Please wait a minute...
J Chin Soc Corr Pro  2005, Vol. 25 Issue (5): 312-316     DOI:
Research Report Current Issue | Archive | Adv Search |
ELECTROCHEMICAL CORROSION AND CAVITATION EROSION BEHAVIOR OF Cr-Ni HYDRAULEC TURBINE MATERIAL
Yanchun Lou;Fangxin Zhao;Bo Yu;Jingcheng Wang;Yunlong Xiong
沈阳铸造研究所
Cite this article: 

Yanchun Lou; Fangxin Zhao; Bo Yu; Jingcheng Wang; Yunlong Xiong. ELECTROCHEMICAL CORROSION AND CAVITATION EROSION BEHAVIOR OF Cr-Ni HYDRAULEC TURBINE MATERIAL. J Chin Soc Corr Pro, 2005, 25(5): 312-316 .

Download:  PDF(172KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Based on ZG06Cr13Ni4Mo (13-4),while its chromium content being reduced to 10.61%,8.34% and 6.64% respectively,their anodic polarization curves compared with that of ZG20Cr13 have been tested in 1mol/L H2SO4 solution.Using ultrasonic vibration cavitation erosion device and Rockwell apparatus,the 13-4,the 8.5Cr-4Ni (8.5-4) and the high strength and high toughness stainless steel -SRIF have been studied on the behaviors of cavitation erosion resistance and local micro-zone elasticity respectively.Their microstructures and mechanical properties have also been investigated.The results show that electrochemical corrosion properties decrease as chromium content decreases comparing with these of the 13-4.When chromium content decreases to 8.34%,the material and ZG20Cr13 are matched in electrochemical corrosion properties,which is still in the category of stainless steel.The values of local micro-zone elasticity he of 8.5-4,13-4 and SRIF are very close.The cavitation erosion resistances of the 13-4 are higher a little than these of the 8.5-4,and these of the SRIF are obviously higher than those of 8.5-4 and 13-4.
Key words:  Cr-Ni stainless steel      hydraulic turbine material      electrochemical corrosion      cavitation erosion      mechan     
Received:  20 January 2005     
ZTFLH:  TG174.36  

URL: 

https://www.jcscp.org/EN/     OR     https://www.jcscp.org/EN/Y2005/V25/I5/312

[1]Gysel W,Gerber E,Trautwein A.CA6NM:New developmentsbased on 20 years experience[J].Stainless Steel Castings,1982,(3):403-435
[2]Lou Y C,Lang X,Zhao F X.Effect of variation in chromium on thecharacteristic and regulation of heat treatment for Cr-Ni hydraulicturbine material[J].Foundry,2004,53(5):345-349(娄延春,朗霄,赵芳欣.铬含量对Cr-Ni型水轮机材料特性的影响与调控[J].铸造,2004,53(5):345-349)
[3]Pandey J L,Singh I,Singh M N.Electrochemical corrosion be-haviour of heat-treated AISI 304 austenitic stainless steel in inor-ganic acid mixture[J].Anti-Corrosion Methods and Materials,1997,44(1):6-9
[4]Barreau S,Morton J,Hermas A A.A correlation between phospho-rous impurity in stainless steel and a second anodic current maxi-mum in H2SO4[J].Corros.Sci.,1999,41(12):2251-2266
[5]Wang Z Y,Zhu J H.Effect of primary factors on cavitation erosionresistance of some metastable austenitic metals[J].Acta Metall.Sin.,2003,39(3):273-277(王再友,朱金华.亚稳奥氏体金属抗空蚀性能及其主要控制因素[J].金属学报,2003,39(3):273-277)
[6]Liu W,Zheng Y G,Yao Z M.Cavitation erosion of 20SiMn and0Cr13Ni5Mo steels in distilled water with and without sand[J].Ac-ta Metall.Sin.,2001,37(2):197-201(柳伟,郑玉贵,姚治铭.清水和含沙水中20SiMn和0Cr13Ni5Mo钢的空蚀行为[J].金属学报,2001,37(2):197-201)
[7]Mann B S.Boronizing of cast martensitic chromium nickel stainlesssteel and its abrasion and cavitation-erosion behaviour[J].Wear,1997,208(1):125-131
[8]Long N D,Zhu J H.Cavitation erosion resistance of Fe-26Mn-6Si-7Cr-1Cu shape memory alloy[J].Mater.Sci.Technol.,2003,19(12):1733-1736
[9]Kwok C T,Man H C,Cheng F T.Cavitation erosion of duplex andsuper duplex stainless steels[J].Scripta Materialia,1998,39(9):1229-1236
[10]Luo S Z,Jing H M,Zheng Y G.Cavitation-corrosion behavior ofCrMnN duplex stainless steel[J].J.Chin.Soc.Corros.Prot.,2003,23(5):276-281(骆素珍,敬和民,郑玉贵.CrMnN双相不锈钢的空泡腐蚀行为研究[J].中国腐蚀与防护学报,2003,23(5):276-281)
[11]Wang B,Wang Y D,Zhang Z H.Plating rare earth chromium onhydraulic turbine’s substrates to improve resistance to cavitationerosion and abrasion[J].J.Chin.Soc.Corros.Prot.,2003,23(1):34-37(王飚,王宇栋,张自华.电镀稀土铬提高水轮机的抗空蚀磨损能力[J].中国腐蚀与防护学报,2003,23(1):34-37)
[12]Kaesche H.The Corrosion of Metal[J].The 2ndEdition.Berlin:Springer Press,1979(Kaesche H.Die Korrosion der Metalle—Zweite V llig neubear-beitete und erweiterte Auflage[M].Berlin:Springer,1979)
[13]Geng C W,He S S,Yu B.Study on martensitic stainless steelZG0Cr13Ni4Mo for nuclear power[J].Metal Physics Examinationand Testing,1992,(4):13-25(耿承伟,何树生,于波.核电站用ZG0Cr13Ni4Mo马氏体不锈钢研制[J].物理测试,1992,(4):13-25)
[1] HUANG Hui, LI Shuli, DENG Shuduan, LI Xianghong. Research Progress and Prospects of Smart Materials for Protective Coatings[J]. 中国腐蚀与防护学报, 2026, 46(5): 1369-1388.
[2] BAI Yujie, ZHAI Xiaoliang, CUI Zhongyu. Research Progress on Hydro-thermo-mechanical Multi-field Coupling Environment of Plateau Permafrost and Its Effect on Material Damage Behavior[J]. 中国腐蚀与防护学报, 2026, 46(5): 1389-1399.
[3] XU Jiacheng, LIU Jiabing, HUANG Shiyu, JIN Linghao, TAN Wei, GUO Na, LIU Tao. Mechanical Property Damage and Stress Corrosion Behavior of EH40 Steel Ship Plate in Artificial Polar Marine Environments[J]. 中国腐蚀与防护学报, 2026, 46(5): 1437-1451.
[4] TANG Min, DU Pengfei, XU Juan, LEI Ran, LI Xingxin, LI Xianghong. Corrosion Inhibition Effect and Mechanism of Invasive Species Bidens pilosa L. Extract on ST12 Steel in H2SO4 Medium[J]. 中国腐蚀与防护学报, 2026, 46(5): 1485-1496.
[5] JIA Mengyao, ZHANG Weiqiang, WANG Yuan, TAN Jibo, QIU Jianke, HAO Yantian, WU Xinqiang. Effect of Pressure Variation on Stress Corrosion Behavior of Ti80 Alloy in 3.5%NaCl Solution[J]. 中国腐蚀与防护学报, 2026, 46(5): 1508-1516.
[6] LI Xiaofeng, LI Yanru, LU Yunfei, ZHANG Taihua, CHANG Xueting, AN Yan. Polypyrrole-modified Aramid Fiber/Epoxy Composite Coating with Synergistically Enhanced Mechanical and Anti-corrosion Properties[J]. 中国腐蚀与防护学报, 2026, 46(5): 1517-1526.
[7] PANG Chengze, XING Shaohua, DU Min, XU Cheng. Research Progress on Wear Corrosion Al-alloys in Marine Environment[J]. 中国腐蚀与防护学报, 2026, 46(4): 962-970.
[8] LING Wei, LI Hongyan, HE Lili, JIN Long, HAO Hongtao. Research Progress on Microbial Corrosion in Oil and Gas Gathering Pipelines[J]. 中国腐蚀与防护学报, 2026, 46(4): 1001-1014.
[9] MA Huanhuan, LV Shengdong, QIAN Yixin, LIN Yong, HAO Xiangping, ZHANG Dawei, WANG Luning. Localized Corrosion and Service Life Prediction of Copper Heat Exchange Tubes in a Sodium Acetate Trihydrate Phase Change Thermal Energy Storage System[J]. 中国腐蚀与防护学报, 2026, 46(4): 1045-1057.
[10] HUANG Tao, ZHU Yu, DENG Yu, WANG Qishan, TIAN Yichen, CHEN Xu. Effect of Hydrogen on Mechanical Properties and Corrosion Behavior in 3.5%NaCl Solution of X65 Steel and Its Weld Zone[J]. 中国腐蚀与防护学报, 2026, 46(4): 1107-1116.
[11] XU Huiqiang, LAI Changqing, WANG Xixi, WANG Ziming. Influence of Sacrificial Anode Materials on Corrosion Behavior of B30 Cu-Ni Alloy Heat Transfer Tubes in a Simulated System of Circulating Seawater[J]. 中国腐蚀与防护学报, 2026, 46(4): 1139-1147.
[12] ZHOU Weilong, GUO Yubing, HU Mengru, SHEN Kaijie, YANG Zhenghuan, XIE Linjun. Effect of Sodium Phosphate Concentration on Corrosion Resistance of 40Cr Steel[J]. 中国腐蚀与防护学报, 2026, 46(4): 1185-1196.
[13] PANG Yu, ZHANG Wenyan, PANG Yu, WANG Xiwei, WANG Feng, LING Taoqiang, LI Wenpo. Influence of Factors Related with Environment and Anti-corrosion Coating on External Corrosion of Gathering and Transport Pipelines[J]. 中国腐蚀与防护学报, 2026, 46(4): 1249-1256.
[14] WANG Liuhuo, SUN Qiang, QI Han, HU Sukai, YE Huanhuan, LIU Jiahan, WANG Dayang, ZHANG Tao. Salt Spray Corrosion of DH460 Steel for Offshore Converter Stations and Protectiveness of Ceramic Coatings[J]. 中国腐蚀与防护学报, 2026, 46(4): 1257-1268.
[15] WANG Yanfeng, WANG Liuhuo, SUN Shida, LIU Qi, LI Yamei, WANG Xianzong. Research Progress on Failure of Key Materials and Mitigation Measures for Cooling System of Flexible DC Converter Valve[J]. 中国腐蚀与防护学报, 2026, 46(3): 653-662.
No Suggested Reading articles found!