenbin. Localized Corrosion Mechanism of 5083-H111 Al Alloy in Simulated Dynamic Seawater Zone[J]. 中国腐蚀与防护学报, 2023, 43(4): 683-692.
No Suggested Reading articles found!