[1] Wortman, D. J.; Fryxel, R. E.; Luthra, K. L.; Bergman, P. A., Thin Solid Films, 64, 281(1979) [2] Jones, R. L.; Gadomski, S. T., J. Electrochem. Soc., 129(7) , 1613(1982) [3] Phase Diagrams for Ceramists, Ernest M. Levin et at ed., 346(1964) [4] Goebel, J. A.; Pettit, F. S., Met. Trans., 1A(7) , 1943(1970) [5] Luthra, K. L., Worrell, W. L.; Met. Trans., 10A(5) , 621(1979) [6] Singh, P.; Birks, N., OXido Met., 12(1) . 23(1978) [7] Giggrus, C. S.; Pettit, F. S., Oxid. Met., 14(6) , 363(1980) [8] Bastow, B. D.; Wood, O. C., Oxid. Met., 9(5) , 473(1975) [9] Freer. R.; J. Met. Sci., 15, 803(1980) [10] Kohl, N. N.: Smeltzer, W. W.: Embury, J. D., J. Electroehem, Soc., 122(11) . 1495(1975) [11] Stoklosa, A., Oxid, Met., 11(5) , 277(1977) [12] 《热力学数据表》,东北工学院冶金物化专业编,(1979) [13] Lin, R. Y.: Hu, D. C.: Chang. Y. A., Met. Trans.. 9B(12) , 531(1978) [14] Misra, A. K., Whittle, D. P.: Worrell, W. L., J. Electrochem, Soc., 129(8) , 1840(1982) [15] Kostin, L. P.: Pluzhnikov, L. L.: Ketov, A. N.: Russian J. of Phys, Chem.. 49, P1313 [16] Andersen. R. E., J. Eleetrochem, Soc., 126(2) , 328(1979) |