Abstract The crevice corrosion of 316, 904L, 254sMo and 2507 stainless steels in a liquid of the so called green death at 70 ℃, which aims to simulate the corrosive environment of flue gas desulfurization process, was comparatively investigated by means of electrochemical cyclic polarization test and SEM. The results showed that 254sMo and 2507 stainless steel have excellent resistance to crevice corrosion, while the crevice corrosion induced damage of SS316 and SS904L is serious. The "lace cover" structures were observed on the edges of the gap of SS316 and SS904L, but not on that of SS254sMo and SS2507. At the bottom of crevice corrosion pit, duplex super stainless steel 2507 exhibits galvanic corrosion characteristics.
|
Received: 25 December 2017
|
|
Fund: Supported by National Natural Science Foundation of China(51071160);National High Technology Research and Development Plan(2015AA034301) |
Corresponding Authors:
Junhua DONG
E-mail: jhdong@imr.ac.cn
|
[1] | Han W. Safety and corrosion prevention of chimney after flue gas desulphurization [J]. Electr. Safety Technol., 2010, 12(8): 12 | [1] | 韩伟. 烟气脱硫改造后烟囱的安全性及其防腐 [J]. 电力安全技术, 2010, 12(8): 12 | [2] | Xu S Q. Dew point corrosion and material selection (2) [J]. Petrochem. Corros. Prot., 2000, 17(3): 1 | [2] | 许适群. 关于露点腐蚀及用钢的综述 (二) [J]. 石油化工腐蚀与防护, 2000, 17(3): 1 | [3] | He J J, Xiang X X. A review of chimney corrosion study and anticorrosion material research in WFGD [J]. Environ. Technol., 2011, 35(4): 33 | [3] | 何佳杰, 向贤伟. 湿法烟气脱硫中烟囱腐蚀及其防腐材料研究现状 [J]. 环境技术, 2011, 35(4): 33 | [4] | Gao W, Luo J M, Yang J J. Research progress and application of double phase stainless steel [J]. Ordnance Mater. Sci. Eng., 2005, 28(3): 61 | [4] | 高娃, 罗建民, 杨建君. 双相不锈钢的研究进展及其应用 [J]. 兵器材料科学与工程, 2005, 28(3): 61 | [5] | Xu Q. Corrosion-resisting alloy selection for flue gas desulfurization unit (FGD) [J]. Total Corros. Control, 2010, 24(10): 6 | [5] | 许青. 烟气脱硫(FGD)装置耐腐蚀合金的选择 [J]. 全面腐蚀控制, 2010, 24(10): 6 | [6] | Kim M T, Oh O Y, Chang S Y. Analysis of degradation of a super-austenitic stainless steel for flue gas desulfurization system after a fire accident [J]. Eng. Fail. Anal., 2008, 15: 575 | [7] | Han D, Jiang Y, Deng B, et al. Detecting critical crevice temperature for duplex stainless steels in chloride solutions [J]. Corrosion, 2011, 67: 025004 | [8] | Jamaluddin A M, Malika A U, Andijani I, et al. Crevice corrosion behavior of high-alloy stainless steels in a SWRO pilot plant [J]. Desalination, 2004, 171: 289 | [9] | Rajendran N, Rajeswari S. Super austenitic stainless steels-a promising replacement for the currently used type 316L stainless steel as the construction material for flue-gas desulphurization plant [J]. J. Mater. Sci., 1996, 31: 6615 | [10] | Zhang Y G, Li S Y, Fan H Q, et al. Corrosion behavior of stainless steel in flue gas desulphurization system [J]. Mater. Prot., 2010, 43(3): 64 | [10] | 张贻刚, 李淑英, 范洪强等. 不锈钢在烟气脱硫系统中的腐蚀行为 [J]. 材料保护, 2010, 43(3): 64 | [11] | Feng H. Research on corrosion behaviour of super austenitic stainless steel with high Mo and N in typically extreme environments [D]. Shenyang: Northeastern University Dissertations, 2014: 21 | [11] | 冯浩. 高钼高氮超级奥氏体不锈钢在典型极端环境中的腐蚀行为研究 [D]. 沈阳: 东北大学, 2014: 21 | [12] | Wang C G, Dong J H, Ke W, et al. Research on pitting corrosion behavior of copper in the solution with HCO3- and Cl- [J]. Acta Metall. Sin., 2012, 48: 1365 | [12] | 王长罡, 董俊华, 柯伟等. HCO3-和Cl-混合体系中Cu的点蚀行为研究 [J]. 金属学报, 2012, 48: 1365 | [13] | Wang C G, Dong J H, Ke W, et al. Effect of HCO3- and SO42- on the pitting corrosion behavior of Cu [J]. Acta Metall. Sin., 2012, 48: 85 | [13] | 王长罡, 董俊华, 柯伟等. HCO3-和SO42-对Cu点蚀行为的影响 [J]. 金属学报 2012, 48: 85 | [14] | Yang Y Z, Jiang Y M, Li J. Insitu investigation of crevice corrosion on UNS S32101 duplex stainless steel in sodium chloride solution [J]. Corros. Sci., 2013, 76: 163 | [15] | Al-khamis J N, Pickering H W. IR mechanism of crevice corrosion for alloy T-2205 duplex stainless steel in acidic-chloride media [J]. | [15] | J. Electrochem. Soc., 2001, 148: B314 |
|
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|