Ti-24Al-11Nb金属间化合物的氢致滞后开裂 |
张跃;王忆;王燕斌;褚武扬;肖纪美 |
北京科技大学 |
|
HYDROGEN INDUCED DELAYED CRACKING OF INTERMETALLIC COMPOUND Ti-24Al-11Nb |
Zhang Yue; Wang Yi; Wang Yanbin; Chu Wuyan; Xiao Jimei(University of Science and Technology; Beijing) |
1StoloffNS.In:HydrogenEffectsonMaterialBehavior,EditedbyMoodyNR,ThompsonAW.TheMinerals,MetalsandMaterialsSociety,1990,p4832ZhangDZ,ChuWY,HaialJM.Scripta.Metal.Mater,1992,26:273ChuWY,ThompsonAW,WilliamsJC.ActaMetal.Mater,1992;40:4554ChuWY,ThompsonAW.MetallTrans.A,1992,23A:12995褚武扬,肖纪美,ThompsonAW.ActaMetall.Sinica,1992,5A:2866褚武扬.氢损伤与滞后断裂,北京:冶金出版社,1988,4867ChuWY,ThompsonAW.MetallTrans.A,1991,22A:718ChuWY,ThomponAW.In:HighPerformanceCompositesforthe1990's,EditedbyDasSK,BallardCP,MarikarF.TMS,143 |
|