IMPRESSED CURRENT CATHODIC PROTECTION OF EXTERNAL TANK BOTTOM WITH SOLID-ELECTROLYTE-CONTAINING COATING |
Ge Doufu; Zhang Zongwang (East-China Oil Piping Administration) Zhang Chengdian and Xu Naixin (Shanghai Institute of Metallurgy;Chinese Academy of Sciences) |
|
|
Abstract A new approach of impressed current cathodic protection for external tank bottom has been developed. An electronically conducting anode coating was applied on the bituminous sand base for above-ground storage tank, followed by a specially formulated CK coating, which contains the solid electrolyte sodiumβ(β″)alumina as an ionically conducting component. Graphite electrodes were embedded in the CK coating to control and/or monitor the cathode potential. The multilayer structure consisting of external tank bottom, CK coating and anode coating enables the completion of current circuit. An appropriate d.c. power source was used to provide current. Compared with conventional cathodic protection techniques, the new approach has significant advantages. Due to the close proximity of cathodically proretted urface to coating anode, the cathodic protection current would not be lost outwards. As a result, the tank to be protected is not necessarily isolated from neighbouring underground metallic structures. At the same time, it also leads to more uniform distribution of protective potential. The feasibility of the proposed technique has been verified both by small simulating tank and by practical applications. Such a cathodic protection system for an above-ground storage tank of 30-m in diameter by 15.8-m in height has already been in operation successfully for two years.
|
Received: 25 April 1992
|
Cite this article:
Ge Doufu; Zhang Zongwang (East-China Oil Piping Administration) Zhang Chengdian and Xu Naixin (Shanghai Institute of Metallurgy;Chinese Academy of Sciences). IMPRESSED CURRENT CATHODIC PROTECTION OF EXTERNAL TANK BOTTOM WITH SOLID-ELECTROLYTE-CONTAINING COATING. J Chin Soc Corr Pro, 1992, 12(2): 149-153.
URL:
https://www.jcscp.org/EN/ OR https://www.jcscp.org/EN/Y1992/V12/I2/149
|
[1] 星野九平,山室富士雄著,张宴译,《管道及其设备的腐蚀与防蚀》,石油工业出版社,1979年,P.68~69 [2] 山室富士雄,阿部三之.配管,7,4~12(1973) [3] BSI CP 1021: 1973 Code of Practice for Cathodic Protection中译本:《阴极保护实施规范》,英国标准局编,洪定海译,周本省较,国防工业出版社,1987年,P.31~32 [4] 石油工业部部标准SYJ 7~84钢质管道及储罐防腐蚀工程设计规范,第4页 [5] Garrity K. C. and Urbas, M. Materials Performance, 27(4) , 32~35(1988) [6] 葛斗福 张宗旺 张承典 徐乃欣,中国腐蚀与防护学报9(2) ,130~136(1989) [7] Ge Doufu, Zhang Zongwang, Zhang Chengdian and Xu Naixin, British Corrosion Journal, 24(4) , 265~268(1989) [8] Ge Doufu. Zhang Zongwang, Zhang Chengdian and Xu Naixin, Proceedings of the 6th Asian-Pacific Corrosion Control Conference, Part H, 85~88(1989) [9] Merrick,R.D.,Materials Performance,26,(1) ,29~37(1987) 译文刊于腐蚀与防护No.1,46~50(1989) [10] 浅利满赖.须藤皓,水流澈,春山志郎.防食技术,36(1) ,17~22(1987) |