Please wait a minute...
J Chin Soc Corr Pro  2000, Vol. 20 Issue (2): 65-73     DOI:
Research Report Current Issue | Archive | Adv Search |
Effect of Sulfide Inclusions on Propagation of Pitting in Carbon Steels
Xuequn Chen;Xiaodong Kong;Sicheng Yang
武汉市海军工程大学金工教研室
Cite this article: 

Xuequn Chen; Xiaodong Kong; Sicheng Yang. Effect of Sulfide Inclusions on Propagation of Pitting in Carbon Steels. J Chin Soc Corr Pro, 2000, 20(2): 65-73 .

Download:  PDF(318KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Using OCC simulation test, behavior of pitting propagation of two carbon steels for shipbuilding with different sulfide inclusions in synthetic seawater was studied. Test results showed that the zero current potential of the steel with type Ⅱ sulfide was more negative than that of the steel with type Ⅰ sulfilde; and at the same cathodic polarization potential, the anodic dissolution current of the former was greater than that of the latter. The effect of sulfide inclusions on the pitting propagation was examined by means of microanalysis. It was found that the sulfide accelerated propagation of the pit with a higher dissolution speed than that of the steel matrix. Because type Ⅱ sulfide was of the thin piece shape and presented in crowds, the dissolution along it could easily spread from one piece to another. Type Ⅰsulfide, with the shape similar to potato or cigar, presented in steel bulk separately. Such that, the dissolution around the latter couldn't spread as the former did. In addition, because typeⅡ sulfide had much larger Sv (phase boundary surface) than type Ⅰ sulfide, the corrosion propagation of the macro-pit was accelerated much more quickly by the former than by the latter.
Key words:  carbon steel      pitting      OCC      sulfide inclusion      
Received:  27 April 1999     
ZTFLH:  TG172.5  

URL: 

https://www.jcscp.org/EN/     OR     https://www.jcscp.org/EN/Y2000/V20/I2/65

[1 ]WranglenG .Pittingandsulphideinclusionsinsteel[J] CorrSci ,1 974,1 4:331 34 9
[2 ]SimsCE ,DahleFB Effectofaluminumonthepropertiesofmediumcarboncaststeel[J] TransAFA ,1 938,46 :6 5 1 0 8
[3]PourbaixA Characteristicsoflocalizedcorrosionofsteelinchloridesolutions[J] Corrosion ,1 971 ,2 7( 1 1 ) :449 45 4
[4 ]李静媛 钢和钼中夹杂物的鉴定 [M] 北京科学出版社 ,1 988 p93
[5 ]WranglenG .Activesulfidesandthepittingcorrosionofcarbonsteels[A] InterConfOnLocCorr[C] Williamsburg ,USA ,1 971 ,p46 2 476
[6 ]魏宝明 金属腐蚀理论及应用 [M] 北京 :化学工业出版社 ,1 984 p80 ,1 0 0
[7]SrivastavaSC ,IvesMB Dissolutionofinclusionsinlowalloysteelexposedtochloride containingenvironments[J] Cor rosion ,1 987,43( 1 1 ) :6 87 6 92]
[1] XIE Jingli, WANG Youzhi, QIAO Shuzhen, NIU Jiayu, HAO Long, CAO Shengfei, WANG Jianqiu. Recent Advances in Evolution of Carbon Steel Corrosion Products in Near-field Environment of Geological Repositories for High-level Radioactive Waste[J]. 中国腐蚀与防护学报, 2026, 46(5): 1343-1352.
[2] HUANG Hulingtong, WANG Cheng, CHENG Xuequn, YANG Xiaojia, ZHANG Zhanwu, LI Liang. Corrosion Behavior of Q235 Carbon Steel in a Simulated Saline Soil of Southern Xinjiang[J]. 中国腐蚀与防护学报, 2026, 46(5): 1595-1604.
[3] MA Huanhuan, LV Shengdong, QIAN Yixin, LIN Yong, HAO Xiangping, ZHANG Dawei, WANG Luning. Localized Corrosion and Service Life Prediction of Copper Heat Exchange Tubes in a Sodium Acetate Trihydrate Phase Change Thermal Energy Storage System[J]. 中国腐蚀与防护学报, 2026, 46(4): 1045-1057.
[4] WU Fangyun, QIAO Ruixin, LI Xuning, SHANG Haojie, LU Fenghua, ZHOU Cheng, WANG Xin, DONG Liang. Influence of Seawater Flow Characteristics Inside Pipelines on Cathodic Protection of Carbon Steel Pipelines-Experiment and Numerical Simulation[J]. 中国腐蚀与防护学报, 2026, 46(4): 1081-1094.
[5] LU Haifeng, MIAO Qiang, LIANG Wenping, YAO Zhimeng, WEI Shaochong, CHEN Guoxing. Effect of Laser Surface Cleaning on Corrosion Resistance of Stainless Steel[J]. 中国腐蚀与防护学报, 2026, 46(4): 1227-1237.
[6] WEI Xuguang, WANG Weibin, LI Kang, ZHANG Cancan, WU Yuting, LU Yuanwei, WANG Guoqiang, ZHAO Bo. Dynamic Corrosion Behavior of Q345R Carbon Steel in High-temperature Hitec Molten Salt[J]. 中国腐蚀与防护学报, 2026, 46(3): 693-702.
[7] HU Zongwu, LIU Jianguo, WANG Yu, LI Kai. Erosion-corrosion Failure Mechanism of 90° Elbow in 3.5%NaCl Solution Containing Sand[J]. 中国腐蚀与防护学报, 2026, 46(2): 611-619.
[8] GU Qingyu, SONG Yanfei, ZHANG Liangliang, WANG Nan, LEI Xiaowei. Passivation and Pitting Corrosion Behavior of Laser Directed Energy Deposited 17-4PH Stainless Steel[J]. 中国腐蚀与防护学报, 2026, 46(1): 103-114.
[9] LI Zhaonan, HOU Yucen, JU Peng, ZHUANG Tiegang, CHEN Jingjie, WANG Mingyu, XU Yunze. Influence of Simulated Electrolyte Droplets with Varied Conductivity on Atmospheric Corrosion of Carbon Steel[J]. 中国腐蚀与防护学报, 2025, 45(6): 1537-1548.
[10] WANG De, ZHANG Fan, WANG Xingqi, ZHANG Hexin, ZHAO Chengzhi, YANG Yange. Long-term Corrosion Resistance of Carbon Steel and Al-alloy with Single Component Fluorocarbon Modified Epoxy Coating[J]. 中国腐蚀与防护学报, 2025, 45(6): 1549-1562.
[11] DUAN Jingmin, DONG Yong, MIAO Dongmei, YANG Yujing, MAO Lingbo, ZHANG Zhengrong. Corrosion Behavior in Different Media and Mechanical Properties of Al0.5CoCrFeNi High-entropy Alloy After Heat Treatment[J]. 中国腐蚀与防护学报, 2025, 45(4): 983-994.
[12] ZHANG Guoqing, YU Zhixia, WANG Yuesong, WANG Zhi, JIN Zhengyu, LIU Hongwei. Corrosion Behavior of Steel Materials in Marine Supercritical Carbon Dioxide Environment[J]. 中国腐蚀与防护学报, 2025, 45(4): 1061-1069.
[13] PENG Liyuan, XIE Jingli, CAO Shengfei, TAN Jibo, WU Xinqiang, ZHANG Ziyu. Review on Corrosion Thickness Design of Canister for High-level Radioactive Waste in Japan[J]. 中国腐蚀与防护学报, 2025, 45(3): 563-576.
[14] XU Zhiyu, HU Qian, HUANG Feng, LIU Jing, LU Xianzhong. Effect of Crevice Geometry on Chemical Environment of Crevice Solution and Corrosion Behavior of 2205 Duplex Stainless Steel[J]. 中国腐蚀与防护学报, 2024, 44(6): 1581-1588.
[15] HONG Xiaomu, WANG Yongqiang, LI Na, TIAN Kai, DU Juan. Effect of Aging on Microstructures and Localized Corrosion of Custom455 Martensitic Age-hardening Stainless Steel[J]. 中国腐蚀与防护学报, 2024, 44(5): 1285-1294.
No Suggested Reading articles found!